# US 2023/0067466 A1 · Physical vapor deposition process apparatus and method of optimizing thickness of a target material film deposited using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067466 A1
- Document ID: US20230067466A1
- Status: Published application
- Kind: A1
- Application number: 17/462,769
- Filed: 2021-08-31
- Published: 2023-03-02
- Earliest claimed: 2021-08-31
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chen-Hung LIN; Ya-Chin CHIU; Ming-Hsien LIN
- Web page: https://patentgrep.com/patent/US20230067466A1

## CPC

- H10P 74/238: {comprising acting in response to an ongoing measurement without interruption of processing, e.g. endpoint detection or in-situ thickness measurement}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/543: {using measurement on the vapor source}
- C23C 14/545: {using measurement on deposited material}
- H01J 37/3402: {using supplementary magnetic fields}
- H01J 37/3426: {Material}
- H01J 37/3455: {Movable magnets}
- H01J 37/3479: {Detecting exhaustion of target material}
- H10P 14/44: Physical vapour deposition [PVD]
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/185: {by cathodic sputtering}
- H01J 2237/24564: Measurements of electric or magnetic variables, e.g. voltage, current, frequency
- H01J 2237/3323: uniformity
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments are directed to a method of optimizing thickness of a target material film deposited on a semiconductor substrate in a semiconductor processing chamber, wherein the semiconductor processing chamber includes a magnetic assembly positioned on the semiconductor processing chamber, the magnetic assembly including a plurality of magnetic columns within the magnetic assembly. The method includes operating the semiconductor processing chamber to deposit a film of target material on a semiconductor substrate positioned within the semiconductor processing chamber, measuring an uniformity of the deposited film, adjusting a position of one or more magnetic columns in the magnetic assembly, and operating the semiconductor processing chamber to deposit the film of the target material after adjusting position of the one or more magnetic columns.

## Claims

### Claim 1

A method of optimizing thickness of a target material film deposited on a semiconductor substrate in a semiconductor processing chamber, wherein the semiconductor processing chamber includes a magnetic assembly positioned on the semiconductor processing chamber, the magnetic assembly including a plurality of magnetic columns within the magnetic assembly, the method comprising:
operating the semiconductor processing chamber to deposit a film of target material on a semiconductor substrate positioned within the semiconductor processing chamber;
measuring an uniformity of the deposited film;
adjusting a position of one or more magnetic columns in the magnetic assembly; and
operating the semiconductor processing chamber to deposit the film of the target material after adjusting position of the one or more magnetic columns.

### Claim 2 (depends on 1)

The method of claim 1, wherein adjusting the position includes stopping an operation of the semiconductor processing chamber, and
removing the one or more magnetic columns from the magnetic assembly.

### Claim 3 (depends on 1)

The method of claim 1, wherein adjusting the position includes stopping an operation of the semiconductor processing chamber, and
moving the one or more magnetic columns of the magnetic assembly along a direction away from a target material arranged in the semiconductor processing chamber.

### Claim 4 (depends on 1)

The method of claim 1, wherein the uniformity of the deposited film is measured by measuring a resistivity of the deposited film at different regions of the semiconductor substrate to determine a thickness of the film deposited in each of the different regions of the semiconductor substrate.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
decreasing a spacing between the target material and the semiconductor substrate; and
operating the semiconductor processing chamber to deposit the film of the target material after decreasing the spacing and after removing two or more magnetic columns from the magnetic assembly.

### Claim 6 (depends on 5)

The method of claim 5, wherein the spacing is decreased to around 53 mm from around 60 mm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the film of target material includes titanium nitride (TiN) having a resistivity variation of 1% and a resistivity of less than 10 μΩ-cm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the plurality of magnetic columns include permanent magnetic material.

### Claim 9 (depends on 1)

The method of claim 1, wherein the film of target material includes a material selected from the group consisting of aluminum (Al), copper (Cu), tungsten (W), molybdenum (Mo), tantalum (Ta), titanium (Ti), tantalum nitride (TaN), tungsten nitride (W2N, WN, or WN2), titanium nitride (TiN), aluminum nitride (AlN), and scandium aluminum nitride (ScAlN or ScxAlxN).

### Claim 10

A method of manufacturing a semiconductor device using a semiconductor processing chamber, wherein the semiconductor processing chamber includes: a magnetic assembly including a plurality of magnetic columns positioned on the semiconductor processing chamber, the method comprising:
monitoring an erosion of a target material in the semiconductor processing chamber and a thickness of a film of the target material deposited on a semiconductor substrate positioned in the semiconductor processing chamber;
when the erosion uniformity of the target material and/or the thickness uniformity of the deposited film exceeds a corresponding threshold, removing three magnetic columns from the magnetic assembly such that the target material is eroded in a substantially uniform manner and a film having a substantially uniform thickness is deposited on the semiconductor substrate; and
performing a semiconductor manufacturing process on the semiconductor substrate using the magnetic assembly after the removing three magnetic columns.

### Claim 11 (depends on 10)

The method of claim 10, further comprising:
decreasing a spacing between the target material and the semiconductor substrate; and
performing the semiconductor manufacturing process to deposit the film of the target material after decreasing the spacing.

### Claim 12 (depends on 11)

The method of claim 11, wherein the spacing is decreased to around 53 mm from around 60 mm.

### Claim 13 (depends on 12)

The method of claim 12, wherein the film of target material includes titanium nitride (TiN) having a resistivity variation of 1% and a resistivity of less than 10 μΩ-cm.

### Claim 14 (depends on 10)

The method of claim 10, wherein the semiconductor manufacturing operation includes a deposition operation or an etching operation.

### Claim 15 (depends on 10)

The method of claim 10, wherein the plurality of magnets include permanent magnets.

### Claim 16 (depends on 10)

The method of claim 10, wherein removing three magnetic columns of the plurality of magnetic columns from the magnetic assembly includes removing three magnetic columns such that a magnetic flux density due to the plurality of magnets is substantially uniform.

### Claim 17 (depends on 10)

The method of claim 10, wherein the plurality of magnetic columns are arranged in two or more groups, and removing three magnetic columns of the plurality of magnetic columns includes removing magnetic columns from one or more groups.

### Claim 18

A method, comprising:
measuring a magnetic field formed by a plurality of magnets in a magnetic assembly positioned over a vacuum chamber in which a target is placed, and the magnetic assembly includes a plurality of magnets;
adjusting positions of one or more magnets along a direction away from the target; and
performing a sputtering operation on a semiconductor substrate using the target.

### Claim 19 (depends on 18)

The method of claim 18, wherein the positions of the one or more magnets are adjusted based on a thickness of a film of the target deposited on the semiconductor substrate.

### Claim 20 (depends on 18)

The method of claim 18, wherein the positions of the one or more magnets are adjusted such that a substantially uniform magnetic field is generated.