# US 2023/0066053 A1 · Stiffener ring and surface packaging assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0066053 A1
- Document ID: US20230066053A1
- Status: Published application
- Kind: A1
- Application number: 17/974,619
- Filed: 2022-10-27
- Published: 2023-03-02
- Earliest claimed: 2020-04-28
- Assignees: Huawei Technologies Co., Ltd.
- Applicants: Huawei Technologies Co., Ltd.
- Inventors: Chuncheng GONG; Li FAN; Weijin PAN; Junwei MU; Ge ZHANG
- Web page: https://patentgrep.com/patent/US20230066053A1

## CPC

- H05K 1/0271: {Arrangements for reducing stress or warp in rigid printed circuit boards, e.g. caused by loads, vibrations or differences in thermal expansion}
- H05K 1/181: associated with surface mounted components
- H10W 42/121: {protecting against mechanical damage (H10W76/00, H10W74/00 take precedence)}
- H10W 76/40: Fillings or auxiliary members in containers, e.g. centering rings (fillings or auxiliary members for thermal protection or control in containers or encapsulations H10W40/70)
- H10W 78/00: Detachable holders for supporting packaged chips in operation
- H05K 2201/09136: Means for correcting warpage
- H05K 2201/10424: Frame holders
- H10W 72/07236: {Soldering or alloying}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 74/117: {the substrate having spherical bumps for external connection}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

This application provides a stiffener ring and a surface packaging assembly. The stiffener ring is configured to correct warpage of a substrate of the surface packaging assembly. The stiffener ring includes an annular stiffener ring body and an adjustment block that is disposed at a same layer as the stiffener ring body and that is fastened to at least one corner of the stiffener ring body. A coefficient of thermal expansion of the adjustment block is less than a coefficient of thermal expansion of the stiffener ring body. Coordination between the adjustment block and the stiffener ring body alleviates an “M-shape” overpressure phenomenon of a warpage deformation caused by the stiffener ring to the substrate at a high temperature, reduces warpage of the substrate, and improves flatness of the surface packaging assembly.

## Claims

### Claim 1

A stiffener ring, configured to correct warpage of a substrate of a surface packaging assembly, wherein the stiffener ring comprises an annular stiffener ring body and an adjustment block that is disposed at a same layer as the stiffener ring body and that is fastened to at least one corner of the stiffener ring body; and
a coefficient of thermal expansion of the adjustment block is less than a coefficient of thermal expansion of the stiffener ring body.

### Claim 2 (depends on 1)

The stiffener ring according to claim 1, wherein the stiffener ring body comprises a material layer made of one material; and
the coefficient of thermal expansion of the adjustment block is less than a coefficient of thermal expansion of the material layer.

### Claim 3 (depends on 1)

The stiffener ring according to claim 1, wherein the stiffener ring body comprises two material layers, and a lamination direction of the two material layers is perpendicular to a surface that is of the stiffener ring and that is used for being attached to the substrate; and
a warpage direction of thermal expansion of the stiffener ring body is opposite to a warpage direction of thermal expansion of the substrate.

### Claim 4 (depends on 3)

The stiffener ring according to claim 3, wherein when the stiffener ring is laminated on the substrate, a coefficient of thermal expansion of a material layer close to the substrate is less than a coefficient of thermal expansion of a material layer away from the substrate; or
a coefficient of thermal expansion of a material layer close to the substrate is greater than a coefficient of thermal expansion of a material layer away from the substrate.

### Claim 5 (depends on 1)

The stiffener ring according to claim 1, wherein the stiffener ring comprises three material layers, and two outer material layers are material layers of a same coefficient of thermal expansion, and a coefficient of thermal expansion of a middle material layer is different from the coefficient of thermal expansion of the outer material layers.

### Claim 6 (depends on 1)

The stiffener ring according to claim 1, wherein the stiffener ring body has a first side wall and a second side wall that are opposite, and a distance between the first side wall and a chip is less than a distance between the second side wall and the chip;
the adjustment block comprises a first adjustment block group and a second adjustment block group;
the first adjustment block group comprises at least one first adjustment block, and first adjustment blocks are disposed in a one-to-one correspondence at corners of the first side wall;
the second adjustment block group comprises at least one second adjustment block, and second adjustment blocks are disposed in a one-to-one correspondence at corners of the second side wall; and
a coefficient of expansion of the second adjustment block is less than a coefficient of expansion of the first adjustment block.

