# US 2023/0066264 A1 · Coating compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0066264 A1
- Document ID: US20230066264A1
- Status: Published application
- Kind: A1
- Application number: 17/791,693
- Filed: 2021-01-13
- Published: 2023-03-02
- Earliest claimed: 2020-01-14
- Assignees: GKN Aerospace Services Limited
- Applicants: Gkn Aerospace Services Limited
- Inventors: Jieming LI; Marlowe MONCUR; Lin H. HOO
- Web page: https://patentgrep.com/patent/US20230066264A1

## CPC

- C09D 175/06: from polyesters
- B32B 17/10: of synthetic resin
- B32B 17/10174: {Coatings of a metallic or dielectric material on a constituent layer of glass or polymer}
- B64C 1/1476: {Canopies; Windscreens or similar transparent elements}
- C08G 18/0852: {the solvents being organic}
- C08G 18/10: Prepolymer processes involving reaction of isocyanates or isothiocyanates with compounds having active hydrogen in a first reaction step
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/289: {containing silicon}
- C08G 18/4277: {Caprolactone and/or substituted caprolactone}
- C08G 18/758: {containing two or more cycloaliphatic rings}
- C08G 77/14: containing silicon bound to oxygen-containing groups
- C08G 77/458: containing polyurethane sequences
- C08L 75/06: from polyesters
- C09D 4/00: Coating compositions, e.g. paints, varnishes or lacquers, based on organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond {; Coating compositions, based on monomers of macromolecular compounds of groups C09D183/00 - C09D183/16}
- C09D 5/32: Radiation-absorbing paints {(protection against X-, gamma- or corpuscular radiation G21F)}
- C09D 7/20: Diluents or solvents
- C09D 7/47: Levelling agents
- C09D 7/48: Stabilisers against degradation by oxygen, light or heat
- C09D 7/63: organic
- C09D 175/04: Polyurethanes
- C09D 183/04: Polysiloxanes
- C09D 183/06: containing silicon bound to oxygen-containing groups (C09D183/12 takes precedence)
- B60J 1/2094: {Protective means for window, e.g. additional panel or foil, against vandalism, dirt, wear, shattered glass, etc.}
- C08G 77/16: to hydroxy groups
- C08G 77/18: to alkoxy or aryloxy groups
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B64C: AEROPLANES; HELICOPTERS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B60J: WINDOWS, WINDSCREENS, NON-FIXED ROOFS, DOORS, OR SIMILAR DEVICES FOR VEHICLES; REMOVABLE EXTERNAL PROTECTIVE COVERINGS SPECIALLY ADAPTED FOR VEHICLES (fastening, suspending, closing, or opening of such devices E05)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Disclosed are polyurethane-polysiloxane hybrid coating compositions (PUPSHCC) and their uses, processes for their preparation, and substrates incorporating the coating compositions.

## Claims

### Claim 1

A two-part curable coating composition comprising:
(A) a composition comprising an alkoxysilane terminated polyester urethane prepolymer, comprising a prepolymer chain having a terminal group of general formula (I):
wherein:
Y represents: H; R1 wherein R1 represents hydrocarbyl preferably alkyl or aryl; or wherein Y represents the group:
L represents a hydrocarbylene group, preferably an alkylene or an arylene group, preferably a C1 to C10 hydrocarbylene group, and preferably methylene, ethylene, or propylene and most preferably propylene;
W1, W2, W3, W4, W5 and W6 may be the same or different and each independently represents —OR2, wherein R2 at each occurrence may be the same or different, and each R2 is independently selected from an alkyl group, preferably wherein the alkyl group has 1 to 10 carbon atoms, and preferably wherein the alkyl group has 1 to 8 atoms, preferably methyl or ethyl, and most preferably methyl;
and
(B) a composition comprising a silanol terminated polysiloxane prepolymer obtainable by sol-gel process of an alkoxysilane selected from a compound of general formula (II), (III) or (IV):
wherein:
X1, X2, X3, X4, X5, and X6 each represents —OR3;
R3 at each occurrence is the same or different, and each is independently selected from an alkyl group, preferably wherein the alkyl group has 1 to 10 carbon atoms, 1 to 8 atoms, 1 to 6 carbon atoms, and most preferably 1 to 4 carbon atoms; and
m represents an integer from 1 to 6, preferably 1 to 3.

