# US 2023/0067295 A1 · Magnetoresistive element having a nano-current-channel sturcture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067295 A1
- Document ID: US20230067295A1
- Status: Published application
- Kind: A1
- Application number: 17/460,189
- Filed: 2021-08-28
- Published: 2023-03-02
- Earliest claimed: 2021-08-28
- Inventors: YIMIN GUO; RONGFU XIAO; JUN CHEN
- Web page: https://patentgrep.com/patent/US20230067295A1

## CPC

- H10N 50/80: Constructional details
- G11C 11/161: {details concerning the memory cell structure, e.g. the layers of the ferromagnetic memory cell}
- H01F 10/3268: {the exchange coupling being asymmetric, e.g. by use of additional pinning, by using antiferromagnetic or ferromagnetic coupling interface, i.e. so-called spin-valve [SV] structure, e.g. NiFe/Cu/NiFe/FeMn}
- H01F 10/3286: {Spin-exchange coupled multilayers having at least one layer with perpendicular magnetic anisotropy}
- H01F 10/329: {Spin-exchange coupled multilayers wherein the magnetisation of the free layer is switched by a spin-polarised current, e.g. spin torque effect}
- H01F 41/32: for applying conductive, insulating or magnetic material on a magnetic film {, specially adapted for a thin magnetic film}
- H10N 50/01: Manufacture or treatment
- G11C 11/1675: {Writing or programming circuits or methods}
- H01F 10/3259: {Spin-exchange-coupled multilayers comprising at least a nanooxide layer [NOL], e.g. with a NOL spacer}
- H10B 61/20: {comprising components having three or more electrodes, e.g. transistors}
- H10N 50/85: Materials of the active region
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A magnetoresistive element comprises a nonmagnetic nano-current-channel (NCC) structure provided on a surface of the magnetic recording layer, which is opposite to a surface of the magnetic recording layer where the tunnel barrier layer is provided, and comprising a spatial distribution of perpendicular conducting channels throughout the NCC structure thickness and surrounded by an insulating medium, making the magnetic recording layer a magnetically soft-hard composite structure. Correspondingly, the critical write current and write power are reduced with reversal modes of exchange-spring magnets of the magnetically soft-hard composite structure.

## Claims

### Claim 1

A magnetoresistive element comprising:
a magnetic reference layer having a reference layer magnetization fixed in a direction perpendicular to the magnetic reference layer;
a tunnel barrier layer provided on a surface of the reference layer;
a magnetic recording layer provided on a surface of the tunnel barrier layer, which is opposite to a surface of the tunnel barrier layer where the magnetic reference layer is provided, and having a recording layer magnetization that is perpendicular to the magnetic recording layer and is changeable relative to the reference layer magnetization;
a nonmagnetic nano-current-channel (NCC) structure provided on a surface of the magnetic recording layer, which is opposite to a surface of the magnetic recording layer where the tunnel barrier layer is provided, and comprising a spatial distribution of perpendicular conducting channels throughout the NCC structure thickness and surrounded by an insulating medium; and
a cap layer provided on a surface of the NCC structure, which is opposite to a surface of the NCC structure where the magnetic recording layer is provided;
wherein said tunnel barrier layer has a first resistance-area product (RA1), each of said perpendicular conducting channels is electrically conductive in a perpendicular direction between said magnetic recording layer and said cap layer and has a second resistance-area product (RA2), said insulating medium comprises at least one oxide layer and is less electrically conductive in a perpendicular direction between said magnetic recording layer and said cap layer than each of said perpendicular conducting channels and has a third resistance-area product (RA3), and said magnetic recording layer has channeled regions which directly contact said perpendicular conducting channels of said NCC structure, and non-channeled regions which directly contact said insulating medium of said NCC structure.

### Claim 2 (depends on 1)

The element of claim 1, wherein each of said channeled regions of said magnetic recording layer has a lower perpendicular magnetic anisotropy (PMA) than said non-channeled regions of said magnetic recording layer.

### Claim 3 (depends on 1)

The element of claim 1, wherein said second resistance-area product (RA2) is no more than 15% of said first resistance-area product (RA1), and said third resistance-area product (RA3) is at least 25% of said first resistance-area product (RA1).

