# US 2023/0067539 A1 · Semiconductor structure and formation thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067539 A1
- Document ID: US20230067539A1
- Status: Published application
- Kind: A1
- Application number: 17/458,711
- Filed: 2021-08-27
- Published: 2023-03-02
- Earliest claimed: 2021-08-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Limited
- Inventors: Kai-Lan CHANG; Yu-Lung Yeh; Yen-Hsiu Chen; Shuo Yen Tai; Yung-Hsiang Chen
- Web page: https://patentgrep.com/patent/US20230067539A1

## CPC

- B81B 7/0041: {maintaining a controlled atmosphere with techniques not provided for in B81B7/0038}
- B81C 1/00333: {Aspects relating to packaging of MEMS devices, not covered by groups B81C1/00269 - B81C1/00325}
- B81B 7/0058: {for protecting against damages due to external chemical or mechanical influences, e.g. shocks or vibrations}
- B81B 2201/0264: Pressure sensors
- B81B 2203/0315: Cavities
- B81B 2203/0353: Holes
- B81B 2207/015: the micromechanical device and the control or processing electronics being integrated on the same substrate
- B81C 2203/0136: Growing or depositing of a covering layer
- B81C 2203/0145: Hermetically sealing an opening in the lid
- B81C 2203/0735: Post-CMOS, i.e. forming the micromechanical structure after the CMOS circuit
- B81C 2203/0771: Stacking the electronic processing unit and the micromechanical structure
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)

## Abstract

A method is provided that includes forming a first metal layer of a seal structure over a micro-electromechanical system (MEMS) structure and over a channel formed through the MEMS structure to an integrated circuit of a semiconductor structure. The first metal layer is formed at a first temperature. The method includes forming a second metal layer over the first metal layer. The second metal layer is formed at a second temperature less than the first temperature. The method includes performing a first cooling process to cool the semiconductor structure.

## Claims

### Claim 1

A method, comprising:
forming a first metal layer of a seal structure over a micro-electromechanical system (MEMS) structure and over a channel formed through the MEMS structure to an integrated circuit of a semiconductor structure, wherein the first metal layer is formed at a first temperature;
forming a second metal layer over the first metal layer, wherein the second metal layer is formed at a second temperature less than the first temperature; and
performing a first cooling process to cool the semiconductor structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming the first metal layer comprises:
cooling the semiconductor structure with a cooling gas.

### Claim 3 (depends on 2)

The method of claim 2, wherein the cooling gas comprises argon.

### Claim 4 (depends on 1)

The method of claim 1, wherein:
forming the first metal layer comprises performing a first sputter process with a first sputter power;
forming the second metal layer comprises performing a second sputter process with a second sputter power; and
the first sputter power is less than the second sputter power.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first metal layer has a resistivity between about 2.00E-08 Ω·m to about 4.00E-08 Ω·m.

### Claim 6 (depends on 1)

The method of claim 1, wherein the second metal layer has a resistivity between about 1.00E-07 Ω·m to about 1.00E-06 Ω·m.

### Claim 7 (depends on 1)

The method of claim 1, comprising:
forming a third metal layer over the second metal layer, wherein the third metal layer is formed at a third temperature greater than the second temperature.

### Claim 8 (depends on 7)

The method of claim 7, wherein:
forming the first metal layer comprises performing a first sputter process with a first sputter power;
forming the third metal layer comprises performing a second sputter process with a second sputter power; and
the first sputter power is less than the second sputter power.

### Claim 9 (depends on 7)

The method of claim 7, comprising:
forming a fourth metal layer over the third metal layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein:
forming the first metal layer comprises performing a first sputter process with a first sputter power;
forming the fourth metal layer comprises performing a second sputter process with a second sputter power; and
the first sputter power is less than the second sputter power.

### Claim 11 (depends on 9)

The method of claim 9, comprising:
performing a second cooling process to cool the semiconductor structure after forming the fourth metal layer.

### Claim 12

A method, comprising:
performing a first sputter process with a first sputter power to form a first metal layer of a seal structure over a micro-electromechanical system (MEMS) structure and over a channel formed through the MEMS structure to an integrated circuit of a semiconductor structure;
performing a second sputter process with a second sputter power greater than the first sputter power to form a second metal layer over the first metal layer; and
performing a first cooling process to cool the semiconductor structure.

### Claim 13 (depends on 12)

The method of claim 12, wherein performing the first sputter process comprises performing the first sputter process at a first temperature between about 200 degrees Celsius to about 300 degrees Celsius.

### Claim 14 (depends on 13)

The method of claim 13, wherein performing the second sputter process comprises performing the second sputter process at a second temperature between about 200 degrees Celsius to about 250 degrees Celsius.

### Claim 15 (depends on 12)

The method of claim 12, comprising:
forming one or more additional metal layers over the second metal layer.

### Claim 16 (depends on 15)

The method of claim 15, comprising:
performing a second cooling process to cool the semiconductor structure after forming the one or more additional metal layers.

### Claim 17

A semiconductor structure, comprising:
an integrated circuit;
a micro-electromechanical system (MEMS) structure, wherein a channel is formed through the MEMS structure to the integrated circuit; and
a seal structure over the channel, wherein the seal structure comprises a first metal layer and a second metal layer over the first metal layer, wherein the first metal layer has a first resistivity different than a second resistivity of the second metal layer.

### Claim 18 (depends on 17)

The semiconductor structure of claim 17, wherein the seal structure comprises a third metal layer over the second metal layer, and wherein a grain of the first metal layer is larger than a grain of the third metal layer.

### Claim 19 (depends on 17)

The semiconductor structure of claim 17, wherein the first metal layer has a first region height to second region height ratio less than 0.25 over the channel.

### Claim 20 (depends on 17)

The semiconductor structure of claim 17, wherein the first resistivity is between about 2.00E-08 Ω·m to about 4.00E-08 Ω·m and the second resistivity is between about 1.00E-07 Ω·m to about 1.00E-06 Ω·m.