### Claim 2 (depends on 1)

The composition according to claim 1 wherein the compositions (A) and/or (B) include at least one or more of the following: solvent; urethane forming catalyst; antistatic agent; stabilizer selected from one or more of a UV absorber, light stabilizer and thermal stabilizer; and surface active agent selected from one or more of a flow or levelling agent and surfactant; preferably wherein composition (A) comprises at least one solvent, a flow or levelling agent, at least one stabilizer, a urethane forming catalyst and a surface additive and wherein composition (B) comprises at least one solvent, and an antistatic additive.

### Claim 3 (depends on 1)

The composition according to claim 1, wherein R1 at each occurrence is the same or different, and each is independently selected from: a C1 to C6 alkyl, or a C1 to C4 alkyl group; and preferably wherein R1 at each occurrence is the same and each represents a C1 to C6 alkyl, or a C1 to C4 alkyl group, and preferably a methyl or ethyl group.

### Claim 4 (depends on 1)

The composition according to claim 1, wherein Y is H.

### Claim 5 (depends on 1)

The composition according to claim 1, comprising at least one solvent, preferably comprising two or more solvents, preferably wherein the solvent comprises an aprotic solvent and a protic solvent, preferably wherein the aprotic solvent is selected from the group consisting of ethyl 3-ethoxypropionate (EEP), n-pentyl propionate (nPP), 2-butoxyethyl acetate (BEA), di-isobutyl ketone (DIBK), and methyl isobutyl ketone (MIBK), or a combination thereof, and/or the protic solvent is a hydroxyketone, preferably a β-hydroxyketone, and more preferably diacetone alcohol (DAA); preferably wherein the composition (A) comprises a mixture of an alkoxysilane terminated polyester urethane prepolymer in ethyl 3-ethoxypropionate and diacetone alcohol.

### Claim 6 (depends on 1)

The composition according to claim 1, comprising a urethane forming catalyst, preferably wherein the urethane forming catalyst is selected from the group consisting of: dibutyltin dilaurate (DBTDL) or dibutyltin diacetate (DBTDA); and/or wherein the urethane forming catalyst is present in an amount of about 0.1 ppm to about 100 ppm, and preferably about 1 ppm to about 10 ppm, based on the total weight of solids in the composition.

