# US 2023/0067641 A1 · Display substrate and manufacturing method thereof, and display apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067641 A1
- Document ID: US20230067641A1
- Status: Published application
- Kind: A1
- Application number: 17/626,708
- Filed: 2020-11-24
- Published: 2023-03-02
- Earliest claimed: 2020-11-24
- Assignees: Chengdu Boe Optoelectronics Technology Co., Ltd.; Boe Technology Group Co., Ltd.
- Applicants: Chengdu Boe Optoelectronics Technology Co., Ltd.; Boe Technology Group Co., Ltd.
- Inventors: Cheng ZENG; Jaeho LEE; Myoungsoo LEE; Xuemei CUI; Ruitao LI; Shiqi LI; Zhen SUN; Lulin MA
- Web page: https://patentgrep.com/patent/US20230067641A1

## CPC

- H10K 59/873: {Encapsulations}
- H10K 59/879: {comprising refractive means, e.g. lenses}
- H10K 59/80: Constructional details
- H10K 59/8731: {multilayered coatings having a repetitive structure, e.g. having multiple organic-inorganic bilayers}
- H10K 59/876: {comprising a resonant cavity structure, e.g. Bragg reflector pair}
- H10K 2101/00: Properties of the organic materials covered by group H10K85/00
- H10K 2102/00: Constructional details relating to the organic devices covered by this subclass
- H10K 2102/351: {Thickness}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES

## Abstract

A display substrate includes a backplane, first light-emitting devices capable of emitting first color light, second light-emitting devices capable of emitting second color light that are all disposed on the backplane, a low-refractive-index intercalation layer disposed at a side, away from the backplane, of the first light-emitting devices and the second light-emitting devices, and an encapsulation layer. The encapsulation layer includes a first inorganic barrier layer, a first organic barrier layer and a second inorganic barrier layer that are sequentially stacked on a side of the low-refractive-index intercalation layer away from the backplane. A refractive index of the low-refractive-index intercalation layer is less than a refractive index of the first inorganic barrier layer. In a direction perpendicular to the backplane, a transmittance of the low-refractive-index intercalation layer to the first color light is less than a transmittance of the low-refractive-index intercalation layer to the second color light.

## Claims

### Claim 1

A display substrate, comprising:
a backplane;
first light-emitting devices capable of emitting first color light and second light-emitting devices capable of emitting second color light that are disposed on the backplane;
a low-refractive-index intercalation layer disposed at a side, away from the backplane, of the first light-emitting devices and the second light-emitting devices; and
an encapsulation layer including a first inorganic barrier layer, a first organic barrier layer and a second inorganic barrier layer that are sequentially stacked on a side of the low-refractive-index intercalation layer away from the backplane;
wherein a refractive index of the low-refractive-index intercalation layer is less than a refractive index of the first inorganic barrier layer; and in a direction perpendicular to the backplane, a transmittance of the low-refractive-index intercalation layer to the first color light is less than a transmittance of the low-refractive-index intercalation layer to the second color light.

### Claim 2 (depends on 1)

The display substrate according to claim 1, further comprising:
third light-emitting devices capable of emitting third color light disposed on the backplane, in the direction perpendicular to the backplane, the transmittance of the low-refractive-index intercalation layer to the first color light being less than a transmittance of the low-refractive-index intercalation layer to the third color light.

### Claim 3 (depends on 1)

The display substrate according to claim 1, wherein the refractive index of the low-refractive-index intercalation layer is in a range from 1.45 to 1.73, inclusive; and a thickness of the low-refractive-index intercalation layer is in a range from 0.03 μm to 0.10 μm, inclusive.

### Claim 4 (depends on 1)

The display substrate according to claim 1, wherein a material of the low-refractive-index intercalation layer includes silicon oxide and silicon oxynitride, a ratio of the silicon oxide to the silicon oxynitride is in a range from 0.001 to 0.1, inclusive.

### Claim 5 (depends on 1)

The display substrate according to claim 1, wherein a sum of a thickness of the first inorganic barrier layer and a thickness of the low-refractive-index intercalation layer is less than or equal to 1.1 μm.

### Claim 6 (depends on 1)

The display substrate according to claim 1, wherein a thickness of the low-refractive-index intercalation layer is less than a thickness of the first inorganic barrier layer.

