# US 2023/0059329 A1 · Method for constructing molds and cores layer by layer by means of a binder containing water glass, and a binder containing water glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0059329 A1
- Document ID: US20230059329A1
- Status: Published application
- Kind: A1
- Application number: 18/046,191
- Filed: 2022-10-13
- Published: 2023-02-23
- Earliest claimed: 2014-12-12
- Assignees: ASK Chemicals GmbH
- Applicants: ASK Chemicals GmbH
- Inventors: Heinz Deters; Henning Zupan
- Web page: https://patentgrep.com/patent/US20230059329A1

## CPC

- B22C 1/188: {Alkali metal silicates}
- B22C 9/02: Sand moulds or like moulds for shaped castings
- B22C 9/10: Cores; Manufacture or installation of cores {(breaker cores B22C9/084)}
- B28B 1/001: {Rapid manufacturing of 3D objects by additive depositing, agglomerating or laminating of material (selective deposition modelling of metallic powder B22F10/00; rapid manufacturing of 3D objects in general and in particular of plastics B29C64/00)}
- B28B 11/241: {using microwave heating means}
- B29C 64/165: using a combination of solid and fluid materials, e.g. a powder selectively bound by a liquid binder, catalyst, inhibitor or energy absorber
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- B33Y 10/00: Processes of additive manufacturing
- B33Y 50/02: for controlling or regulating additive manufacturing processes
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C04B 35/14: based on silica
- C04B 35/6303: {Inorganic additives}
- C04B 35/6313: {Alkali metal or alkaline earth metal phosphates}
- C04B 35/6316: {Binders based on silicon compounds}
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3409: Boron oxide, borates, boric acids, or oxide forming salts thereof, e.g. borax
- C04B 2235/3427: Silicates other than clay, e.g. water glass
- C04B 2235/5427: millimeter or submillimeter sized, i.e. larger than 0,1 mm
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/6026: Computer aided shaping, e.g. rapid prototyping
- C04B 2235/667: Sintering using wave energy, e.g. microwave sintering
- C04B 2237/704: of one or more of the ceramic layers or articles
- Y02P 10/25: Process efficiency
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The invention relates to a binder, which contains water glass and further a phosphate or a borate or both. The invention further relates to a method for constructing molds and cores layer by layer, the molds and cores comprising a construction material mixture, which at least comprises a refractory molding base material, and the binder. In order to produce the molds and cores layer by layer in 3-D printing, the refractory molding base material is applied layer by layer and is selectively printed with the binder layer by layer, and consequently a body corresponding to the molds or cores is constructed and the molds or cores are released after the unbonded construction material mixture has been removed.

## Claims

### Claim 1

A method for constructing bodies layer by layer, comprising at least the following steps:
a) providing a refractory molding base material as a component of a construction material mixture;
b) spreading a thin layer of the construction material mixture with a layer thickness of 0.05 mm to 3 mm;
c) printing selected areas of the thin layer with a binder having a dynamic viscosity at 25° C. of greater than 1 mPas and less than 25 mPas, comprising
water glass in the form of an aqueous alkali silicate solution, the water glass having a molar ratio of Na2O/M2O of greater than 0.4 and a molar modulus SiO2/M2O of greater 1.4 to less than 2.8, and
at least one phosphate or at least one borate or phosphate and borate; and
d) repeatedly repeating steps b) and c).

### Claim 2 (depends on 1)

The method according to claim 1, wherein the thin layer of the construction material mixture is spread with a layer thickness of 0.1 mm to 1 mm.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising the step of curing the printed areas.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the curing is performed by temperature increase.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the temperature increase is effected by microwaves and/or infrared light.

### Claim 6 (depends on 3)

The method according to claim 3, wherein the curing of the printed areas takes place in each case after constructing 1 to 10 printed layers of the construction material mixture.

### Claim 7 (depends on 3)

The method according to claim 3, wherein the curing of the printed areas takes place in each case after constructing 3 to 8 printed layers of the construction material mixture.