### Claim 7 (depends on 1)

The composition according to claim 1, comprising a UV absorber, a light absorber and a thermal stabilizer; preferably:
wherein the UV absorber is selected from:
a mixture of 2-[4-[2-Hydroxy-3-tridecyloxypropyl]oxy]-2-hydroxyphenyl]-4,6-bis(2,4-dimethylphenyl)-1,3,5-triazine and 2-[4-[2-hydroxy-3-didecyloxypropyl]oxy]-2-hydroxyphenyl]-4,6-bis(2,4-dimethylphenyl)-1,3,5-triazine (Tinuvin 400);
[2-hydroxy-4-[3-(2-ethylhexyl-1-oxy)-2-hydroxypropyloxy]phenyl]-4,6bis(2,4-dimethylphenyl)-1,3,5-triazine) (Tinuvin 405);
2,4-bis(2-hydroxy-4-butoxyphenyl)-6-(2,4-dibutoxyphenyl)-1,3,5-triazine (Tinuvin 460);
2-hydroxyphenyl-s-triazine with 18-20% 2-methoxy-1-propyl-acetate (Tinuvin 477);
6-methylheptyl 2-[4-[4,6-bis(4-phenylphenyl)-1H-1,3,5-triazin-2-ylidene]-3-oxocyclohexa-1,5-dien-1-yl]oxypropanoate (Tinuvin 479);
2-(2H-benzotriazol-2-yl)-6-(1-methyl-1-phenylethyl)-4-(1,1,3,3-tetramethylbutyl)phenol (Tinuvin 928);
a mixture of: a) 50% b-[3-(2-H-Benzotriazole-2-yl)-4-hydroxy-5-tert.butylphenyl]-propionic acidpoly(ethylene glycol) 300-ester and b) 50% Bis{b-[3-(2-H-Benzotriazole-2-yl)-4-hydroxy-5-tert.butylphenyl]-propionic acid}-poly(ethylene glycol) 300-ester (Tinuvin 1130);
2-(benzotriazol-2-yl)-4,6-bis(2-methylbutan-2-yl)phenol (Tinuvin 328);
a mixture of 95% Benzenepropanoic acid, 3-(2H-benzotriazol-2-yl)-5-(1,1-dimethylethyl)-4-hydroxy-, C7-9-branched and linear alkyl esters and 5% 2-Propanol, 1-methoxy-, 2-acetate (Tinuvin 99-2); and
a mixture of 95% Benzenepropanoic acid, 3-(2H-benzotriazol-2-yl)-5-(1,1-dimethylethyl)-4-hydroxy-, C7-9-branched and linear alkyl esters and 5% 1-methoxy-2-propyl acetate (Tinuvin 384-2); and/or
wherein the light absorber is a hindered amine light stabilizer (HALS), more preferably selected from:
decanedioic acid, bis (2,2,6,6-tetramethyl-1-(octyloxy)-4-piperidinyl) ester (Tinuvin 123);
bis(1,2,2,6,6-pentamethyl-4-piperidinyl)-[[3,5-bis(1,1-dimethylethyl)-4-hydroxyphenyl]methyl]butylmalonate (Tinuvin 144);
2,4-bis[N-butyl-N-(1-cyclohexyloxy-2,2,6,6-tetramethylpiperidin-4-yl)amino]-6-(2-hydroxyethylamine)-1,3,5-triazine (Tinuvin 152);
mixture of bis(1,2,2,6,6-pentamethyl-4-piperidinyl)sebacate (75-85%) and methyl 1,2,2,6,6-pentamethyl-4-piperidyl sebacate (15-25%) (Tinuvin 292); or
a liquid, non-basic amino-ether (NOR) non-interacting hindered amine light stabilizer (Tinuvin 5100); and/or
wherein the thermal stabilizer is a sterically hindered phenolic antioxidant, preferably selected from the group consisting of: pentaerythritol tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate); octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate; benzenepropanoic acid, 3,5-bis(1,1-dimethylethyl)-4-hydroxy-, C7-9-branched alkyl esters; and triethylene glycol bis(3-tert-butyl-4-hydroxy-5-methylphenyl)propionate; and more preferably wherein the thermal stabilizer is pentaerythritol tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate).

### Claim 8 (depends on 1)

The composition according to claim 1, comprising a stabilizer combination comprising: a UV absorber, a light absorber and a thermal stabilizer, preferably:
wherein the composition comprises a stabilizer combination of: 6-methylheptyl 2-[4-[4,6-bis(4-phenylphenyl)-1H-1,3,5-triazin-2-ylidene]-3-oxocyclohexa-1,5-dien-1-yl]oxypropanoate (Tinuvin 479), 2,4-bis[N-butyl-N-(1-cyclohexyloxy-2,2,6,6-tetramethylpiperidin-4-yl)amino]-6-(2-hydroxyethylamine)-1,3,5-triazine (Tinuvin 152) and pentaerythritol tetrakis(3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate) (IRGANOX 1010); and/or
wherein the total amount of stabilizers is about 0.5 wt % to about 4 wt %, and preferably about 1 wt % to about 3 wt %, based on the total weight of solids in the two part curable composition.