### Claim 4 (depends on 1)

The element of claim 1, wherein said third resistance-area product (RA3) is at least 5 times said first resistance-area product (RA1).

### Claim 5 (depends on 1)

The element of claim 1, wherein the total area of said channeled regions of said magnetic recording layer is at least one third of the total area of said magnetic recording layer.

### Claim 6 (depends on 1)

The element of claim 1, wherein each of said perpendicular conducting channels comprises at least one layer of transition metal or conductive transition metal oxide, preferred to be Cu, Mo, W, Pt, Ru, Au, Ag, Ru, Rh, Ir, Os, Re, or alloy thereof, or oxide thereof.

### Claim 7 (depends on 6)

The element of claim 6, wherein each of said perpendicular conducting channels further comprises at least one layer of oxide or nitride, preferred to be selected from the group consisting of Al2O3, HfO2, ZrO2, TiO2, SiO2, Y2O3, RuO, OsO, TcO, ReO, CoO, NiO, BeO, SiN, RuN, OsN, TcN, ReN.

### Claim 8 (depends on 6)

The element of claim 6, wherein each of said perpendicular conducting channels further comprises at least one layer of rocksalt crystalline metal oxide, preferred to be selected from the group consisting of NiO, CoO, FeO, FeCoO2, NiFeO2, CoNiO2, MnO, CrO, VO, TiO, MgO, MgAl2O4, MgZnO, ZnO and CdO.

### Claim 9 (depends on 6)

The element of claim 6, wherein each of said perpendicular conducting channels further comprises a first layer of metal oxide or metal nitride, and a second layer of metal oxide or metal nitride, that sandwich at least one layer of said transition metal or said conductive transition metal oxide.

### Claim 10 (depends on 1)

The element of claim 1, wherein said insulating medium comprises at least one layer of oxide or nitride, preferred to be selected from the group consisting of Al2O3, HfO2, ZrO2, TiO2, SiO2, Y2O3, RuO, OsO, TcO, ReO, CoO, NiO, BeO, SiN, RuN, OsN, TcN, ReN.

### Claim 11 (depends on 1)

The element of claim 1, wherein said insulating medium comprises at least one layer of rocksalt crystalline metal oxide, preferred to be selected from the group consisting of NiO, CoO, FeO, FeCoO2, NiFeO2, CoNiO2, MnO, CrO, VO, TiO, MgO, MgAl2O4, MgZnO, ZnO and CdO.

### Claim 12 (depends on 1)

The element of claim 1, wherein said magnetic recording layer comprises at least one ferromagnetic layer selected from the group consisting of CoFe, Fe, Co, CoFeB, CoB and FeB, the B composition percentage is no more than 35%.

### Claim 13 (depends on 1)

The element of claim 1, further comprising an assisting magnetic layer between said NCC structure and said cap layer, said assisting magnetic layer comprising at least one of an iron (Fe) layer, a cobalt (Co) layer, an alloy layer of cobalt iron (CoFe), an alloy layer of iron boron (FeB), an alloy layer of cobalt boron (CoB), an alloy layer of cobalt iron boron (CoFeB), an alloy layer of cobalt nickel iron (CoNiFe), an alloy layer of cobalt nickel (CoNi), an alloy layer of iron platinum (FePt), an alloy layer of iron palladium (FePd), an alloy layer of iron nickel (FeNi), a laminated layer of (Fe/Co)n, a laminated layer of (Fe/CoFe)n, a laminated layer of (Fe/Pt)n, a laminated layer of (Fe/Pd)n and a laminated layer of (Fe/Ni)n, wherein n is a lamination number, and the B composition percentage is no more than 35%.

### Claim 14 (depends on 1)

The element of claim 1, wherein said NCC structure has a thickness of no more than 20 angstroms.

### Claim 15 (depends on 1)

The element of claim 1, further comprising an upper electrode and a lower electrode which sandwich said magnetoresistive element, and further comprising a write circuit which bi-directionally supplies a current to said magnetoresistive element, and a select transistor electrically connected between said magnetoresistive element and said write circuit.

