# US 2023/0067206 A1 · Aluminum alloy for casting high-strength and high electrically conductive components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067206 A1
- Document ID: US20230067206A1
- Status: Published application
- Kind: A1
- Application number: 17/462,536
- Filed: 2021-08-31
- Published: 2023-03-02
- Earliest claimed: 2021-08-31
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Qigui Wang; Margarita P. Thompson
- Web page: https://patentgrep.com/patent/US20230067206A1

## CPC

- C22C 21/08: with silicon
- C22F 1/047: of alloys with magnesium as the next major constituent
- H02K 15/023: Cage rotors
- H02K 17/20: having deep-bar rotors
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- H02K: DYNAMO-ELECTRIC MACHINES (dynamo-electric relays H01H53/00; conversion of DC or AC input power into surge output power {H03K3/53})

## Abstract

An electrically conductive aluminum diecast alloy and an induction motor rotor made of the diecast aluminum alloy. The aluminum alloy includes commercially pure aluminum and a sufficient weight percent (wt%) of Copper (Cu), Magnesium (Mg), and Silicon (Si) to precipitate a 0.1 wt% to 5.0 wt% of a thermally stable Q-phase precipitate, AlwCuxMgySiz, after age hardening. Wherein w = about 14.3 at% to about 23.82 at% of Al; x = about 5.90 at% to about 9.52 at% of Cu; y = about 35.30 at% to about 42.85 at% of Mg; and z = about 28.57 at% to about 35.30 at% of Si. The induction motor rotor includes an aluminum squirrel cage rotor diecast onto a laminated electrical steel. The aluminum diecast squirrel cage rotor includes about 1.0 wt% of thermally stable Al5Cu2Mg8Si6 after age hardening.

## Claims

### Claim 1

An aluminum alloy for diecasting an electrically conductive work piece, comprising:
aluminum (Al); and
a sufficient weight percent (wt%) of Copper (Cu), a sufficient wt% of Magnesium (Mg), and a sufficient wt% of Silicon (Si) to precipitate a 0.1 wt% to 5.0 wt% of at least one thermally stable Q-phase precipitate after age hardening, wherein the at least one thermally stable Q-phase precipitate is AlwCuxMgySiz:
w = atomic percent (at%) of AI;
x = at% of Copper (Cu);
y = at% of Magnesium (Mg); and
z = at% of Silicon (Si).

### Claim 2 (depends on 1)

The aluminum alloy of claim 1, wherein:
w = about 14.3 at% to about 23.82 at% of AI;
x = about 5.90 at% to about 9.52 at% of Cu;
y = about 35.30 at% to about 42.85 at% of Mg; and
z = about 28.57 at% to about 35.30 at% of Si.

### Claim 3 (depends on 1)

The aluminum alloy of claim 1, comprising about 1.0 wt% of the Q-phase precipitate AlwCuxMgySiz, wherein:
w = about 23.82 at% of AI;
x = about 9.52 at% of Cu;
y = about 38.09 at% of Mg; and
z = about 28.57 at% of Si.

### Claim 4 (depends on 1)

The aluminum alloy of claim 1, comprising:
about 0.027 wt% to about 1.734 wt% Si;
about 0.030 wt% to about 1.754 wt% Mg;
about 0.013 wt% to about 1.019 wt% Cu; and
remaining wt% of Al.

### Claim 5 (depends on 1)

The aluminum alloy of claim 1, comprising:
about 0.270 wt% to about 1.041 wt% Si;
about 0.300 wt% to about 1.053 wt% Mg;
about 0.131 wt% to about 0.611 wt% Cu; and
remaining wt% of Al.

### Claim 6 (depends on 1)

The aluminum alloy of claim 1, comprising:
about 0.270 wt% to about 0.347 wt% Si;
about 0.300 wt% to about 0.351 wt% Mg;
about 0.131 wt% to about 0.204 wt% Cu; and
remaining wt% of Al.

### Claim 7 (depends on 1)

The aluminum alloy of claim 1, wherein the Q-phase precipitate is Al5Cu2MgsSi6.