### Claim 9 (depends on 1)

The composition according to claim 1, comprising an antistatic agent, preferably:
wherein the antistatic agent is a hydrophilic or a hydrophobic antistatic agent, more preferably wherein the antistatic agent is a salt of (bis)trifluoromethane-sulfonimide, particularly wherein the antistatic agent is: lithium (bis)trifluoromethanesulfonimide, tri-n-butylmethylammonium bis-(trifluoromethanesulfonyl)-imide, or a quaternary alkyl ammonium salt of (bis)trifluoromethane-sulfonimide, and particularly preferably lithium (bis)trifluoromethanesulfonimide; and/or
wherein the antistatic additive is present in the range of 1 to 5 weight percent, and preferably in the range of 2 to 3 weight percent, based on the total weight of solids in the composition.

### Claim 10 (depends on 1)

The composition according to claim 1, comprising a flow or levelling agent and/or a surfactant, preferably:
wherein the flow or levelling agent is a silicone-based flow or levelling agent, particularly a modified siloxane silicone based flow or levelling agent and more preferably wherein the flow or levelling agent is selected from the group consisting of: polyethylene glycol mono(3-(tetramethyl-1-(trimethylsiloxy)disiloxanyl)propyl)ether (Silwet L-77); a mixture of siloxane polyalkyleneoxide copolymer and octamethylcyclotetrasiloxane (Silwet L-7200); an organosilicone of the polyalkyleneoxide modified polydimethylsiloxane (Silwet L-7600); an organosilicone surface tension reducing agent with siloxane polyalkyleneoxide coplymer and octamethylcyclotetrasiloxane (Silwet L-7604); a polyether silicone of polyalkyleneoxide modified polydimethylsiloxane (Silwet L-7605); and an organosilicone surface tension reducing agent with a polyalkyleneoxide modified polydimethylsiloxane (Silwet L-7657); and preferably wherein the flow or levelling agent is polyethylene glycol mono(3-(tetramethyl-1-(trimethylsiloxy)disiloxanyl)propyl)ether; and/or
wherein the surfactant is a silicone based surface additive, preferably wherein the surfactant is a polyether modified polydimethylsiloxane (particularly BYK-300, BYK-306, BYK-313, and BYK-378); or a polyester-modified polydimethylsiloxane (particularly BYK-333 and BYK-370; and/or
wherein the flow or levelling agent is polyethylene glycol mono(3-(tetramethyl-1-(trimethylsiloxy)disiloxanyl)propyl)ether (Silwet L-77), and the surfactant is polyester modified hydroxyl functional polydimethylsiloxane (BYK-370).

### Claim 11 (depends on 1)

The composition according to claim 1, wherein the alkoxysilane-terminated polyester urethane prepolymer in composition (A) is obtainable by a process comprising:
(i) reacting an aliphatic diisocyanate with a polyester diol to form an isocyanate-terminated polyester urethane prepolymer; and
(ii) silanization of the isocyanate-terminated polyester urethane prepolymer with an amino-functional alkoxysilane to form an alkoxysilane-terminated polyester urethane prepolymer.

### Claim 12 (depends on 11)

The composition according to claim 11, wherein the aliphatic diisocyanate in step (i) is a monomeric aliphatic diisocyanate, or a monomeric cycloaliphatic diisocyanate, preferably selected from: hexamethylene diisocyanate, methylene bis (4-cyclohexylisocyanate), and isophorone diisocyanate, and more preferably methylene bis (4-cyclohexylisocyanate).

### Claim 13 (depends on 11)

The composition according to claim 11, wherein the polyester diol is a polycaprolactone-based polyester diol, preferably a linear polyester diol derived from caprolactone monomer which is terminated by primary hydroxyl groups, more preferably wherein the polyester diol is obtainable by catalytic ring-opening polymerization of caprolactone monomer in the presence of a diol initiator, preferably wherein the diol initiator is alkylenediol or an dialkyleneglycol initiator, and most preferably wherein the diol initiator is selected from the group consisting of 1,4-butanediol (BDO), diethylene glycol (DEG) and neopentyl glycol (NEO), and particularly diethylene glycol; wherein the polyester diol preferably has a molecular weight of about 300 g/mol to about 5000 g/mol, preferably about 380 g/mol to about 4500 g/mol, or about 600 g/mol to about 1000 g/mol, or particularly about 700 g/mol to about 900 g/mol, and especially about 800 g/mol to about 850 g/mol.

