# US 2023/0068164 A1 · 3xx aluminum casting alloys, and methods for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0068164 A1
- Document ID: US20230068164A1
- Status: Published application
- Kind: A1
- Application number: 17/967,708
- Filed: 2022-10-17
- Published: 2023-03-02
- Earliest claimed: 2015-08-13
- Assignees: Alcoa USA Corp.
- Applicants: Alcoa USA Corp.
- Inventors: Xinyan Yan; Jen C. Lin
- Web page: https://patentgrep.com/patent/US20230068164A1

## CPC

- C22C 21/04: Modified aluminium-silicon alloys
- B22D 21/00: Casting non-ferrous metals or metallic compounds so far as their metallurgical properties are of importance for the casting procedure; Selection of compositions therefor {(non-ferrous ingots B22D7/005)}
- B22D 21/04: Casting aluminium or magnesium {(no material; see B22D21/007)}
- C22C 21/02: with silicon as the next major constituent
- C22F 1/043: of alloys with silicon as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

New 3xx aluminum casting alloys are disclosed. The aluminum casting alloys generally include from 6.5 to 11.0 wt. % Si, from 0.20 to 0.80 wt. % Mg, from 0.05 to 0.50 wt. % Cu, from 0.10 to 0.80 wt. % Mn, from 0.005 to 0.05 wt. % Sr, up to 0.25 wt. % Ti, up to 0.30 wt. % Fe, and up to 0.20 wt. % Zn, the balance being aluminum and impurities.

## Claims

### Claim 1

A method, comprising:
(a) shape casting a 3 xx aluminum casting alloy into a shape cast product, wherein the 3 xx aluminum casting alloy comprises:
6.5-11.0 wt. % Si;
0.20-0.80 wt. % Mg;
0.05-0.50 wt. % Cu;
0.10-0.80 wt. % Mn;
0.005-0.050 wt. % Sr;
up to 0.25 wt. % Ti;
up to 0.30 wt. % Fe; and
up to 0.20 wt. % Zn;
the balance being aluminum (Al) and impurities, wherein the 3 xx aluminum casting alloy includes not greater than 0.10 wt. % of any one impurity, and wherein the 3 xx aluminum casting alloy includes not greater than 0.35 wt. %, in total, of the impurities,
wherein the shape casting step is selected from the group consisting of: high pressure die casting, gravity permanent mold casting, semi-permanent mold casting, squeeze casting, sand mold casting, centrifugal casting, and ablation casting;
(b) optionally machining the shape cast product;
(c) tempering the shape cast product, wherein, due to the tempering, the shape cast product is in a T temper.

### Claim 2 (depends on 1)

The method of claim 1, wherein the T temper is selected from the group consisting of: T4, T5, T6, and T7 tempers.

### Claim 3 (depends on 1)

The method of claim 1, wherein the shape cast product is an automotive product.