### Claim 7 (depends on 1)

The stiffener ring according to claim 1, wherein stiffness of the adjustment block is greater than stiffness of the stiffener ring body.

### Claim 8 (depends on 7)

The stiffener ring according to claim 7, wherein the stiffener ring body comprises at least one material layer, and the stiffness of the adjustment block is greater than stiffness of the material layer.

### Claim 9 (depends on 1)

The stiffener ring according to claim 1, wherein the adjustment block is welded or bonded to the stiffener ring body.

### Claim 10 (depends on 1)

The stiffener ring according to claim 1, wherein a gap corresponding to each adjustment block is disposed at the corner of the stiffener ring body.

### Claim 11 (depends on 1)

The stiffener ring according to claim 1, wherein the adjustment block may be of a triangular structure, a circular structure, or a fan-shaped structure.

### Claim 12 (depends on 1)

The stiffener ring according to claim 1, wherein the stiffener ring is used in a chip in an FC-BGA package or a Flip chip package.

### Claim 13

A surface packaging assembly, comprising a laminated substrate and a chip, wherein the substrate is electrically connected to the chip, and further comprising a stiffener ring configured to correct warpage of a substrate of a surface packaging assembly;
wherein the stiffener ring comprises an annular stiffener ring body and an adjustment block that is disposed at a same layer as the stiffener ring body and that is fastened to at least one corner of the stiffener ring body; and a coefficient of thermal expansion of the adjustment block is less than a coefficient of thermal expansion of the stiffener ring body;
wherein, the stiffener ring is sleeved outside the chip, and the stiffener ring is laminated on and fastened to the substrate.

### Claim 14 (depends on 13)

The surface packaging assembly according to claim 13, wherein the stiffener ring body comprises a material layer made of one material; and
the coefficient of thermal expansion of the adjustment block is less than a coefficient of thermal expansion of the material layer.

### Claim 15 (depends on 13)

The surface packaging assembly according to claim 13, wherein the stiffener ring body comprises two material layers, and a lamination direction of the two material layers is perpendicular to a surface that is of the stiffener ring and that is used for being attached to the substrate; and
a warpage direction of thermal expansion of the stiffener ring body is opposite to a warpage direction of thermal expansion of the substrate.

### Claim 16 (depends on 15)

The surface packaging assembly according to claim 15, wherein when the stiffener ring is laminated on the substrate, a coefficient of thermal expansion of a material layer close to the substrate is less than a coefficient of thermal expansion of a material layer away from the substrate; or
a coefficient of thermal expansion of a material layer close to the substrate is greater than a coefficient of thermal expansion of a material layer away from the substrate.

### Claim 17 (depends on 13)

The surface packaging assembly according to claim 13, wherein the stiffener ring comprises three material layers, and two outer material layers are material layers of a same coefficient of thermal expansion, and a coefficient of thermal expansion of a middle material layer is different from the coefficient of thermal expansion of the outer material layers.

### Claim 18 (depends on 13)

The surface packaging assembly according to claim 13, wherein the stiffener ring body has a first side wall and a second side wall that are opposite, and a distance between the first side wall and a chip is less than a distance between the second side wall and the chip;
the adjustment block comprises a first adjustment block group and a second adjustment block group;
the first adjustment block group comprises at least one first adjustment block, and first adjustment blocks are disposed in a one-to-one correspondence at corners of the first side wall;
the second adjustment block group comprises at least one second adjustment block, and second adjustment blocks are disposed in a one-to-one correspondence at corners of the second side wall; and
a coefficient of expansion of the second adjustment block is less than a coefficient of expansion of the first adjustment block.

### Claim 19 (depends on 13)

The surface packaging assembly according to claim 13, wherein stiffness of the adjustment block is greater than stiffness of the stiffener ring body.

### Claim 20 (depends on 19)

The surface packaging assembly according to claim 19, wherein the stiffener ring body comprises at least one material layer, and the stiffness of the adjustment block is greater than stiffness of the material layer.