### Claim 14 (depends on 11)

The composition according to claim 11, wherein the molar ratio of the polyester diol to aliphatic diisocyanate in step (i) is from: about 1:1.1 to about 1:5, about 1:1.1 to about 1:4, about 1:1.1 to about 1:2, about 1:1.3 to about 1:1.7, or about 1:1.6.

### Claim 15 (depends on 7, 8, 10, 11)

The composition according to claim 11, wherein step (i) is carried out in the presence of a urethane forming catalyst, preferably wherein the catalyst is selected from the group consisting of dibutyltin dilaurate (DBTDL) or dibutyltin diacetate (DBTDA); and/or wherein the reaction mixture in step (i) further comprises at least one additive selected from the group consisting of: one or more stabilizers preferably a UV absorber, a light stabilizer and a thermal stabilizer preferably as defined in any of claims 7 to 8; and a flow/levelling agent preferably as defined in claim 10.

### Claim 16 (depends on 11)

The composition according to claim 11, wherein step (i) is carried out at a temperature of: about 50° C. to about 120° C., or about 60° C. to about 100° C., or about 70° C. to about 90° C.; and/or wherein the reaction time in step (i) is about 1 to about 4 hours, or preferably about 1 to about 3 hours.

### Claim 17 (depends on 11)

The composition according to claim 11, wherein step (i) further comprises adding an aprotic solvent to the isocyanate-terminated polyester urethane prepolymer to form a homogeneous mixture having a solid content of about 20 to about 80 wt %, preferably about 30 to about 70 wt %, more preferably about 40 to about 60 wt %; preferably wherein the aprotic solvent is selected from the group consisting of: ethyl 3-ethoxypropionate (EEP), n-pentyl propionate (nPP), 2-butoxyethyl acetate (BEA), di-isobutyl ketone (DIBK), and methyl isobutyl ketone (MIBK), and more preferably 3-ethoxypropionate (EEP).

### Claim 18 (depends on 11)

The composition according to claim 11, wherein the amino-functional alkoxysilane in step (ii) is selected from the group consisting of: an aminoalkyltrialkoxysilane, an aminoaryltrialkoxysilane, an aminoalkyl(alkyl)(dialkoxyl)silane, a [bis(trialkoxylsilyl)-alkyl]amine, an N-(aminoalkyl)-aminoalkyltrialkoxysilane, or an N-alkyltrialkoxylsilyl-N,N-dialkylamine; and preferably wherein the amino-functional alkoxysilane is an aminoalkyltrialkoxysilane, preferably wherein the amino-functional alkoxysilane is selected from the group consisting of 3-aminopropyltrimethoxysilane, 3-aminopropyltriethoxysilane, 4-aminobutyltrimethoxysilane, 4-aminobutyltriethoxy-silane, aminophenyltrimethoxysilane, aminophenyltriethoxysilane, 3-aminopropyl-methyldiethoxysilane,3-aminopropylmethyldimethoxysilane, bis(trimethoxysilyl-propyl)amine, bis(triethoxysilylpropyl)amine, N-ethyl-3-trimethoxysilyl-2-methylpropanamine; more preferably 3-aminopropyltrimethoxysilane (APTMS) or 3-aminopropyltriethoxysilane (APTES); and most preferably 3-aminopropyltrimethoxysilane (APTMS).

### Claim 19 (depends on 11, 17)

The composition according to claim 11, wherein step (ii) comprises addition of the amino-functional alkoxysilane to the isocyanate-terminated polyester urethane prepolymer; and/or wherein step (ii) is conducted in the presence of at least one aprotic solvent preferably as defined in claim 17, and optionally additionally in the presence of a protic solvent in which the isocyanate-terminated polyester urethane prepolymer and the amino-functional alkoxysilane is soluble; preferably wherein the protic solvent is a hydroxyketone, more preferably a β-hydroxyketone, and particularly diacetone alcohol (DAA).

