# US 2023/0067197 A1 · Method of manufacturing silicon carbide ingot

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0067197 A1
- Document ID: US20230067197A1
- Status: Published application
- Kind: A1
- Application number: 17/975,639
- Filed: 2022-10-28
- Published: 2023-03-02
- Earliest claimed: 2020-07-27
- Assignees: GlobalWafers Co., Ltd.
- Applicants: GlobalWafers Co., Ltd.
- Inventors: Ching-Shan Lin
- Web page: https://patentgrep.com/patent/US20230067197A1

## CPC

- C30B 23/025: {characterised by the substrate}
- C30B 23/063: {Heating of the substrate}
- C30B 23/066: {Heating of the material to be evaporated}
- C30B 29/36: Carbides
- C01B 32/956: Silicon carbide
- H10D 62/50: Physical imperfections
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The disclosure provides a silicon carbide seed crystal and a method of manufacturing a silicon carbide ingot. The silicon carbide seed crystal has a silicon surface and a carbon surface opposite to the silicon surface. A difference D between a basal plane dislocation density BPD1 of the silicon surface and a basal plane dislocation density BPD2 of the carbon surface satisfies the following formula (1), a local thickness variation (LTV) of the silicon carbide seed crystal is 2.5 μm or less, and a stacking fault (SF) density of the silicon carbide seed crystal is 10 EA/cm2 or less: D=(BPD1−BPD2)/BPD1≤25% (1).

## Claims

### Claim 1

A method of manufacturing a silicon carbide ingot, comprising:
disposing a silicon carbide seed crystal on a top of a crucible;
disposing a silicon carbide based raw material in the crucible;
heating the silicon carbide based raw material to form a thermal field in the crucible, so that the silicon carbide based raw material is sublimated in the thermal field of the crucible, wherein a radial temperature gradient of the thermal field in the crucible is greater than or equal to 5° C./cm and less than or equal to 50° C./cm;
growing the sublimed silicon carbide into a silicon carbide single crystal after being in contact with the silicon carbide seed crystal disposed on the top of the crucible;
growing the silicon carbide single crystal continuously on the silicon carbide seed crystal to obtain silicon carbide ingots.

### Claim 2 (depends on 1)

The method of manufacturing the silicon carbide ingot according to claim 1, wherein the radial temperature gradient is greater than or equal to 5° C./cm and less than or equal to 45° C./cm.

### Claim 3 (depends on 1)

The method of manufacturing the silicon carbide ingot according to claim 1, a basal plane dislocation density (BPD) of a carbon surface of the grown silicon carbide ingot is 300 EA/cm2 or less, a stacking fault (SF) density of the carbon surface of the grown silicon carbide ingot is 10 EA/cm2 or less, and a threading screw dislocation (TSD) density of the carbon surface of the grown silicon carbide ingot is 35 EA/cm2 or less.

### Claim 4 (depends on 1)

The method of manufacturing the silicon carbide ingot according to claim 1, wherein the silicon carbide seed crystal comprises a silicon surface and a carbon surface opposite to the silicon surface, wherein a difference D between a basal plane dislocation density BPD1 of the silicon surface and a basal plane dislocation density BPD2 of the carbon surface satisfies a formula (1) as follows, a local thickness variation (LTV) of the silicon carbide seed crystal is 2.5 μm or less, and a stacking fault (SF) density of the silicon carbide seed crystal is 10 EA/cm2 or less:
D=(BPD1−BPD2)/BPD1≤25% (1).