### Claim 16

A method of manufacturing a perpendicular magnetic tunnel junction (pMTJ) element for being used in a magnetic memory device comprising the steps of:
forming a magnetic reference layer;
forming a tunnel barrier layer atop the magnetic reference layer;
forming a magnetic recording layer atop the tunnel barrier layer;
forming a nonmagnetic nano-current-channel (NCC) structure atop the magnetic recording layer and comprising a spatial distribution of perpendicular conducting channels throughout the NCC structure thickness and surrounded by an insulating medium; and
forming a metal cap layer atop the oxide cap layer,
wherein said tunnel barrier layer has a first resistance-area product (RA1), each of said perpendicular conducting channels is electrically conductive in a perpendicular direction between said magnetic recording layer and said cap layer and has a second resistance-area product (RA2), said insulating medium comprises at least one oxide layer and is less electrically conductive in a perpendicular direction between said magnetic recording layer and said cap layer than each of said perpendicular conducting channels and has a third resistance-area product (RA3), and said magnetic recording layer has channeled regions which directly contact said perpendicular conducting channels of said NCC structure, and non-channeled regions which directly contact said insulating medium of said NCC structure.

### Claim 17 (depends on 16)

The element of claim 16, wherein each of said channeled regions of said magnetic recording layer has a lower perpendicular magnetic anisotropy (PMA) than said non-channeled regions of said magnetic recording layer.

### Claim 18 (depends on 16)

The element of claim 16, wherein forming of said NCC structure comprises sequential steps comprising of: forming a first thin metal oxide layer atop said magnetic recording layer, forming a discontinuous metal layer atop said first thin metal oxide layer, and forming a second thin metal oxide layer atop said discontinuous metal layer, wherein said first thin metal oxide layer is continuous and has a thickness of no more than 7.5 angstroms, said discontinuous metal layer is discontinuous and comprises at least one transition metal element selected from the group consisting of Cu, W, Pt, Ru, Au, Ag, Ru, Rh, Ir, Os and Re, at least one of said first thin metal oxide layer and said second thin metal oxide layer comprises one layer of rocksalt crystalline metal oxide, preferred to be selected from NiO, CoO, FeO, FeCoO2, NiFeO2, CoNiO2, MnO, CrO, VO, TiO, MgO, MgAl2O4, MgZnO, ZnO and CdO.

### Claim 19 (depends on 16)

The element of claim 16, wherein forming of said NCC structure comprises sequential steps comprising of: increasing the substrate temperature to a first temperature by a substrate heating, maintaining the substrate temperature at said first temperature, forming a discontinuous metal layer atop said recording layer, and forming a thin metal oxide layer atop said discontinuous metal layer, wherein said discontinuous metal layer is discontinuous and comprises at least one transition metal element selected from the group consisting of Mo, W, Pt, Ru, Au, Ag, Ru, Rh, Ir, Os and Re, said thin metal oxide layer comprises at least one layer of rocksalt crystalline metal oxide, preferred to be selected from NiO, CoO, FeO, FeCoO2, NiFeO2, CoNiO2, MnO, CrO, VO, TiO, MgO, MgAl2O4, MgZnO, ZnO and CdO, and has a thickness between 5 angstroms and 20 angstroms.

### Claim 20 (depends on 16)

The element of claim 16, further comprising forming of an assisting magnetic layer between forming of said NCC structure and forming of said cap layer, said assisting magnetic layer comprising at least one of an iron (Fe) layer, a cobalt (Co) layer, an alloy layer of cobalt iron (CoFe), an alloy layer of iron boron (FeB), an alloy layer of cobalt boron (CoB), an alloy layer of cobalt iron boron (CoFeB), an alloy layer of cobalt nickel iron (CoNiFe), an alloy layer of cobalt nickel (CoNi), an alloy layer of iron platinum (FePt), an alloy layer of iron palladium (FePd), an alloy layer of iron nickel (FeNi), a laminated layer of (Fe/Co)n, a laminated layer of (Fe/CoFe)n, a laminated layer of (Fe/Pt)n, a laminated layer of (Fe/Pd)n and a laminated layer of (Fe/Ni)n, wherein n is a lamination number, and the B composition percentage is no more than 35%.