### Claim 7 (depends on 6)

The display substrate according to claim 6, wherein the thickness of the low-refractive-index intercalation layer is in a range from 0.03 μm to 0.10 μm, inclusive; and the thickness of the first inorganic barrier layer is in a range from 1.0 μm to 1.07 μm, inclusive.

### Claim 8 (depends on 1)

The display substrate according to claim 1, further comprising:
a light extraction layer disposed at the side, away from the backplane, of the first light-emitting devices and the second light-emitting devices, and the light extraction layer being located on a side of the low-refractive-index intercalation layer proximate to the backplane, wherein
a refractive index of the light extraction layer is greater than the refractive index of the low-refractive-index intercalation layer.

### Claim 9 (depends on 8)

The display substrate according to claim 8, wherein the refractive index of the low-refractive-index intercalation layer is in a range from 1.45 to 1.63, inclusive; and the refractive index of the light extraction layer is in a range from 1.8 to 2.0, inclusive.

### Claim 10 (depends on 1)

The display substrate according to claim 1, wherein the display substrate has a plurality of sub-pixel areas; each sub-pixel area is provided with a light-emitting device of the first light-emitting devices and the second light-emitting devices therein, and the light-emitting device includes a cathode layer; and
the low-refractive-index intercalation layer is in direct contact with the cathode layer.

### Claim 11 (depends on 10)

The display substrate according to claim 10, wherein the refractive index of the low-refractive-index intercalation layer is in a range from 1.47 to 1.73, inclusive; and a thickness of the low-refractive-index intercalation layer is in a range from 0.05 μm to 0.10 μm, inclusive.

### Claim 12 (depends on 1)

The display substrate according to claim 1, wherein the encapsulation layer further includes a second organic barrier layer and a third inorganic barrier layer that are sequentially stacked on a side of the second inorganic barrier layer away from the backplane.

### Claim 13 (depends on 1)

The display substrate according to claim 1, wherein the refractive index of the first inorganic barrier layer is in a range from 1.75 to 1.85, inclusive.

### Claim 14 (depends on 1)

A display apparatus, comprising the display substrate according to claim 1.

### Claim 15

A manufacturing method of a display substrate, the manufacturing method comprising:
manufacturing a backplane;
forming first light-emitting devices capable of emitting first color light and second light-emitting devices capable of emitting second color light on the backplane;
forming a low-refractive-index intercalation layer at a side, away from the backplane, of the first light-emitting devices and the second light-emitting devices; and
forming an encapsulation layer on a side of the low-refractive-index intercalation layer away from the backplane, the encapsulation layer including a first inorganic barrier layer, a first organic barrier layer and a second inorganic barrier layer that are sequentially stacked on a side of the low-refractive-index intercalation layer away from the backplane;
wherein a refractive index of the low-refractive-index intercalation layer is less than a refractive index of the first inorganic barrier layer; and in a direction perpendicular to the backplane, a transmittance of the low-refractive-index intercalation layer to the first color light is less than a transmittance of the low-refractive-index intercalation layer to the second color light.

### Claim 16 (depends on 15)

The manufacturing method according to claim 15, wherein the low-refractive-index intercalation layer is formed at the side, away from the backplane, of the first light-emitting devices and the second light-emitting devices by using a first film deposition process; and
the first inorganic barrier layer is formed on the side of the low-refractive-index intercalation layer away from the backplane by using a second film deposition process.

### Claim 17 (depends on 16)

The manufacturing method according to claim 16, further comprising:
forming a light extraction layer at the side, away from the backplane, of the first light-emitting devices and the second light-emitting devices before forming the low-refractive-index intercalation layer.

### Claim 18 (depends on 17)

The manufacturing method according to claim 17, wherein a ratio of a power of electrodes used in the second film deposition process to a power of electrodes used in the first film deposition process is in a range from 1.1 to 1.15, inclusive.

### Claim 19 (depends on 2)

The display substrate according to claim 2, wherein the first color light is blue light, the second color light is one of red light and green light, and the third color light is another of red light and green light.

### Claim 20 (depends on 2)

The display substrate according to claim 2, wherein the first color light is green light, the second color light is one of red light and blue light, and the third color light is another of red light and blue light.