### Claim 8 (depends on 7)

The aluminum alloy of claim 7, further comprising:
greater than 0 wt% to 0.2 wt% Iron (Fe);
greater than 0 wt% to 0.5 wt% Manganese (Mn); and
greater than 0 wt% to 0.05 wt% Zinc (Zn).

### Claim 9 (depends on 8)

The aluminum alloy of claim 8, further comprising greater than 0 wt% to 0.25 wt% of a sum of Chromium (Cr), Nickel (Ni), Titanium (Ti), and Vanadium (V).

### Claim 10 (depends on 1)

The aluminum alloy of claim 1, comprising:
0.13 wt% to 0.21 wt% Cu;
0.30 wt% to 0.35 wt% Mg;
0.27 wt% to 0.35 wt% Si; and
remainder wt% Al to precipitate about 1.0 wt% of the at least one thermally stable Q-phase precipitate consisting essentially of Al5Cu2Mg8Si6.

### Claim 11

A diecast electrically conductive cast aluminum work piece, consisting essentially of:
Aluminum (Al);
0.1 wt% to 5.0 wt% of a thermally stable Q-phase precipitate AlwCuxMgySiz, wherein:
w = about 14.3 at% to about 23.82 at% of AI;
x = about 5.9 at% to about 9.52 at% of Cu;
y = about 35.3 at% to about 42.85 at% of Mg; and
z = about 28.57 at% to about 35.3 at% of Si.

### Claim 12 (depends on 11)

The diecast electrically conductive cast aluminum work piece of claim 11, wherein the thermally stable Q-phase precipitate AlwCuxMgySiz consist essentially of:
w = about 23.82 at% of AI;
x = about 9.52 at% of Cu;
y = about 38.09 at% of Mg; and
z = about 28.57% of Si.

### Claim 13 (depends on 11)

The diecast electrically conductive cast aluminum work piece of claim 11, wherein the thermally stable Q-phase precipitate AlwCuxMgySiz is about 1.0 wt. %.

### Claim 14 (depends on 13)

The diecast electrically conductive cast aluminum work piece of claim 13, wherein the thermally stable Q-phase precipitate AlwCuxMgySiz includes one or more of a precipitate selected from a group consisting of Al5Cu2Mg8Si6, Al4Cu2Mg8Si7, Al4Cu1Mg6Si6, and Al3Cu2Mg9Si7.

### Claim 15 (depends on 14)

The diecast electrically conductive cast aluminum work piece of claim 14, wherein diecast electrically conductive cast aluminum work piece is a squirrel cage of an induction motor rotor assembly.

### Claim 16

An induction motor rotor, comprising:
a laminated electrical steel;
a squirrel cage rotor cast onto the laminated electrical steel, wherein the squirrel cage rotor includes an age hardened aluminum alloy comprising:
about 0.1 weight percent (wt%) to about 5.0 wt% percent of a thermally stable Q-phase precipitate; and
a remaining wt% of commerciallly pure Aluminum (Al).

### Claim 17 (depends on 16)

The induction motor rotor of claim 16, wherein the Q-phase precipitate comprises at least one AlwCuxMgySiz precipitate, where:
w = about 14.3 atomic percent (at%) to about 23.82 at% of AI;
x = about 5.9 at% to about 9.52 at% of Copper (Cu);
y = about 35.3 at% to about 42.85 at% of Magnesium (Mg); and
z = about 28.57 at% to about 35.3 at% of Silicon (Si).

### Claim 18 (depends on 17)

The induction motor rotor of claim 17, wherein the age hardened aluminum alloy comprising about 1.0 wt% of the Q-phase precipitate.

### Claim 19 (depends on 18)

The induction motor rotor of claim 18, wherein Q-phase precipitate comprises Al5Cu2Mg8Si6.

### Claim 20 (depends on 16)

The induction motor rotor of claim 16, wherein the age hardened aluminum alloy comprises:
about 0.270 wt% to about 0.347 wt% Si;
about 0.300 wt% to about 0.351 wt% Mg; and
about 0.131 wt% to about 0.204 wt% Cu.