# US 2023/0065803 A1 · Neutron Detectors and Methods of Fabricating the Same Using Boron as Neutron Conversion Layer and Conformal Doping Source

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0065803 A1
- Document ID: US20230065803A1
- Status: Published application
- Kind: A1
- Application number: 17/759,802
- Filed: 2021-01-29
- Published: 2023-03-02
- Earliest claimed: 2020-01-31
- Assignees: Board of Regents, The University of Texas System
- Applicants: Board of Regents, The University of Texas System
- Inventors: Siddartha Srinivasan Nandagopala Krishnan; Jesus Alfonso Caraveo Frescas; Carlos Hugo Avila-Avendano; Manuel Quevedo Lopez
- Web page: https://patentgrep.com/patent/US20230065803A1

## CPC

- G01T 3/08: with semiconductor detectors
- H10F 30/29: the devices being sensitive to radiation having very short wavelengths, e.g. X-rays, gamma-rays or corpuscular radiation
- H10F 30/295: Surface barrier or shallow PN junction radiation detectors, e.g. surface barrier alpha-particle detectors
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/1223: characterised by the dopants
- H10F 77/148: {Shapes of potential barriers}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Thermal neutron detectors and methods of fabricating the same are provided. A thermal neutron detector can use boron in both the neutron conversion layer and as a source for conformal doping in a semiconductor substrate. The neutron detector can be a micro-structured diode with cavities having a depth of 60 microns or less. The boron can be filled in the cavities and diffused into the semiconductor substrate via a diffusion annealing process.

## Claims

### Claim 1

A method of fabricating a thermal neutron detector, the method comprising:
performing n-type doping on a first surface of a semiconductor substrate;
performing p-type doping on a second surface of the semiconductor substrate using a p-type dopant material, the second surface being opposite from the first surface;
etching microstructures in the second surface of the semiconductor substrate;
backfilling the p-type dopant material in the microstructures; and
performing diffusion annealing on the semiconductor substrate having the p-type dopant material backfilled in the microstructures such that at least one element from the p-type dopant material diffuses into the semiconductor substrate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the p-type dopant material comprises boron, and wherein the at least one element from the p-type dopant material comprises boron.

### Claim 3 (depends on 1)

The method according to claim 1, wherein each microstructure of the microstructures etched in the second surface of the semiconductor substrate has a depth of 500 μm or less.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising:
before performing the p-type doping on the second surface of the semiconductor substrate, depositing an insulating layer dielectric on the second surface of the semiconductor substrate to leave an active pattern exposed on the second surface, wherein the p-type doping is performed on the active pattern.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the n-type doping uses an n-type dopant material comprising at least one of phosphorous and lithium.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the p-type dopant material is a powder comprising boron.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the p-type dopant material comprises boron-10 (10B).

### Claim 8

(canceled)

### Claim 9 (depends on 1)

The method according to claim 1, further comprising depositing a first electrical contact on the first surface of the semiconductor substrate and a second electrical contact on the second surface of the semiconductor substrate.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the microstructures are etched in the second surface of the semiconductor substrate using reactive ion etching (RIE).

### Claim 11 (depends on 1)

The method according to claim 1, wherein the microstructures are etched in the second surface of the semiconductor substrate using a wet etching process.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the p-type doping is performed by spin-on-glass doping, and
wherein the n-type doping is performed by solid state diffusion.

### Claim 13 (depends on 1)

The method according to claim 1, wherein at least one microstructure of the microstructures etched in the second surface of the semiconductor substrate has a circular hole geometry.

### Claim 14 (depends on 1)

The method according to claim 1, wherein at least one microstructure of the microstructures etched in the second surface of the semiconductor substrate has a square hole geometry.

### Claim 15 (depends on 1)

The method according to claim 1, wherein at least one microstructure of the microstructures etched in the second surface of the semiconductor substrate has a trench geometry.

### Claim 16 (depends on 1)

The method according to claim 1, wherein each microstructure of the microstructures etched in the second surface of the semiconductor substrate has a circular hole geometry with an opening radius of 4 μm and a depth of no more than 60 μm.

### Claim 17 (depends on 1)

The method according to claim 1, wherein each microstructure of the microstructures etched in the second surface of the semiconductor substrate has a depth of 60 μm or less,
wherein the method further comprises:
before performing the p-type doping on the second surface of the semiconductor substrate, depositing an insulating layer dielectric on the second surface of the semiconductor substrate to leave an active pattern exposed on the second surface, wherein the p-type doping is performed on the active pattern; and
depositing a first electrical contact on the first surface of the semiconductor substrate and a second electrical contact on the second surface of the semiconductor substrate, wherein the p-type dopant material is a powder comprising 10B,
wherein the microstructures are etched in the second surface of the semiconductor substrate using RIE, and
wherein at least one microstructure of the microstructures etched in the second surface of the semiconductor substrate has a circular hole geometry, a square hole geometry, or a trench geometry.

### Claim at position 18

18-19. (canceled)

### Claim 20 (depends on 1)

The method according to claim 1, wherein a thermal neutron detection efficiency of the fabricated thermal neutron detector is in a range of from 12.5% to 21%.

### Claim 21

A thermal neutron detector, comprising:
a semiconductor substrate comprising microstructures on a first surface thereof,
wherein the semiconductor substrate comprises:
an n-doped section formed by n-type doping on a second surface of the semiconductor substrate, the second surface being opposite from the first surface; and
a p-doped section formed by p-type doping on the first surface of the semiconductor substrate using a p-type dopant material,
wherein the p-type dopant material is filled in the microstructures,
wherein diffusion annealing has been performed on the semiconductor substrate having the p-type dopant material backfilled in the microstructures such that at least one element from the p-type dopant material has diffused into the semiconductor substrate through sidewalls of the microstructures, and
wherein each microstructure of the microstructures in the first surface of the semiconductor substrate has a depth of 500 μm or less.

### Claim 22 (depends on 21)

The thermal neutron detector according to claim 21, wherein the p-type dopant material comprises boron, and wherein the at least one element from the p-type dopant material comprises boron.

### Claim 23 (depends on 21)

The thermal neutron detector according to claim 21, wherein the p-type dopant material comprises 10B.

### Claim 24 (depends on 21)

The thermal neutron detector according to claim 21, further comprising:
a first electrical contact on the first surface of the semiconductor substrate; and
a second electrical contact on the second surface of the semiconductor substrate.

### Claim 25 (depends on 21)

The thermal neutron detector according to claim 21, wherein at least one microstructure of the microstructures etched in the second surface of the semiconductor substrate has a circular hole geometry, a square hole geometry, or a trench geometry.

### Claim 26 (depends on 21)

The thermal neutron detector according to claim 21, wherein each microstructure of the microstructures etched in the second surface of the semiconductor substrate has a circular hole geometry with an opening radius of 4 μm and a depth of no more than 60 μm.

### Claim at position 26

27-28. (canceled)

### Claim 29 (depends on 21)

The thermal neutron detector according to claim 21, wherein a thermal neutron detection efficiency of the thermal neutron detector is in a range of from 12.5% to 21%.