# US 2023/0066183 A1 · Method of fabricating a semiconductor structure and semiconductor structure obtained therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0066183 A1
- Document ID: US20230066183A1
- Status: Published application
- Kind: A1
- Application number: 17/461,798
- Filed: 2021-08-30
- Published: 2023-03-02
- Earliest claimed: 2021-08-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: KENICHI SANO; CHUNG-LIANG CHENG; DE-YANG CHIOU; KUANLIANG LIU; PINYEN LIN
- Web page: https://patentgrep.com/patent/US20230066183A1

## CPC

- H10P 90/1914: {using bonding}
- H10P 72/0424: {using mainly spraying means, e.g. nozzles}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a semiconductor structure and the semiconductor structure are disclosed. The method uses high flow rate of an etchant and an optimized scan pattern, so that the obtained semiconductor structure is a device upside-down bonded to the carrier wafer without any silicon remaining and is ready for subsequent lithography process for back via contact.

## Claims

### Claim 1

A method of fabricating a semiconductor structure, comprising the steps of:
providing a device wafer having a front surface and a back surface, the device wafer comprising a first dielectric layer, a semiconductor material layer, and a second dielectric layer at least on the front surface;
bonding the front surface of the device wafer to a carrier wafer; and
thinning the device wafer until the first dielectric layer is exposed;
wherein the thinning step comprises grinding the back surface of the device wafer, and etching the back surface of the device wafer by using a chemical etching instrument, and wherein a scanning speed of a spray nozzle of the chemical etching instrument is higher at a central portion of the device wafer than at a peripheral portion of the device wafer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the carrier wafer comprises a bonding material layer formed thereon.

### Claim 3 (depends on 2)

The method of claim 2, wherein the bonding step comprises bonding the second dielectric layer of the device wafer to the bonding material layer of the carrier wafer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the thinning step comprises grinding the back surface of the device wafer to a first predetermined thickness, etching the back surface of the device wafer by using a first etching aqueous solution to a second predetermined thickness, and etching the back surface of the device wafer by using a second etching aqueous solution so that the device wafer is completed removed.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first predetermined thickness is larger than the second predetermined thickness.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first predetermined thickness ranges from about 15 μm to about 20 μm, and the second predetermined thickness ranges from about 0.1 μm to about 5 μm.

### Claim 7 (depends on 4)

The method of claim 4, wherein the first etching aqueous solution comprises hydrofluoric acid, nitric acid, sulfuric acid, phosphorous acid, or mixtures thereof, and the second etching aqueous solution comprises tetramethylammonium hydroxide (TMAH), ammonium hydroxide, or mixtures thereof.

### Claim 8 (depends on 4)

The method of claim 4, wherein a flow rate of the first etching aqueous solution ranges from about 3 L/min to about 5 L/min.

### Claim 9 (depends on 1)

The method of claim 1, wherein the device wafer comprises features in the semiconductor material layer, and the features comprise a front end of line (FEOL) portion on the first dielectric layer, a middle end of line (MEOL) portion on the front end of line portion, and a back end of line (BEOL) portion on the middle end of line portion.

### Claim 10

A method of fabricating a semiconductor structure, comprising the steps of:
providing a device wafer having a front surface and a back surface, the device wafer comprising a first dielectric layer, a semiconductor material layer, and a second dielectric layer at least on the front surface;
providing a carrier wafer having a bonding material layer formed thereon;
bonding the second dielectric layer of the device wafer to the bonding material layer of the carrier wafer; and
thinning the device wafer;
wherein the thinning step comprises grinding the back surface of the device wafer to a first predetermined thickness, and etching the back surface of the device wafer to a second predetermined thickness by using a chemical etching instrument, and wherein a scanning speed of a spray nozzle of the chemical etching instrument is higher at a central portion of the device wafer than at a peripheral portion of the device wafer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first predetermined thickness ranges from about 15 μm to about 20 μm, and the second predetermined thickness is less than about 5 μm.

### Claim 12 (depends on 10)

The method of claim 10, wherein the grinding step comprises using a grinding machine, and the etching step comprises using an etching aqueous solution comprising hydrofluoric acid, nitric acid, sulfuric acid, phosphorous acid, or mixtures thereof.

### Claim 13 (depends on 10)

The method of claim 10, wherein the scanning speed of the spray nozzle of the chemical etching instrument is substantially constant at the central portion of the device wafer.

### Claim 14 (depends on 10)

The method of claim 10, wherein the scanning speed of the spray nozzle of the chemical etching instrument gradually decreases from the central portion to the peripheral portion of the device wafer.

### Claim 15 (depends on 12)

The method of claim 12, wherein a flow rate of the etching aqueous solution ranges from about 3 L/min to about 5 L/min.

### Claim 16 (depends on 10)

The method of claim 10, wherein a uniformity of the thinned surface of the device wafer is about 2% or less.

### Claim 17 (depends on 10)

The method of claim 10, wherein the device wafer is thinned until the first dielectric layer is exposed.

### Claim 18 (depends on 10)

The method of claim 10, wherein the semiconductor structure includes a backside silicon illuminated (BSI) image sensor, a complementary metal-oxide-semiconductor (CMOS) image sensors (CIS), or a power rail device.

### Claim 19

A semiconductor structure, comprising:
a wafer;
a bond oxide layer disposed over the wafer;
a semiconductor material layer comprising features disposed over the bond oxide layer, the features comprising a back end of line (BEOL) portion disposed on the first dielectric layer and a middle end of line (MEOL) portion on the back end of line portion; and a dielectric layer disposed over the semiconductor material layer.

### Claim 20 (depends on 19)

The semiconductor structure of claim 19, wherein no residual silicon is present on the dielectric layer.