# US 2023/0059113 A1 · Cast steel alloy component having reduced ferrite and enhanced ultimate tensile strength for a vehicle

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0059113 A1
- Document ID: US20230059113A1
- Status: Published application
- Kind: A1
- Application number: 17/407,884
- Filed: 2021-08-20
- Published: 2023-02-23
- Earliest claimed: 2021-08-20
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Jianghuai Yang; Qigui Wang; Anil K. Sachdev
- Web page: https://patentgrep.com/patent/US20230059113A1

## CPC

- B22D 29/04: Handling or stripping castings or ingots (grippers in general, see the relevant subclasses, e.g. B66C)
- B22D 30/00: Cooling castings, not restricted to casting processes covered by a single main group (accessories for cooling cast stock in continuous casting of metals B22D11/124; controlling or regulating processes or operations for cooling cast stock or mould in continuous casting of metals B22D11/22; chill casting B22D15/00)
- B22D 35/04: into moulds, e.g. base plates, runners
- C22C 38/001: {containing N}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/50: with titanium or zirconium
- C21D 2211/005: Ferrite
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A cast steel alloy for an engine of a vehicle is provided. The cast steel alloy comprises 0.29 to 0.65 weight percent (wt %) carbon, 0.40 to 0.80 wt % silicon, 0.6 to 1.5 wt % manganese, up to 0.03 wt % phosphorus, 0.04 to 0.07 wt % sulfur, 0.8 to 1.4 wt % chromium, 0.2 to 0.6 wt % nickel, 0.15 to 0.55 wt % molybdenum, 0.25 to 2.0 wt % copper, up to 0.03 wt % titanium, 0.07 to 0.17 wt % vanadium, 0.02 to 0.06 wt % aluminum, up to 0.03 wt % nitrogen (N), and 0.01 to 0.06 wt % of at least one of cerium (Ce) and lanthanum. The cast steel alloy has unexpected and unconventional results such as reduced ferrite and enhanced strengths.

## Claims

### Claim 1

A method of casting a steel alloy having reduced ferrite and enhanced ultimate tensile strength for a component of an engine, the method comprising:
providing a mold of the component, the mold having at least one molded cavity;
melting a steel solution at between 1620 degrees Celsius (° C.) and 1700° C., the steel solution comprising at least one of carbon (C), silicon (Si), manganese (Mn), phosphorus (P), sulfur (S), chromium (Cr), nickel (Ni), molybdenum (Mo), copper (Cu), titanium (Ti), vanadium (V), aluminum (Al), and nitrogen (N), defining a raw charge;
adding a master alloy solute to the raw charge at between 1620° C. and 1700° C. to define the steel melt, the steel melt comprising greater than 0.29 weight percent (wt %) C, greater than 0.40 wt % Si, greater than 0.6 wt % Mn, up to 0.03 wt % P, greater than 0.04 wt % S, greater than 0.8 wt % Cr, about 0.2 wt % Ni, greater than 0.15 wt % Mo, greater than 0.25 wt % Cu, up to 0.03 wt % Ti, greater than 0.07 wt % V, greater than 0.02 wt % Al, up to 0.03 wt % N, and 0.01 to 0.06 wt % of at least one of cerium (Ce) and lanthanum (La),
wherein the steel melt has a target composition of 0.35 wt % C, 0.45 wt % Si, 1.0 wt % Mn, up to 0.03 wt % P, 0.06 wt % S, 1.0 wt % Cr, 0.2 wt % Ni, 0.25 wt % Mo, 0.45 wt % Cu, up to 0.03 wt % Ti, 0.1 wt % V, 0.03 wt % Al, 0.03 wt % N, and 0.02 wt % of at least one of Ce and La;
pouring the steel melt in the at least one molded cavity at about 1600° C.;
solidifying the target steel alloy in the at least one molded cavity at about 450° C.; and
separating the target steel alloy from the at least one molded cavity defining a cast steel component having reduced ferrite and enhanced strengths.

### Claim 2 (depends on 1)

The method of claim 1 wherein the steel melt comprises 0.02 wt % of La and Ce, the steel melt having a La—Ce weight ratio of greater than 2:1.

### Claim 3 (depends on 1)

The method of claim 1 wherein the steel melt comprises 0.02 wt % of Ce and La, the steel melt having a Ce—La weight ratio of greater than 2:1.

### Claim 4 (depends on 1)

The method of claim 1 wherein the cast steel component has an ultimate tensile strength of about 840 MPa and about 1100 MPa.

### Claim 5 (depends on 1)

The method of claim 1 wherein the cast steel component has an elongation percent of between about 7% and about 10%.

### Claim 6 (depends on 1)

The method of claim 1 wherein the step of separating comprises:
shaking out the at least one molded cavity from target steel alloy;
degating the target steel alloy after the step of shaking out;
cleaning the target steel alloy after the step of degating; and
inspecting the target steel alloy after the step of cleaning to define the cast steel component.

### Claim 7 (depends on 1)

The method of claim 1 wherein the step of providing comprises:
making the mold of the component, the mold having a pattern with dimensions identical to the cast steel component.

