# US 2023/0069057 A1 · Growth Device and Method for Low-Stress Crystals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0069057 A1
- Document ID: US20230069057A1
- Status: Published application
- Kind: A1
- Application number: 17/797,063
- Filed: 2021-07-05
- Published: 2023-03-02
- Earliest claimed: 2021-02-03
- Assignees: The 13th Research Institute of China Electronics Technology Group Corporation
- Applicants: The 13Th Research Institute of China Electronics Technology Group Corporation
- Inventors: Yanlei SHI; Niefeng SUN; Shujie WANG; Lijie FU; Huimin SHAO; Hongfei ZHAO; Yaqi LI; Huisheng LIU; Tongnian SUN; Yong KANG; Xiaodan ZHANG; Xin ZHANG; Jian JIANG; Xiaolan LI; Yang WANG; Jing XUE
- Web page: https://patentgrep.com/patent/US20230069057A1

## CPC

- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B 15/02: adding crystallising materials or reactants forming it in situ to the melt
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/206: {the thermal history of growing the ingot}
- C30B 27/02: by pulling from a melt
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A growth device and method for low-stress crystals are provided, which relate to the field of preparation of crystals, in particular to a device and method for preparing low-stress and low-defect crystals by using a pulling method. The growth device includes a furnace body; a crucible and a heating and insulation system which are arranged at a bottom of the furnace body; a crystal pulling mechanism, and a quartz observation window; the device further includes a liftable heating mantle mechanism including a heating mantle body, a heating mantle supporting component, a heating wire arranged around the heating mantle body, and a heating mantle lifting mechanism. The method includes: after crystals are pulled out of a melt, covering the crystals with a liftable heating mantle mechanism. By the use of the present invention, a temperature gradient inside the crystals in a crystal growth process and in a cooling process after the crystals are pulled can be reduced, thereby reducing the crystal stress, reducing defects, and avoiding the crystals from being cracked; and at the same time, the temperature gradient in the melt is maintained, thereby guaranteeing a stable crystal growth process and ensuring the yield of the crystals.

## Claims

### Claim 1

A growth device for low-stress crystals, characterized by comprising a furnace body (19); a crucible (18) and a heating and insulation system which are arranged at a bottom of the furnace body (19); a crystal pulling mechanism directly facing a center of the crucible (18); and a quartz observation window (11) arranged on a side surface of the furnace body (19), wherein the heating and insulation system comprises a heater (7), a crucible rod (12), and a heat insulation sleeve (13); the crystal pulling mechanism comprises a seed rod (3) and a seed chuck (2); the device further comprises a liftable heating mantle mechanism; the liftable heating mantle mechanism comprises a heating mantle body (8), a heating mantle supporting component (9), a heating wire (14) arranged around the heating mantle body (8), and a heating mantle lifting mechanism (10); and a thermocouple (21) is arranged inside the heating mantle body (8).

### Claim 2 (depends on 1)

The growth device for the low-stress crystals according to claim 1, characterized in that a top of the heating mantle body (8) is a conical multi-layer hollow structure, and a bottom is cylindrical; the heating mantle body is made of a transparent material; and an outer diameter of the cylindrical part is less than an inner diameter of the crucible (18).

### Claim 3 (depends on 1, 2)

The growth device for the low-stress crystals according to claim 1 or 2, characterized in that the seed rod (3) passes through the heating mantle body (8); and the heating mantle lifting mechanism (10) drives the liftable heating mantle mechanism to move up and down along the seed rod (3); and a gap reserved between the seed rod (3) and the top of the heating mantle body (8) does not exceed 2 mm.

### Claim 4 (depends on 1)

The growth device for the low-stress crystals according to claim 1, characterized in that a gas source box (17) is further arranged inside the liftable heating mantle mechanism; and the gas source box (17) is positioned at an inner upper end of the heating mantle body (8) by using a gas source box fixing pin (15).

### Claim 5 (depends on 1)

The growth device for the low-stress crystals according to claim 1, characterized in that a heating wire (14) is disposed at a start position upward from the bottom of the heating mantle body (8), which is ⅙ greater than the length of the heating mantle body (8).

### Claim 6 (depends on 1)

The growth device for the low-stress crystals according to claim 1, characterized in that a depth marking line is set at a periphery of the heating mantle body (8) from the bottom.

### Claim 7 (depends on 6)

The growth device for the low-stress crystals according to claim 6, characterized in that after the liftable heating mantle mechanism is lowered, the quartz observation window (11) is aligned to the set marking line.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

A growth method for low-stress crystals, which is completed on the basis of the growth device for low-stress crystals according to any one of claims 1 to 7, characterized in that the growth method comprises the following step:
after crystals are pulled out of a melt, covering the crystals with a liftable heating mantle mechanism.

### Claim 9 (depends on 8)

The growth method for the low-stress crystals according to claim 8, characterized in that the growth method comprises the following steps:
A. placing a raw material and the covering agent (5) in the crucible (18); placing a gas source material (16) in the gas source box (17); and turning on the heater (7) for heating until the raw material and the covering agent (5) are melted, wherein the raw material becomes a melt (6);
B. disposing a seed (1) on a seed chuck (2), and lowing the seed rod (3) until the seed (1) is in contact with a surface of the melt (6);
C. when a crystal (4) grows to a desired diameter, turning on a power supply of a heating wire (14); and lowering the liftable crystal heating mantle to enable the bottom of the heating mantle body (8) to be in contact with the covering agent (5), wherein the desired diameter refers to a wafer size +5 mm;
D. in a growth process of the crystal (4), maintaining a temperature in the heating mantle body (8);
lowering the heating mantle mechanism with a decline in a liquid level of the covering agent (5) to keep the bottom of the heating mantle body (8) being in contact with the covering agent (5);
measuring the temperature inside the mantle through the thermocouple (21) inside the mantle; and
when the crystal (4) is to be pulled out of the covering agent (5), increasing the power of the heating wire (14) to ensure that the temperature inside the mantle reaches a gasification temperature of the gas source material (16);
E. after the growth of the crystal (4) is completed, pulling the crystal (4) to a position above the liquid level of the covering agent (5);
F. enabling a program to cool the heating wire 14 to room temperature in 5-20 h; and configuring a cooling program for the heater (7) to cool the same to the room temperature in 5-20 h;
G. disassembling the furnace, and removing the crystal (4), wherein the heating wire (14) is disposed at a start position upward from the bottom of the heating mantle body (8), which is ⅙ greater than the length of the heating mantle body (8);
in the steps C and D, the heating wire (14) is avoided form being immersed in the covering agent (5);
in the step A, the raw material is a semiconductor material for generating a wafer.

### Claim 10 (depends on 9)

The growth method for the low-stress crystals according to claim 9, characterized in that the raw material is one of indium phosphide, gallium arsenide, gallium phosphide, indium arsenide, indium antimonide, gallium antimonide, and phosphorus germanium zinc; and the gas source material (16) is selected according to the raw material, and is one of phosphorus, arsenic, and antimony.