# US 2023/0068588 A1 · Chemically strengthened glass, and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0068588 A1
- Document ID: US20230068588A1
- Status: Published application
- Kind: A1
- Application number: 18/053,573
- Filed: 2022-11-08
- Published: 2023-03-02
- Earliest claimed: 2020-07-31
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Kaname SEKIYA; Yusuke FUJIWARA
- Web page: https://patentgrep.com/patent/US20230068588A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/095: containing rare earths
- C03C 4/18: for ion-sensitive glass
- C03C 2204/00: Glasses, glazes or enamels with special properties
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The present invention relates to a chemically strengthened glass having a thickness of t [mm], and having a profile of a stress value CSx [MPa,] at a depth x [µm] from a surface of the glass, the stress value being measured by a scattered-light photoelastic stress meter, in which a second-order differential value CSx" of the stress value CSx in the profile satisfies the following expression within a range of CSx≥0: 0<CSx"≤0.050.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A method of manufacturing a chemically strengthened glass, the method comprising:
immersing a lithium-containing glass into a first molten salt composition comprising sodium ions and potassium ions to thereby perform first ion exchange; and
immersing the lithium-containing glass into a second molten salt composition comprising potassium ions and an additive to thereby perform second ion exchange,
wherein in the first molten salt composition, a concentration of potassium nitrate is higher than a concentration of sodium nitrate,
in the second molten salt composition, a concentration of potassium nitrate is 85 mass% or higher, and a mass ratio of sodium ions to lithium ions is 0 or higher and 15 or lower, and
the additive comprises either one of silicic acid or carbonate.

### Claim 9 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the concentration of potassium nitrate in the first molten salt composition is higher than 50 mass%.

### Claim 10 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the second molten salt composition comprises sodium nitrate whose concentration is higher than 0 mass% and 5 mass% or lower.

### Claim 11 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the second molten salt composition comprises lithium ions whose concentration is 0.1 mass% or higher and 10 mass% or lower.

### Claim 12 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein in the first ion exchange, the first molten salt composition has a temperature of 380° C. or higher and 450° C. or lower.

### Claim 13 (depends on 12)

The method of manufacturing a chemically strengthened glass according to claim 12, wherein in the first ion exchange, the lithium-containing glass is immersed in the first molten salt composition for 0.5 hours or more and 8 hours or less.

### Claim 14 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein in the second ion exchange, the second molten salt composition has a temperature of 380° C. or higher and 450° C. or lower.

### Claim 15 (depends on 14)

The method of manufacturing a chemically strengthened glass according to claim 14, wherein in the second ion exchange, the lithium-containing glass is immersed in the second molten salt composition for an immersion time t2 [min] satisfying the following expression using a temperature T [°C] of the second molten salt composition:
-0
.38T+173<t2<-1
.4T+650
.

### Claim 16 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the chemical strengthening is performed so that a tensile stress value CT2 [MPa] of the chemically strengthened glass after the second ion exchange is a value corresponding to 50% to 93% of a tensile stress value CT1 [MPa] of the chemically strengthened glass after the first ion exchange.

### Claim 17 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein a tensile stress value CT1 [MPa] of the chemically strengthened glass after the first ion exchange satisfies the following expression using a thickness t [mm] of the chemically strengthened glass:
CT
1
>-120t+164
.

### Claim 18 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the lithium-containing glass comprises, by mol% in terms of oxides:
52
to
75%
of
SiO
2;
8
to
20%
of
Al
2
O
3
;
5
to
16%
of
LiO
2
;
and
8%
or
lower
of
NaO
2
.

### Claim 19 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the additive comprises the silicic acid and the content of the silicic acid in the second molten salt is 0.1 mass% or higher and 3 mass% or lower.

### Claim 20 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein the additive comprises the carbonate and the content of the carbonate in the second molten salt is 2 mass% or lower.

### Claim 21 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein in the first ion exchange, the first molten salt composition has a temperature of 421° C. or higher and 450° C. or lower.

### Claim 22 (depends on 8)

The method of manufacturing a chemically strengthened glass according to claim 8, wherein in the second ion exchange, the second molten salt composition has a temperature of 380° C. or higher and 400° C. or lower.