# US 2023/0061312 A1 · Method for preparing semiconductor device with wire bond

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0061312 A1
- Document ID: US20230061312A1
- Status: Published application
- Kind: A1
- Application number: 17/465,328
- Filed: 2021-09-02
- Published: 2023-03-02
- Earliest claimed: 2021-09-02
- Assignees: Nanya Technology Corporation
- Applicants: Nanya Technology Corporation
- Inventors: WEI-ZHONG LI; YI-TING SHIH; CHIEN-CHUNG WANG; HSIH-YANG CHIU
- Web page: https://patentgrep.com/patent/US20230061312A1

## CPC

- H10W 72/019: {of bond pads}
- H10W 72/90: Bond pads, in general
- H10W 72/01553: {by etching}
- H10W 72/01953: {by etching}
- H10W 72/075: {of bond wires}
- H10W 72/07511: {Treating the bonding area before connecting, e.g. by applying flux or cleaning}
- H10W 72/536: {the connected ends being ball-shaped}
- H10W 72/551: {Materials of bond wires}
- H10W 72/5524: {comprising aluminium [Al]}
- H10W 72/5525: {comprising copper [Cu]}
- H10W 72/59: Bond pads specially adapted therefor
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/983: {Reinforcing structures, e.g. collars}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for preparing a semiconductor device includes providing an integrated circuit die having a bond pad. The bond pad includes aluminum (Al). The method also includes etching a top portion of the bond pad to form a recess, and bonding a wire bond to the recess in the bond pad. The wire bond includes copper (Cu).

## Claims

### Claim 1

A method for preparing a semiconductor device, comprising:
providing an integrated circuit die having a bond pad, wherein the bond pad includes aluminum (Al);
etching a top portion of the bond pad to form a recess; and
bonding a wire bond to the recess in the bond pad, wherein the wire bond includes copper (Cu).

### Claim 2 (depends on 1)

The method for preparing a semiconductor device of claim 1, wherein a maximum width of the recess in the bond pad is greater than or equal to a maximum width of the wire bond in a cross-sectional view.

### Claim 3 (depends on 1)

The method for preparing a semiconductor device of claim 1, wherein a maximum depth of the recess in the bond pad is less than or equal to half of a thickness of the bond pad.

### Claim 4 (depends on 1)

The method for preparing a semiconductor device of claim 1, wherein before the recess is formed, the method further comprises:
forming a first dielectric layer over the bond pad;
forming a second dielectric layer over the first dielectric layer; and
etching the first dielectric layer and the second dielectric layer using a first photoresist layer as a mask to form a first opening exposing the bond pad.

### Claim 5 (depends on 4)

The method for preparing a semiconductor device of claim 4, wherein before the recess is formed, the method further comprises:
forming a second photoresist layer over the first photoresist layer and extending into the first opening, wherein the second photoresist layer has a second opening exposing the bonding pad.

### Claim 6 (depends on 5)

The method for preparing a semiconductor device of claim 5, wherein a bottom width of the first opening is greater than a bottom width of the second opening.

### Claim 7 (depends on 5)

The method for preparing a semiconductor device of claim 5, further comprising:
etching the top portion of the bond pad to form the recess through the second opening.

### Claim 8

A method for preparing a semiconductor device, comprising:
providing an integrated circuit die having a bond pad;
forming a first dielectric layer over the bond pad;
forming a second dielectric layer over the first dielectric layer;
etching the first dielectric layer and the second dielectric layer to form a first opening exposing a top surface area of the bond pad;
partially recessing the top surface area of the bond pad to form a concave depression; and
bonding a wire bond to the concave depression.

### Claim 9 (depends on 8)

The method for preparing a semiconductor device of claim 8, wherein the top surface area of the bond pad exposed by the first opening is greater than an area of the concave depression from a top view.

### Claim 10 (depends on 8)

The method for preparing a semiconductor device of claim 8, wherein a footprint of the concave depression is greater than or equal to a footprint of the wire bond.

### Claim 11 (depends on 8)

The method for preparing a semiconductor device of claim 8, wherein the bond pad includes aluminum (Al), and the wire bond includes copper (Cu).

### Claim 12 (depends on 8)

The method for preparing a semiconductor device of claim 8, wherein the first dielectric layer is made of an oxide, and the second dielectric layer is made of a nitride.

### Claim 13 (depends on 8)

The method for preparing a semiconductor device of claim 8, further comprising:
forming a first photoresist layer over the second dielectric layer, wherein the first opening is formed by using the first photoresist layer as a mask; and
forming a second photoresist layer over the first photoresist layer before the concave depression is formed.

### Claim 14 (depends on 13)

The method for preparing a semiconductor device of claim 13, wherein the second photoresist layer extends into the first opening to cover sidewalls of the first photoresist layer, sidewalls of the second dielectric layer, and sidewalls of the first dielectric layer, and the concave depression is formed by using the second photoresist layer as a mask.

### Claim 15

A method for preparing a semiconductor device, comprising:
providing an integrated circuit die having a bond pad, wherein the bond pad includes aluminum (Al);
forming a first dielectric layer over the bond pad;
forming a second dielectric layer over the first dielectric layer;
forming a first photoresist layer over the second dielectric layer;
etching the first dielectric layer and the second dielectric layer using the first photoresist layer as a mask to form an opening;
forming a second photoresist layer over the first photoresist layer and extending into the opening;
etching the bond pad using the second photoresist layer as a mask to form a recess; and
performing a bonding process to bond a wire bond to the recess of the bond pad, wherein the wire bond includes copper (Cu).

### Claim 16 (depends on 15)

The method for preparing a semiconductor device of claim 15, wherein a top surface area of the bond pad exposed by the opening is partially covered by the second photoresist layer.

### Claim 17 (depends on 15)

The method for preparing a semiconductor device of claim 15, further comprising:
removing the second photoresist layer before the wire bond is bonded to the recess.

### Claim 18 (depends on 15)

The method for preparing a semiconductor device of claim 15, wherein a splash is formed around the wire bond and in the opening during the bonding process.

### Claim 19 (depends on 18)

The method for preparing a semiconductor device of claim 18, wherein the splash is formed from the bond pad.

### Claim 20 (depends on 18)

The method for preparing a semiconductor device of claim 18, wherein the splash does not extend above a top surface of the first photoresist layer.