# US 2023/0067524 A1 · Method for making a friction material, in particular for making brake pads and relative brake pads

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067524 A1
- Document ID: US20230067524A1
- Status: Published application
- Kind: A1
- Application number: 17/794,238
- Filed: 2021-01-20
- Published: 2023-03-02
- Earliest claimed: 2020-01-20
- Assignees: ITT ITALIA S.r.I.
- Applicants: ITT Italia S.r.I.
- Inventors: Agustin Sin Xicola; Francesco Vannucci; Paolo Colombo; Alberto Conte; Luca Martinotto
- Web page: https://patentgrep.com/patent/US20230067524A1

## CPC

- B28B 1/14: by simple casting, the material being neither forcibly fed nor positively compacted (for molten material B28B1/54)
- B28B 11/24: for curing, setting or hardening (processes for influencing or modifying the setting or hardening ability of mortars, concrete or artificial stone compositions, in general C04B40/00)
- C04B 12/005: {Geopolymer cements, e.g. reaction products of aluminosilicates with alkali metal hydroxides or silicates}
- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- F16D 65/092: for axially-engaging brakes, e.g. disc brakes
- F16D 69/028: {containing fibres}
- C04B 2111/00362: {Friction materials, e.g. used as brake linings, anti-skid materials}
- F16D 2200/0043: Ceramic base, e.g. metal oxides or ceramic binder
- F16D 2200/0065: Inorganic, e.g. non-asbestos mineral fibres
- F16D 2250/0007: Casting
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Method for producing a friction material, including the following steps in sequence: mixing an aluminosilicate source with an alkaline silicate solution to form a geopolymer, adding a friction mix to the geopolymer solution of the previous step to obtain a slurry, casting the slurry in a mold at temperature between room temperature and 120° C. and for between 5 min and 2 h and demolding to obtain a pad, attaching a backplate to the pad, curing for a time between X and Y hours at a temperature of between X and Y. The friction material obtained with the method is for the manufacture of friction layers/blocks for friction elements such as braking elements, including vehicle brake pads or blocks, and/or friction discs.

## Claims

### Claim at position 1

1-9. (canceled)

### Claim 10

A method for making a braking element, in particular a brake pad, including the following steps, in sequence:
a) mixing an aluminosilicate source with an alkaline silicate solution to form a geopolymeric solution;
b) adding a friction mix to the geopolymeric solution of the previous mixing step to obtain a slurry;
c) casting the slurry in a mold at a temperature between room temperature and 120° C. and maintaining the slurry inside the hot mold for a time comprised between 5 minutes and 2 hours until the slurry is substantially solidified;
d) demolding the solidified slurry to obtain a pad or block of solid friction material;
e) attaching a backplate to the pad or block of solid friction material either as a consequence of the casting step or after the pad or block of solid friction material is demolded; and
f) curing for a time between 1 and 24 hours and at a temperature of between 60° C. and 120° C. the pad or block of solid friction material having the backplate attached to it.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the aluminosilicate source is chosen from the group consisting of metakaolin, kaolin or fly ash or bottom ash and their mixtures.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the aluminosilicate source comprises metakaolin.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the alkaline silicate solution is chosen from the group consisting of sodium silicate and sodium hydroxide system, potassium hydroxide and potassium silicate system, lithium hydroxide and lithium silicate system, cesium hydroxide and cesium silicate system, and rubidium hydroxide and rubidium silicate system and their mixtures.

### Claim 14 (depends on 10)

The method according to claim 10, wherein the friction mix comprises:
fibers chosen in the group consisting of organic, inorganic or metallic fiber and their mixture and added in a quantity comprised between 2% in volume and 30% in volume out of the total volume of friction material
organic or inorganic fillers added in a quantity comprised between 2% to 40% in volume based on the total composition of the friction material; and
friction modifier added in a quantity between 4% and 30% of the entire volume of friction material.

### Claim 15 (depends on 10)

The method according to claim 10, wherein the fillers are chosen from the group consisting of calcium carbonate, barium sulphate, magnesium oxide, calcium hydroxide, calcium fluoride, slaked lime, talc, mica and their mixtures.

### Claim 16 (depends on 10)

The method according to claim 10, wherein the aluminosilicate source and the alkaline silicate in step a) are chosen so that the SiO2/Al2O3 molar ratio in the final friction material is between 3 and 5.

### Claim 17 (depends on 10)

The method according to claim 10, wherein the alkaline silicate solution in step a) is chosen so that the SiO2/R2O molar ratio in the final friction material is between 0.7 and 1.5 and where R is chosen among Na, K, Li.

### Claim 18 (depends on 10)

The method according to claim 10, wherein the solution in step a) is chosen so that the H2O/Al2O3 molar ratio is between 10 and 25.