# US 2023/0067691 A1 · Negative electrode active material, negative electrode including the same and lithium secondary battery including the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067691 A1
- Document ID: US20230067691A1
- Status: Published application
- Kind: A1
- Application number: 17/983,280
- Filed: 2022-11-08
- Published: 2023-03-02
- Earliest claimed: 2018-01-31
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Sun-Young SHIN; Dong-Hyuk KIM; Yong-Ju LEE; Rae-Hwan JO; Je-Young KIM
- Web page: https://patentgrep.com/patent/US20230067691A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- C01B 33/02: Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B)
- C01B 33/113: Silicon oxides; Hydrates thereof {(preparing monoxide by reduction of siliceous material C01B33/182)}
- C01B 33/24: Alkaline-earth metal silicates
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/364: {as mixtures}
- H01M 4/366: {as layered products}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Disclosed is a negative electrode active material which includes: a silicon oxide composite including i) Si, ii) a silicon oxide represented by SiOx (0 < x ≤ 2), and iii) magnesium silicate containing Si and Mg; and a carbon coating layer positioned on the surface of the silicon oxide composite and including a carbonaceous material, wherein X-ray diffractometry of the negative electrode active material shows peaks of Mg2SiO4 and MgSiO3 at the same time and shows no peak of MgO; the ratio of peak intensity, I (Mg2SiO4)/I (MgSiO3), which is intensity I (Mg2SiO4) of peaks that belong to Mg2SiO4 to intensity I (MgSiO3) of peaks that belong to MgSiO3 is smaller than 1, the peaks that belong to Mg2SiO4 are observed at 2θ = 32.2 ± 0.2°, and the peaks that belong to MgSiO3 are observed at 2θ = 30.9 ± 0.2°.

## Claims

### Claim 1 (depends on 1)

A method for preparing the negative electrode active material according to claim 1, comprising:
carrying out a reaction of SiOx (0 < x < 2) gas with Mg gas,
cooling the reaction mixture at 400-900° C. and depositing a silicon oxide composite;
pulverizing the deposited silicon oxide composite; and
injecting a carbonaceous material gas into the pulverized silicon oxide composite and carrying out a heat treatment at 800-1,150° C. for 30 minutes to 8 hours to form a carbonaceous material-containing coating layer on a surface of the silicon oxide composite.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the SiOx (0 < x < 2) gas is prepared by evaporating a mixture of Si and SiO2 at 1,000-1,800° C., and the Mg gas is prepared by evaporating Mg at 800-1,600° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the reaction of the SiOx (0 < x < 2) gas with the Mg gas is carried out at 800-1,800° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, in injecting a carbonaceous material gas, the carbonaceous material gas is injected to the pulverized silicon oxide composite, and then the heat treatment is carried out at 900-1,050° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the reaction mixture is cooled at 500-800° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the cooling is conducted for 1-6 hours.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the heat treatment is conducted at 900-1,050° C. to form the carbonaceous material-containing coating layer.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the heat treatment is conducted at 950-1,000° C. to form the carbonaceous material-containing coating layer.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the heat treatment is conducted at a rate of 3-10° C. /min to form the carbonaceous material-containing coating layer.