### Claim 20 (depends on 10, 11)

The composition according to claim 11, wherein step (ii) further comprises adding at least one surfactant to the alkoxysilane-terminated polyester urethane prepolymer, preferably wherein the surfactant is as defined in claim 10.

### Claim 21 (depends on 1)

The composition according to claim 1, wherein the silanol terminated polysiloxane prepolymer (B) is obtainable by sol-gel process of an alkyltrioxysilane, an alkylorthosilicate or a bis(trialkyloxysilyl)alkane, preferably an alkylorthosilicate; preferably wherein the silanol terminated polysiloxane prepolymer (B) is obtainable by sol-gel process of an alkoxysilane selected from the group consisting of: tetraethyl orthosilicate, tetramethyl orthosilicate, methyltrimethoxysilane, methyltriethoxysilane, ethyltrimethoxysilane, ethyltriethoxysilane, 1,2-bis(triethoxysilyl)ethane, and 1,2-bis(trimethoxysilyl)ethane; and more preferably tetraethyl orthosilicate; preferably wherein the silanol terminated polysiloxane prepolymer in composition (B) is obtainable by a process comprising: reacting an alkoxysilane, preferably an alkyltrioxysilane, an alkylorthosilicate or a bis(trialkyloxysilyl)alkane, and more preferably an alkylorthosilicate, with at least one acid, in the presence of a solvent comprising an alcohol and water.

### Claim 22 (depends on 21)

The composition according to claim 21, wherein the process comprises adding the alkoxysilane to a mixture comprising the at least one acid, water and an alcohol; preferably wherein the reaction mixture in step (a) is held at a temperature of: about 15° C. to about 30° C., about 18° C. to about 25° C. or about 20° C. to about 25° C., preferably for: about 8 to about 120 hours, about 12 to about 96 hours, about 20 to about 60 hour, or about 30 to about 50 hours.

### Claim 23 (depends on 21)

The composition according to claim 21, wherein the acid comprises a carboxylic acid and/or a mineral acid, preferably wherein the acid comprises a carboxylic acid and a mineral acid; preferably wherein the carboxylic acid is a C2-C6 alkylcarboxylic acid, preferably acetic acid; and/or wherein the mineral acid is selected from the group consisting of hydrochloric acid, sulfuric acid, nitric acid, hydrobromic acid, hydrofluoric acid, and phosphoric acid, and preferably wherein the mineral acid is hydrochloric acid.

### Claim 24 (depends on 21)

The composition according to claim 21, wherein the acid is present in an amount to maintain a pH in the range of about 1.5 to about 5, preferably about 1.8 to about 4.5, and more preferably about 2 to about 4; preferably wherein the acid comprises acetic acid and hydrochloric acid.

### Claim 25 (depends on 9, 21)

The composition according to claim 21, further comprising adding an antistatic agent to the silanol terminated polysiloxane prepolymer, preferably wherein the antistatic agent is as defined in claim 9.

### Claim 26 (depends on 11)

The composition according to claim 11, wherein the molar ratio of the amino-functional alkoxysilane in step (ii) to the alkoxysilane in composition (B) is about 1:4 to about 4:1, preferably about 1:3 to about 3:1, and more preferably about 1:2 to about 1:3.

### Claim 27 (depends on 1)

The composition according to claim 1, which is thermally curable, preferably in the presence of a catalyst, more preferably wherein the catalyst is selected from the group consisting of: dibutyltin dilaurate (DBTDL) or dibutyltin diacetate (DBTDA).