### Claim 8

The method according to at least one of the preceding claims, further comprising the following steps:
i) curing the body after completion of the layer by layer construction in a furnace or by means of a microwave, and subsequent
ii) removing the unbonded construction material mixture from the at least partially cured casting mold.

### Claim 9

The method according to at least one of the preceding claims, wherein the refractory molding base material comprises quartz sand, zirconium sand or chromium ore sand, olivine, vermiculite, bauxite, fire clay, glass beads, glass granules, hollow aluminum silicate microspheres and mixtures thereof.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the refractory molding base material consists of more than 50% by weight of quartz sand.

### Claim 11

The method according to at least one of the preceding claims, wherein more than 80% by weight of the construction material mixture is refractory molding base material.

### Claim 12

The method according to at least one of the preceding claims, wherein more than 95% by weight of the construction material mixture is refractory molding base material.

### Claim 13

The method according to at least one of the preceding claims, wherein the refractory molding base material has average grain diameters from 50 μm to 600 μm determined by sieving analysis.

### Claim 14

The method according to at least one of the preceding claims, wherein the refractory molding base material has average grain diameters between 80 μm and 300 μm, determined by sieving analysis.

### Claim 15

The method according to at least one of the preceding claims, wherein the water glass, including solvent/diluent, is used in an amount of between 0.5% by weight and 7% by weight based on the molding base material.

### Claim 16

The method according to at least one of the preceding claims, wherein the water glass, including solvent/diluent, is used in an amount of between 1% by weight and 5.0% by weight, based on the molding base material.

### Claim 17

The method according to at least one of the preceding claims, wherein an inorganic curing agent for water glass-based binders is added to the construction material mixture.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the inorganic curing agent is a phosphate.

### Claim 19 (depends on 17, 18)

The method according to claim 17 or 18, wherein the proportion of the curing agent relative to the binder is greater than or equal to 5 to less than 25% by weight.

### Claim 20 (depends on 17, 18)

The method according to claim 17 or 18, wherein the proportion of the curing agent relative to the binder is greater than or equal to 10 to less than 15% by weight.

### Claim 21 (depends on 17)

The method according to claim 17, wherein between 0.05% by weight and 2% by weight of the inorganic curing agent is used based on the molding base material.

### Claim 22 (depends on 17)

The method according to claim 17, wherein between 0.1% by weight and 0.6% by weight of the inorganic curing agent is used based on the molding base material.

### Claim 23

The method according to at least one of the preceding claims, wherein the printing is carried out with a printing head having a plurality of nozzles.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the nozzles are individually selectively controllable.

### Claim 25 (depends on 23, 24)

The method according to claim 23 or 24, wherein the print head is movable in at least one plane controlled by a computer, and the nozzles apply the liquid binder layer by layer.

### Claim 26 (depends on 23, 24, 25)

The method according to claim 23, 24 or claim 25, wherein the print head is a drop-on-demand print head with bubble-jet or piezo technology.

### Claim 27

The method according to at least one of the preceding claims, wherein the at least one phosphate is sodium hexametaphosphate or sodium polyphosphate.

### Claim 28 (depends on 1)

The method according claim 1, wherein the at least one phosphate is an alkali phosphate.

### Claim 29 (depends on 1)

The method according claim 1, wherein the at least one phosphate is sodium polyphosphate or sodium metaphosphate or both.

### Claim 30

The method according to at least one of the preceding claims, wherein the binder contains phosphates.

### Claim 31 (depends on 30)

The method according to claim 30, wherein the binder contains phosphates in a molar ratio of P2O5/SiO2 (calculated as P2O5 and relative to SiO2 in the binder) of greater than 0.01 and less than 0.5.

### Claim 32

The method according to at least one of the preceding claims, wherein the binder contains borates.

### Claim 33 (depends on 32)

The method according to claim 32, wherein the binder contains borates in a molar ratio of B2O3/SiO2 (calculated as B2O3 and SiO2 in the binder) from 0.01 to 0.5.

