# US 2023/0068733 A1 · Method for monitoring an attachment area during the laser welding of bent bar-type conductors containing copper

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0068733 A1
- Document ID: US20230068733A1
- Status: Published application
- Kind: A1
- Application number: 18/054,550
- Filed: 2022-11-11
- Published: 2023-03-02
- Earliest claimed: 2020-05-15
- Assignees: TRUMPF Laser- und Systemtechnik GmbH
- Applicants: TRUMPF Laser- und Systemtechnik GmbH
- Inventors: Oliver Bocksrocker; Nicolai Speker
- Web page: https://patentgrep.com/patent/US20230068733A1

## CPC

- B23K 31/125: {Weld quality monitoring}
- H02K 15/35: Form-wound windings
- B23K 26/22: Spot welding
- G01N 25/72: Investigating presence of flaws
- G01N 33/207: Welded or soldered joints; Solderability
- B23K 2101/38: Conductors
- G01N 2021/1761: {A physical transformation being implied in the method, e.g. a phase change}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method for monitoring an attachment area during laser welding of bent bar-type conductors containing copper, includes the steps of arranging a first bar-type conductor relative to a second bar-type conductor in partially overlapping fashion and welding the first and second bar-type conductors to one another using a processing laser beam, the welding including forming a weld bead interconnecting the bar-type conductors to one another. After the welding, at least one measurement variable is measured on at least one portion of the weld bead, wherein the at least one measurement variable changes with the temperature of the weld bead as a function of the time during a cooling down of the weld bead. A parameter depending on a heat capacity of the weld bead is determined from the at least one measured measurement variable, and the attachment area qualitatively or quantitatively determined from the parameter.

## Claims

### Claim 1

A method for monitoring an attachment area during laser welding of bent bar-type conductors containing copper, the method comprising:
arranging a first bar-type conductor relative to a second bar-type conductor in partially overlapping fashion;
welding the first and second bar-type conductors to one another using a processing laser beam, the welding including forming a weld bead interconnecting the bar-type conductors to one another;
after the welding, measuring on at least one portion of the weld bead at least one measurement variable that changes with the temperature of the weld bead as a function of the time during a cooling down of the weld bead;
determining a parameter depending on a heat capacity of the weld bead from the at least one measured measurement variable; and
determining the attachment area qualitatively or quantitatively from the parameter.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein
the arranging of the first and second bar-type conductors is performed such that end regions of the first and second bar-type conductors are respectively parallel to one another and next to one another,
end surfaces of the first and second bar-type conductors are located approximately level in relation to a direction of a longitudinal extent of the end regions, and
the processing laser beam is directed at the two bar-type conductors in such a way that the weld bead is formed at the end surfaces of the bar-type conductors.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the measuring of the at least one measurement variable includes observing at least a portion of the weld bead in the visible spectral range and/or in the infrared spectral range.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein the measuring of the at least one measurement variable is performed on a portion of the weld bead opposite to a portion of the bar-type conductors on which the processing laser beam acted.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the at least one measurement variable comprises an intensity of a thermionic emission of at least the portion of the weld bead.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the intensity of the thermionic emission is measured in a restricted spectral range.

### Claim 7 (depends on 1)

The method as claimed in claim 1, further comprising illuminating the weld bead using an observation light beam while the said weld bead cools down,
and wherein the at least one measurement variable comprises an intensity of the observation light beam reflected at the surface of the weld bead.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the intensity of the reflected observation light beam is measured in a restricted spectral range about a central wavelength of the observation light beam.

### Claim 9 (depends on 7)

The method as claimed in claim 7, further comprising disposing a polarization filter in front of a sensor device used to measure the intensity of the reflected observation light beam.

### Claim 10 (depends on 5)

The method as claimed in claim 5, wherein
the weld bead is observed using a camera and the intensity of the thermionic emission is determined using the camera by virtue of a mean grayscale value from the camera in a partial region of the image recorded by the camera being determined.

### Claim 11 (depends on 5)

The method as claimed in claim 5, wherein the weld bead is observed using a photodiode and the intensity of the thermionic emission is determined as a grayscale value from the photodiode.

### Claim 12 (depends on 1)

The method as claimed in claim 1, wherein the measurement variable comprises a temperature at least on a portion of the weld bead.

### Claim 13 (depends on 12)

The method as claimed in claim 12, wherein the temperature is measured using quotient pyrometry, with intensities of a thermionic emission at least of the portion of the weld bead being measured at two different wavelengths.

### Claim 14 (depends on 1)

The method as claimed in claim 1, wherein the parameter is a time duration that elapses between a first defined state and a second defined state while the weld bead cools down.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the first defined state is the end of the processing laser beam exposure.

### Claim 16 (depends on 14)

The method as claimed in claim 14, wherein the second defined state is a complete solidification of the weld bead.

### Claim 17 (depends on 14)

The method as claimed in claim 14, wherein the first and/or the second defined state is recognized by virtue of the measurement variable reaching a threshold value.

### Claim 18 (depends on 14)

The method as claimed in claim 14, wherein the first and/or the second defined state is recognized by virtue of a first and/or second time derivative of the measurement variable reaching a threshold value.

### Claim 19 (depends on 1)

The method as claimed in claim 1, wherein the parameter is a gradient of the measurement variable with respect to time and is determined at a specified time or averaged over a specified time period.

### Claim 20 (depends on 1)

The method as claimed in claim 1, further comprising comparing the parameter or the attachment area to a decision value,
wherein, when the decision value is not reached, recognizing that the attachment area of the weld as being too small,
and, when the decision value is reached, recognizing the attachment area as being sufficiently large and permitting the affected bar-type conductors to be used further.

### Claim 21 (depends on 20)

The method as claimed in claim 20, further comprising determining a proportion of a cross section of the bar-type conductors not covered by the weld bead using a camera and recognizing the attachment area of the weld of the bar-type conductors as being too small when the uncovered proportion of the cross section exceeds a limit value, even if the decision value is reached.

### Claim 22 (depends on 1)

The method as claimed in claim 1, further comprising welding a multiplicity of pairs of bar-type conductors in succession, with one or more welding parameters being optimized and/or updated in a control loop when the pairs of bar-type conductors are welded such that the parameter or an attachment area quantitatively determined from the parameter is set to a specified target value for the pairs of welded bar-type conductors.

### Claim 23

An apparatus for laser welding bent bar-type conductors containing copper, the apparatus comprising:
a holding device configured to arrange two bar-type conductors in overlapping fashion, the holding device comprising a stator mount with a multiplicity of bar-type conductors to be welded;
a laser processing head configured to provide a processing laser beam configured to weld the two bar-type conductors to one another such that a weld bead interconnecting the bar-type connectors is formed;
a sensor device configured to measure at least one measurement variable that changes with a temperature of the weld bead at least on one portion of the weld bead following an end of exposure to the processing laser beam and while the weld bead cools down;
an electronic evaluation device configured to determine a parameter depending on a heat capacity of the weld bead from the at least one measurement variable
and furthermore configured to qualitatively or quantitatively determine an attachment area set up by the weld bead from the parameter.