# US 2023/0065793 A1 · Heterogenous bonding layers for direct semiconductor bonding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0065793 A1
- Document ID: US20230065793A1
- Status: Published application
- Kind: A1
- Application number: 17/446,549
- Filed: 2021-08-31
- Published: 2023-03-02
- Earliest claimed: 2021-08-31
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Limited
- Inventors: Kuang-Wei CHENG; Chyi-Tsong NI
- Web page: https://patentgrep.com/patent/US20230065793A1

## CPC

- H10W 90/00: Package configurations
- H10W 72/073: {of die-attach connectors}
- H10W 72/30: Die-attach connectors
- H10W 80/00: Direct bonding of chips, wafers or substrates
- H10W 72/07331: {Connecting techniques}
- H10W 90/732: {between stacked chips}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A first semiconductor device and a second semiconductor device may be directly bonded using heterogeneous bonding layers. A first bonding layer may be formed on the first semiconductor device and the second bonding layer may be formed on the second semiconductor device. The first bonding layer may include a higher concentration of hydroxy-containing silicon relative to the second bonding layer. The second bonding layer may include silicon with a higher concentration of nitrogen relative to the first bonding layer. An anneal may be performed to cause a dehydration reaction that results in decomposition of the hydroxy components of the first bonding layer, which forms silicon oxide bonds between the first bonding layer and the second bonding layer. The nitrogen in the second bonding layer increases the effectiveness of the dehydration reaction and the effectiveness and strength of the bond between the first bonding layer and the second bonding layer.

## Claims

### Claim 1

A method, comprising:
forming a first bonding layer on a surface of a first semiconductor device;
forming a second bonding layer on a surface of a second semiconductor device,
wherein a chemical composition of the first bonding layer is different from a chemical composition of the second bonding layer to promote bonding between the first semiconductor device and the second semiconductor device; and
performing an annealing operation to bond the first semiconductor device with the second semiconductor device via the first bonding layer and the second bonding layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first bonding layer and the second bonding layer each includes a thickness in a range from approximately 10 angstroms to approximately 100,000 angstroms.

### Claim 3 (depends on 1)

The method of claim 1, wherein a silicon-to-nitrogen ratio of the chemical composition of the first bonding layer is greater relative to a silicon-to-nitrogen ratio of the chemical composition of the second bonding layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the chemical composition of the first bonding layer comprises a hydroxy-containing silicon dioxide; and
wherein the chemical composition of the second bonding layer comprises a silicon nitride.

### Claim 5 (depends on 1)

The method of claim 1, wherein performing the annealing operation to bond the first semiconductor device with the second semiconductor device via the first bonding layer and the second bonding layer comprises:
performing the annealing operation to bond the first semiconductor device with the second semiconductor device via the first bonding layer and the second bonding layer without pretreating the first bonding layer or the second bonding layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein performing the annealing operation to bond the first semiconductor device with the second semiconductor device via the first bonding layer and the second bonding layer comprises:
performing the annealing operation to fuse the first bonding layer and the second bonding layer,
wherein the chemical composition of the first bonding layer and the chemical composition of the second bonding layer cause formation of silicon-oxygen-silicon bonds between the first bonding layer and the second bonding layer to directly bond the first semiconductor device and the second semiconductor device.

### Claim 7 (depends on 1)

The method of claim 1, wherein a roughness of the first bonding layer or the second bonding layer is less than approximately 1 angstrom.

### Claim 8

A device, comprising:
a first semiconductor device;
a second semiconductor device; and
a first bonding layer and a second bonding layer, both joining the first semiconductor device and the second semiconductor device,
wherein a chemical composition of the first bonding layer includes a greater silicon concentration relative to a chemical composition of the second bonding layer to cause formation of silicon-oxygen-silicon bonds between the first bonding layer and the second bonding layer, and
wherein the chemical composition of the second bonding layer includes a greater nitrogen concentration relative to the chemical composition of the first bonding layer to increase the formation of the silicon-oxygen-silicon bonds between the first bonding layer and the second bonding layer.

### Claim 9 (depends on 8)

The device of claim 8, wherein a silicon-to-nitrogen ratio of the chemical composition of the first bonding layer is in a range of approximately 20 to approximately 1000.

### Claim 10 (depends on 8)

The device of claim 8, wherein a silicon-to-nitrogen ratio of the chemical composition of the second bonding layer is in a range of approximately 0.5 to approximately 2.

### Claim 11 (depends on 8)

The device of claim 8, wherein the first bonding layer includes at least one of:
silicon oxide,
silicon dioxide, or
a silicon oxycarbide.

### Claim 12 (depends on 8)

The device of claim 8, wherein the second bonding layer includes at least one of:
a silicon nitride,
a silicon carbon nitride, or
a silicon oxynitride.

### Claim 13 (depends on 8)

The device of claim 8, wherein a bond between the first bonding layer and the second bonding layer comprises a silicon-oxygen-silicon bond.

### Claim 14 (depends on 8)

The device of claim 8, wherein a bonding strength between the first bonding layer and the second bonding layer is greater than two Joules per square meter to enable direct bonding of the first semiconductor device and the second semiconductor device.

### Claim 15

A method, comprising:
forming a first bonding layer on a surface of a first semiconductor device;
forming a second bonding layer on a surface of a second semiconductor device; and
performing an annealing operation to bond the first semiconductor device and the second semiconductor device via the first bonding layer and the second bonding layer,
wherein a hydroxy-containing silicon concentration of the first bonding layer results in formation of silicon-oxygen-silicon bonds during the annealing operation, and
wherein a nitrogen concentration of the second bonding layer increases the formation of the silicon-oxygen-silicon bonds during the annealing operation.

### Claim 16 (depends on 15)

The method of claim 15, wherein a silicon-to-nitrogen ratio of the first bonding layer is approximately 20 or greater.

### Claim 17 (depends on 15)

The method of claim 15, wherein a silicon-to-nitrogen ratio of the second bonding layer is approximately 2 or less.

### Claim 18 (depends on 15)

The method of claim 15, wherein the nitrogen concentration of the second bonding layer increases effectiveness of a dehydration reaction that occurs between the first bonding layer and the second bonding layer during the annealing operation.

### Claim 19 (depends on 15)

The method of claim 15, wherein performing the annealing operation to bond the first semiconductor device and the second semiconductor device via the first bonding layer and the second bonding layer comprises:
performing the annealing operation to bond the first semiconductor device and the second semiconductor device via the first bonding layer and the second bonding layer without performing a pretreatment process for the first bonding layer and the second bonding layer prior to the annealing operation.

### Claim 20 (depends on 15)

The method of claim 15, wherein performing the annealing operation to bond the first semiconductor device and the second semiconductor device via the first bonding layer and the second bonding layer comprises:
performing the annealing operation, at a temperature in a range from approximately 150 degrees Celsius to approximately 400 degrees Celsius and for a time period in a range from approximately 30 minutes to approximately 3 hours, to fuse the first bonding layer and the second bonding layer.