# US 2023/0068869 A1 · Method for preparing gradient hardened titanium alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0068869 A1
- Document ID: US20230068869A1
- Status: Published application
- Kind: A1
- Application number: 17/880,652
- Filed: 2022-08-04
- Published: 2023-03-02
- Earliest claimed: 2021-08-27
- Assignees: Beijing Institute of Technology
- Applicants: Beijing Institute of Technology
- Inventors: PENGWAN CHEN; YANSONG GUO; QIANG ZHOU; RUI LIU
- Web page: https://patentgrep.com/patent/US20230068869A1

## CPC

- C22F 3/00: Changing the physical structure of non-ferrous metals or alloys by special physical methods, e.g. treatment with neutrons
- C22C 14/00: Alloys based on titanium
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

In a method for preparing a gradient hardened titanium alloy. A steel momentum block and a cleaned titanium alloy plate are sequentially placed into a steel base with a through hole from bottom to top, a cross sectional size of the through hole is matched with cross sectional sizes of the steel momentum block and the titanium alloy plate, and a height of the through hole is matched with a total thickness of the steel momentum block and the titanium alloy plate. An explosive frame is fixed on a top edge of the steel base, a high explosion velocity explosive with an explosion velocity of 7000 m/s or more pressed into a plate-shaped structure is placed in the explosive frame, and detonation is caused at one end of a top surface of the explosive to perform impact treatment on the titanium alloy plate, thereby obtaining the gradient hardened titanium alloy.

## Claims

### Claim 1

A method for preparing a gradient hardened titanium alloy, comprising:
placing a steel base on a pre-paved sandpile;
putting a steel momentum block and a cleaned titanium alloy plate in the steel base with a through hole sequentially from bottom to top, wherein a size of a cross section of the through hole is matched with sizes of cross sections of the steel momentum block and the titanium alloy plate, and a height of the through hole is matched with a total thickness of the steel momentum block and the titanium alloy plate;
fixing an explosive frame on an edge of a top surface of the steel base;
placing high explosion velocity explosive with an explosion velocity of equal to or greater than 7000 m/s and pressed into a plate-shaped structure in the explosive frame; and
detonating from an end of a top surface of the explosive to perform impact treatment on the titanium alloy plate to thereby obtain the gradient hardened titanium alloy.

### Claim 2 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein the impact treatment is performed twice or three times.

### Claim 3 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein a ratio of a thickness of the titanium alloy plate:a thickness of the steel momentum block:a thickness of the high explosion velocity explosive:a horizontal distance between a side of the steel base close to an explosive detonation position and the titanium alloy plate:a distance between a side of the steel base far away from the explosive detonation position and the titanium alloy plate is 10-50:5-10:3-5:50-80:10-20.

### Claim 4 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein a detonation surface of the titanium alloy plate, and a contact surface of the titanium alloy plate with the steel momentum block both are coated with grease.

### Claim 5 (depends on 4)

The method for preparing the gradient hardened titanium alloy as claimed in claim 4, wherein a coating thickness of the grease is in a range of 0.5 mm to 1 mm.

### Claim 6 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein a material of each of the steel base and the steel momentum block is 45# steel or stainless steel, and a material of the explosive frame is an organic glass.

### Claim 7 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein the high explosion velocity explosive is castable powder explosive, plastic plate-shaped explosive or rubber plate-shaped explosive.

### Claim 8 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein the high explosion velocity explosive is composition 4 (C4) explosive.

### Claim 9 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein the explosive is fixed with the steel base together before the explosive is detonated.

### Claim 10 (depends on 1)

The method for preparing the gradient hardened titanium alloy as claimed in claim 1, wherein the impact treatment is performed twice or three times;
wherein a ratio of a thickness of the titanium alloy plate:a thickness of the steel momentum block:a thickness of the high explosion velocity explosive:a horizontal distance between a side of the steel base close to an explosive detonation position and the titanium alloy plate:a distance between a side of the steel base far away from the explosive detonation position and the titanium alloy plate is 10-50:5-10:3-5:50-80:10-20;
wherein a detonation surface of the titanium alloy plate, and a contact surface of the titanium alloy plate with the steel momentum block both are coated with grease, and a coating thickness of the grease is in a range of 0.5 mm to 1 mm;
wherein a material of each of the steel base and the steel momentum block is 45# steel or stainless steel;
wherein a material of the explosive frame is an organic glass;
wherein the high explosion velocity explosive is composition 4 (C4) explosive; and