# US 2023/0067288 A1 · Bipolar membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067288 A1
- Document ID: US20230067288A1
- Status: Published application
- Kind: A1
- Application number: 17/982,998
- Filed: 2022-11-08
- Published: 2023-03-02
- Earliest claimed: 2016-04-14
- Assignees: Astom Corporation
- Applicants: ASTOM Corporation
- Inventors: Masayuki KISHINO; Kouta YUZUKI; Kenji FUKUTA
- Web page: https://patentgrep.com/patent/US20230067288A1

## CPC

- B01D 61/445: {with bipolar membranes; Water splitting}
- B01D 61/46: Apparatus therefor
- B01D 67/0006: {by chemical reactions (in-situ polymerisation, polycondensation, cross-linking or reaction for manufacturing composite membranes B01D69/125)}
- B01D 69/02: characterised by their properties
- B01D 69/106: {Membranes in the pores of a support, e.g. polymerized in the pores or voids}
- B01D 69/1071: {Woven, non-woven or net mesh}
- B01D 69/1213: {Laminated layers}
- B01D 69/125: {In situ manufacturing by polymerisation, polycondensation, cross-linking or chemical reaction}
- B01D 71/26: Polyalkenes
- B01D 71/261: {Polyethylene}
- B01D 71/262: {Polypropylene}
- B01D 71/281: {Polystyrene}
- B01D 71/301: {Polyvinylchloride}
- B01D 71/82: characterised by the presence of specified groups, e.g. introduced by chemical after-treatment
- B01J 39/04: Processes using organic exchangers
- B01J 39/20: obtained by reactions only involving unsaturated carbon-to-carbon bonds
- B01J 41/04: Processes using organic exchangers
- B01J 41/14: obtained by reactions only involving unsaturated carbon-to-carbon bonds
- B01J 47/12: characterised by the use of ion-exchange material in the form of ribbons, filaments, fibres or sheets, e.g. membranes (electrodialysis or electro-osmosis B01D61/42)
- C08J 5/22: Films, membranes or diaphragms
- C08J 5/2231: {based on macromolecular compounds obtained by reactions involving unsaturated carbon-to-carbon bonds}
- C08J 5/2243: {obtained by introduction of active groups capable of ion-exchange into compounds of the type C08J5/2231}
- C08J 5/2275: {Heterogeneous membranes}
- C08J 5/2287: {After-treatment}
- C25B 13/02: characterised by shape or form
- C25B 13/08: based on organic materials
- B01D 2323/46: Impregnation
- B01D 2325/42: Ion-exchange membranes
- C08J 2325/06: Polystyrene
- C08J 2325/08: Copolymers of styrene (C08J2329/08, C08J2335/06, C08J2355/02 take precedence)
- C08J 2325/14: with unsaturated esters
- C08J 2325/18: Homopolymers or copolymers of aromatic monomers containing elements other than carbon and hydrogen
- C08J 2353/02: of vinyl aromatic monomers and conjugated dienes
- C08J 2423/06: Polyethene
- C08J 2423/12: Polypropene
- C08J 2427/06: Homopolymers or copolymers of vinyl chloride
- Y02E 60/50: Fuel cells
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A bipolar membrane in which a cation-exchange membrane and an anion-exchange membrane are joined to each other, wherein a leakage ratio of gluconic acid at 60° C. is not more than 1.0%, and the cation-exchange membrane is supported by a polyolefin reinforcing member and, further, contains a polyvinyl chloride.

## Claims

### Claim 1

A method of producing a bipolar membrane including a step of forming a cation-exchange membrane, and a step of forming an anion-exchange membrane on the surface of said cation-exchange membrane; wherein
the step of forming said cation-exchange membrane includes:
a step of impregnating a polyolefin reinforcing member with a polymerizable composition obtained by mixing a polyvinyl chloride (A) and a polymerization-curable component(B) that contains a monomer (b1) having a cation-exchange group or a monomer (b2) having a reaction group capable of introducing a cation-exchange group; and
a step of forming a membrane of a cation-exchange resin that contains the polyvinyl chloride or of a cation-exchange resin precursor resin by polymerization-curing said polymerizable composition at a temperature of not lower than 100° C.; and, further, as required,
a step of introducing a cation-exchange group into the cation-exchange resin precursor resin.

### Claim 2 (depends on 1)

The method of producing the bipolar membrane according to claim 1, further including:
a step of impregnating a polyolefin reinforcing member with the polymerizable composition obtained by mixing the polyvinyl chloride (A) and the monomer (b1) having a cation-exchange group; and
a step of forming a membrane of the cation-exchange resin that contains the polyvinyl chloride by the polymerization curing at a temperature of not lower than 100° C.

### Claim 3 (depends on 1)

The method of producing the bipolar membrane according to claim 1, further including:
a step of impregnating a polyolefin reinforcing member with the polymerizable composition obtained by mixing the polyvinyl chloride (A) and the monomer (b2) having a reaction group capable of introducing a cation-exchange group;
a step of forming the membrane of said cation-exchange resin precursor resin by the polymerization curing at a temperature of not lower than 100° C.; and
a step of introducing a cation-exchange group by acting a cation-exchange group introducing agent upon said cation-exchange resin precursor resin.

### Claim 4 (depends on 1)

The method of producing the bipolar membrane according to claim 1, wherein the step of forming the anion-exchange membrane on the surface of said cation-exchange membrane includes:
a step of applying a polar organic solvent solution of the anion-exchange resin on the surface of said cation-exchange membrane; and
a step of removing the polar organic solvent.

### Claim 5 (depends on 1)

The method of producing the bipolar membrane according to claim 1, wherein the step of forming the anion-exchange membrane on the surface of said cation-exchange membrane includes:
a step of applying, on the surface of said cation-exchange membrane, a polar organic solvent solution of an anion-exchange resin precursor resin having a reaction group capable of introducing the anion-exchange group;
a step of forming a membrane of said anion-exchange resin precursor resin on the surface of said cation-exchange membrane by removing the polar organic solvent; and
a step of introducing the anion-exchange group into said anion-exchange resin precursor resin.

### Claim 6 (depends on 1)

The method of producing the bipolar membrane according to claim 1, wherein the step of forming the anion-exchange membrane on the surface of said cation-exchange membrane includes:
a step of applying, on the surface of said cation-exchange membrane, a polar organic solvent solution that contains an anion-exchange resin precursor resin having a reaction group capable of introducing the anion-exchange group and an anion-exchange group introducing agent; and
a step of removing the polar organic solvent.