### Claim 28 (depends on 1)

The polyurethane-polysiloxane hybrid coating composition (PUPSHCC) precursor which is obtainable by a process comprising compounding composition (A) and composition (B) of the two-part curable composition as defined in claim 1, optionally with a urethane forming catalyst preferably wherein the compounding comprises combining the compositions (A) and (B) and optionally a urethane forming catalyst, by agitation, preferably with degassing, to obtain a homogeneous mixture, and more preferably wherein the catalyst is selected from the group consisting of dibutyltin dilaurate (DBTDL) or dibutyltin diacetate (DBTDA).

### Claim 29 (depends on 28)

The polyurethane-polysiloxane hybrid coating composition precursor according to claim 28, having a solids content of about 10 wt % to about 50 wt, and preferably about 20 wt % to about 40 wt % or about 30 wt %.

### Claim 30 (depends on 28)

The polyurethane-polysiloxane hybrid coating composition which is obtainable by a process comprising removing at least a portion of solvent, and preferably at least 80 wt %, at least 90 wt %, at least 95 wt %, or at least 98 wt % of the solvent, from the polyurethane-polysiloxane hybrid coating composition precursor of claim 28, preferably by air drying, and subjecting the PUPSHCC precursor to thermal curing, preferably wherein the thermal curing comprises heating the polyurethane-polysiloxane hybrid coating composition precursor to a temperature of: about 50° C. to about 82° C., about 60° C. to about 82° C. or about 70° C. to about 82° C.

### Claim 31 (depends on 1, 12)

The process for preparing a two-part curable coating composition as defined in claim 1, comprising:
(1) preparing a composition (A) comprising an alkoxysilane-terminated polyester urethane prepolymer by a process comprising: (i) reacting an aliphatic diisocyanate with a polyester diol to form an isocyanate-terminated polyester urethane prepolymer; and (ii) silanization of the isocyanate-terminated polyester urethane prepolymer with an amino-alkoxysilane according to a process as defined in claim 12; and
(2) preparing a silanol terminated polysiloxane prepolymer (B) by sol-gel process of an alkoxysilane with at least one acid, in the presence of a solvent comprising an alcohol and water.

### Claim 32 (depends on 1)

A method comprising, coating a substrate with the composition as defined according to claim 1, preferably wherein the substrate is selected from the group consisting of an aircraft, a spacecraft, a marine craft or vehicle part, preferably an aircraft part, and more preferably an aircraft transparency, and most preferably an aircraft window or an aircraft windscreens, preferably wherein the coating is subjected to thermal curing to provide a polyurethane-polysiloxane hybrid coating composition which is a crosslinked alkyloxysilane-terminated polyester urethane with the polysiloxane.

### Claim 33 (depends on 30)

A substrate, preferably an aircraft, spacecraft, marine craft or vehicle part comprising a polyurethane-polysiloxane hybrid polymer coating composition of claim 30, preferably wherein the substrate is an aircraft part, particularly an aircraft transparency, and more particularly an aircraft window or windscreen.

### Claim 34 (depends on 28, 33)

A process for preparing the substrate according to claim 33, comprising applying a polyurethane-polysiloxane hybrid coating composition precursor as defined in claim 28 to a surface of a substrate, removing at least a portion of the solvent, and preferably at least 80 wt %, at least 90 wt %, at least 95 wt %, or at least 98 wt %, of the solvent, from the polyurethane-polysiloxane hybrid coating composition precursor, preferably by air drying, and thermally curing the coating composition precursor, preferably by heating to a temperature of: about 50° C. to about 82° C., about 60° C. to about 82° C. or about 70° C. to about 82° C., to provide a substrate coated with a polyurethane-polysiloxane hybrid coating composition, and more preferably wherein the substrate is an aircraft transparency, preferably an aircraft window or windshield, and wherein the surface of the substrate comprises an electrically conductive layer, preferably wherein the conductive layer is an indium tin oxide (ITO) layer or a carbon nanotube (CNT) layer, and optionally a silicon binder layer over the conductive layer, onto which the polyurethane-polysiloxane hybrid coating composition precursor is applied.

### Claim 35 (depends on 34)

A substrate, preferably an aircraft transparency, and more preferably an aircraft window or an aircraft windshield, which is obtainable by the process of claim 34.