### Claim 8

A system for casting a steel alloy having reduced ferrite and enhanced strengths for a component of an engine, the system comprising:
a molding unit arranged to form a mold of the component, the mold having at least one molded cavity;
a furnace for melting a steel solution and a master alloy solute at between 1620 degrees Celsius (° C.) and 1700° C. to define a steel melt, the steel solution comprising at least one of carbon (C), silicon (Si), manganese (Mn), phosphorus (P), sulfur (S), chromium (Cr), nickel (Ni), molybdenum (Mo), copper (Cu), titanium (Ti), vanadium (V), aluminum (Al), and nitrogen (N),
wherein the steel solution comprises greater than 0.29 weight percent (wt %) C, greater than 0.40 wt % Si, greater than 0.6 wt % Mn, up to 0.03 wt % P, greater than 0.04 wt % S, greater than 0.8 wt % Cr, about 0.2 wt % Ni, greater than 0.15 wt % Mo, greater than 0.25 wt % Cu, up to 0.03 wt % Ti, greater than 0.07 wt % V, greater than 0.02 wt % Al, up to 0.03 wt % N, and 0.01 to 0.06 wt % of at least one of cerium (Ce) and lanthanum (La),
wherein the steel melt has a composition of 0.29 to 0.65 weight percent (wt %) carbon, 0.40 to 0.80 wt % silicon, 0.6 to 1.5 wt % manganese, up to 0.03 wt % phosphorus, 0.04 to 0.07 wt % sulfur, 0.8 to 1.4 wt % chromium, 0.2 to 0.6 wt % nickel, 0.15 to 0.55 wt % molybdenum, 0.25 to 2.0 wt % copper, up to 0.03 wt % titanium, 0.07 to 0.17 wt % vanadium, 0.02 to 0.06 wt % aluminum, up to 0.03 wt % nitrogen (N), and 0.01 to 0.06 wt % of at least one of cerium (Ce) and lanthanum;
a pouring mechanism for pouring the steel melt in the at least one molded cavity at about 1600° C.;
a cooling area for solidifying the target steel alloy in the at least one molded cavity at about 450° C.;
a separation unit for separating the target steel alloy from the at least one molded cavity defining a cast steel component having reduced ferrite and enhanced strengths;
a controller in communication with the molding unit, the furnace, the pouring mechanism, and the shakeout unit, the controller configured to control the molding unit, the furnace, the pouring mechanism, and the separation unit; and
a power source configured to power the molding unit, the furnace, the pouring mechanism, the separation unit, and the controller.

### Claim 9 (depends on 8)

The system of claim 8 wherein the steel melt comprises 0.02 wt % of La and Ce, the steel melt having a La—Ce weight ratio of greater than 2:1.

### Claim 10 (depends on 8)

The system of claim 8 wherein the steel melt comprises 0.02 wt % of Ce and La, the steel melt having a Ce—La weight ratio of greater than 2:1.

### Claim 11 (depends on 8)

The system of claim 8 wherein the cast steel component has an ultimate tensile strength of about 840 MPa and about 1100 MPa.

### Claim 12 (depends on 8)

The system of claim 8 wherein the cast steel component has an elongation percent of between about 7% and about 10%.

### Claim 13 (depends on 8)

The system of claim 8 wherein the separation unit is arranged to shakeout the at least one molded cavity from target steel alloy, degate the target steel alloy after shaking out the at least one molded cavity, clean the target steel alloy after degating the target steel alloy; and inspect the target steel alloy after the cleaning the target steel alloy, defining the cast steel component.

### Claim 14 (depends on 8)

The system of claim 8 wherein the steel melt has a target composition of 0.35 wt % C, 0.45 wt % Si, 1.0 wt % Mn, up to 0.03 wt % P, 0.06 wt % S, 1.0 wt % Cr, 0.2 wt % Ni, 0.25 wt % Mo, 0.45 wt % Cu, up to 0.03 wt % Ti, 0.1 wt % V, 0.03 wt % Al, 0.03 wt % N, and 0.02 wt % of at least one of Ce and La;

### Claim 15

A cast steel alloy comprising:
0.29 to 0.65 weight percent (wt %) carbon (C);
0.40 to 0.80 wt % silicon (Si);
0.6 to 1.5 wt % manganese (Mn);
up to 0.03 wt % phosphorus (P);
0.04 to 0.07 wt % sulfur (S);
0.8 to 1.4 wt % chromium (Cr);
0.2 to 0.6 wt % nickel (Ni);
0.15 to 0.55 wt % molybdenum (Mo);
0.25 to 2.0 wt % copper (Cu);
up to 0.03 wt % titanium (Ti);
0.07 to 0.17 wt % vanadium (V);
0.02 to 0.06 wt % aluminum (Al);
up to 0.03 wt % nitrogen (N); and
0.01 to 0.06 wt % of at least one of cerium (Ce) and lanthanum (La).

### Claim 16 (depends on 15)

The cast steel alloy of claim 15 wherein the cast steel component comprises:0.35 wt % C, 0.45 wt % Si, 1.0 wt % Mn, up to 0.03 wt % P, 0.06 wt % S, 1.0 wt % Cr, 0.2 wt % Ni, 0.25 wt % Mo, 0.45 wt % Cu, up to 0.03 wt % Ti, 0.1 wt % V, 0.03 wt % Al, 0.03 wt % N, and 0.02 wt % of at least one of Ce and La;

### Claim 17 (depends on 15)

The cast steel alloy of claim 15 wherein the steel alloy has a La—Ce weight ratio of greater than 2:1.

### Claim 18 (depends on 15)

The cast steel alloy of claim 15 wherein steel alloy has a Ce—La weight ratio of greater than 2:1.

### Claim 19 (depends on 15)

The cast steel alloy of claim 15 wherein the steel alloy has an ultimate tensile strength of about 840 MPa and about 1100 MPa.

### Claim 20 (depends on 15)

The cast steel alloy of claim 15 wherein the cast steel alloy is formed of a cast steel component.