### Claim 34

The method according to at least one of the preceding claims, wherein the at least one borate is an alkali borate.

### Claim 35 (depends on 34)

The method according to claim 34, wherein the at least one borate is disodium tetraborate decahydrate.

### Claim 36

A binder, comprising
water glass with a molar ratio of Na2O/M2O of greater than 0.4 and a molar modulus SiO2/M2O of greater 1.4 to less than 2.8,
wherein in each case an amount of M2O is the sum of the mass quantities of lithium, sodium and potassium calculated as oxide, based on the amorphous alkali silicates, alkali oxides, alkali hydroxides, alkali phosphates and/or alkali borates contained in the binder; and
wherein
the binder contains at least one phosphate or at least one borate or phosphate and borate; and
the binder has a dynamic viscosity at 25° C. of greater than 1 mPas and less than 25 mPas.

### Claim 37 (depends on 36)

The binder according to claim 36, wherein any particulate constituents in the binder have a D90 value of less than 70 μm.

### Claim 38 (depends on 36, 37)

The binder according to claim 36 or 37, wherein the binder comprises water glass with a molar ratio of Na2O/M2O of greater than 0.7 and a molar modulus SiO2/M2O of greater 1.9 and less than 2.4.

### Claim 39 (depends on 36)

The binder according to claim 36, wherein the binder has a solids content of greater than 22 to less than 40% by weight.

### Claim 40 (depends on 39)

The binder according to claim 39, wherein the binder has a solids content of greater than 28 to less than 35% by weight.

### Claim 41 (depends on 36, 37, 38, 39, 40)

The binder according to one of claims 36 to 40, wherein particles in the binder
have a D90 value of less than 40 μm and/or
have a D100 value of less than 250 μm.

### Claim 42 (depends on 36, 37, 38, 39, 40)

The binder according to one of claims 36 to 40, wherein particles in the binder
have a D90 value of less than 20 μm, and/or
have a D100 value of less than 30 μm.

### Claim 43 (depends on 36, 37, 38, 39, 40, 41, 42)

The binder according to at least one of claims 36 to 42, wherein the at least one phosphate is sodium hexametaphosphate or sodium polyphosphate.

### Claim 44 (depends on 36)

The binder according to claim 36, wherein the at least one phosphate is sodium polyphosphate or sodium metaphosphate or both.

### Claim 45 (depends on 36, 37, 38, 39, 40, 41, 42, 43, 44)

The binder according to at least one of claims 36 to 44, wherein the binder contains phosphates.

### Claim 46 (depends on 45)

The binder according to claim 45, wherein the binder contains phosphates in a molar ratio of P2O5/SiO2 (calculated as P2O5 and relative to the SiO2 in the binder) of greater than 0.01 and less than 0.5.

### Claim 47 (depends on 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46)

The binder according to at least one of claims 36 to 46, wherein the binder contains borates and preferably the molar ratio B2O3/SiO2 (calculated as B2O3 and SiO2 in the binder) is from 0.01 to 0.5.

### Claim 48 (depends on 47)

The binder according to claim 47, wherein the binder contains borates in a molar ratio B2O3/SiO2 (calculated as B2O3 and SiO2 in the binder) from 0.01 to 0.5.

### Claim 49 (depends on 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48)

The binder according to at least one of claims 36 to 48, wherein the at least one borate is an alkali borate.

### Claim 50 (depends on 49)

The binder according to claim 49, wherein the at least one borate is disodium tetraborate decahydrate.

### Claim 51 (depends on 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50)

The binder according to at least one of claims 36 to 50, wherein the binder further contains surface-active substances.

### Claim 52 (depends on 51)

The binder according to claim 51, wherein the binder contains surface-active substances in between 0.01 and 3.0% by weight.

### Claim 53 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26, 27, 28, 29, 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52)

The method according to at least one of the preceding claims 1 to 35, wherein the binder is further defined by any one of claims 36 to 52.