# US 2023/0058907 A1 · Antiglare film and manufacturing method of antiglare film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0058907 A1
- Document ID: US20230058907A1
- Status: Published application
- Kind: A1
- Application number: 17/954,869
- Filed: 2022-09-28
- Published: 2023-02-23
- Earliest claimed: 2020-04-10
- Assignees: FUJIFILM Corporation
- Applicants: FUJIFILM Corporation
- Inventors: Nobuyuki AKUTAGAWA; Motoki ONISHI
- Web page: https://patentgrep.com/patent/US20230058907A1

## CPC

- B29D 11/00788: {Producing optical films}
- G02B 5/003: {Light absorbing elements}
- B29D 11/00865: {Applying coatings; tinting; colouring (printing, marking or copying processes B41M; identification in general G09F3/00; producing decorative effects in general B44C; positioning or marking of lenses B24B13/0055)}
- B32B 3/30: characterised by a layer formed with recesses or projections, e.g. {hollows, grooves, protuberances, ribs (apertured layer B32B3/266; layer with cavities or internal voids B32B3/26)}
- B32B 7/023: Optical properties
- G02B 1/14: Protective coatings, e.g. hard coatings
- G02B 5/0221: {the surface having an irregular structure (G02B5/0226 takes precedence)}
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

An antiglare film includes, in order: a substrate; a first layer; and a second layer with an uneven structure including elongated projection portions on a surface opposite to a substrate side and an arithmetic mean height Sa on that side of the substrate is 30 to 160 nm, an average distance between adjacent elongated projection portions is 5 to 80 μm, a content of particles having a particle diameter of 300 nm or more in the second layer is 0% to 0.1% by mass with respect to a total mass of the second layer, an average film thickness of the second layer is 0.3 to 3 μm, a haze of the antiglare film is 1% to 20%, and where a surface of the antiglare film on the opposite to the substrate side is rubbed 100 times with #0000 steel wool under a load of 1 kg/cm2, no scratch occurs.

## Claims

### Claim 1

An antiglare film comprising, in the following order:
a substrate;
a first layer; and
a second layer,
wherein the second layer has an uneven structure including elongated projection portions on a surface opposite to a side of the substrate,
an arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 30 to 160 nm,
an average distance between adjacent elongated projection portions in the uneven structure is 5 to 80 μm,
a content of particles having a particle diameter of 300 nm or more in the second layer is 0% to 0.1% by mass with respect to a total mass of the second layer,
an average film thickness of the second layer is 0.3 to 3 μm,
a haze of the antiglare film is 1% to 20%, and
in a case where a surface of the antiglare film opposite to the side of the substrate is rubbed 100 times back and forth with #0000 steel wool under a load of 1 kg/cm2, no scratch occurs.

### Claim 2 (depends on 1)

The antiglare film according to claim 1,
wherein an absolute value Δn of a difference between a refractive index n1 of the first layer and a refractive index n2 of the second layer, the Δn being represented by the following Equation (i), is 0.05 or less,
Δn=|n1−n2|. (i)

### Claim 3 (depends on 1)

The antiglare film according to claim 1,
wherein an absolute value ΔG of a difference between an elastic modulus G1 of the first layer and an elastic modulus G2 of the second layer, the ΔG being represented by the following Equation (ii), is 2 GPa or less,
ΔG=|G1−G2|. (ii)

### Claim 4 (depends on 2)

The antiglare film according to claim 2,
wherein an absolute value ΔG of a difference between an elastic modulus G1 of the first layer and an elastic modulus G2 of the second layer, the ΔG being represented by the following Equation (ii), is 2 GPa or less,
ΔG=|G1−G2|. (ii)

### Claim 5 (depends on 1)

The antiglare film according to claim 1,
wherein the arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 40 to 100 nm.

### Claim 6 (depends on 2)

The antiglare film according to claim 2,
wherein the arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 40 to 100 nm.

### Claim 7 (depends on 3)

The antiglare film according to claim 3,
wherein the arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 40 to 100 nm.

### Claim 8 (depends on 4)

The antiglare film according to claim 4,
wherein the arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 40 to 100 nm.

### Claim 9 (depends on 1)

The antiglare film according to claim 1,
wherein the haze of the antiglare film is 5% to 10%.

### Claim 10 (depends on 1)

The antiglare film according to claim 1,
wherein the average distance between adjacent elongated projection portions in the uneven structure is 5 to 15 μm.

### Claim 11

A manufacturing method of an antiglare film having a substrate, a first layer, and a second layer in this order, in which the second layer has an uneven structure including elongated projection portions on a surface opposite to a side of the substrate, an arithmetic mean height Sa of the surface of the second layer opposite to the side of the substrate is 30 to 160 nm, an average distance between adjacent elongated projection portions in the uneven structure is 5 to 80 μm, a content of particles having a particle diameter of 300 nm or more in the second layer is 0% to 0.1% by mass with respect to a total mass of the second layer, an average film thickness of the second layer is 0.3 to 3 μm a haze of the antiglare film is 1% to 20%, and in a case where a surface of the antiglare film opposite to the side of the substrate is rubbed 100 times back and forth with #0000 steel wool under a load of 1 kg/cm2, no scratch occurs, the manufacturing method comprising, in the following order:
coating the substrate with a composition for forming a first layer containing a polymerizable compound (a1) to form a first layer coating film;
semi-curing the first layer coating film;
coating the semi-cured first layer coating film with a composition for forming a second layer to form a second layer coating film; and
curing the semi-cured first layer coating film and the second layer coating film to form the first layer and the second layer.

### Claim 12 (depends on 11)

The manufacturing method of an antiglare film according to claim 11,
wherein an arithmetic mean height Sat of a surface of the first layer coating film semi-cured in the semi-curing, the surface being opposite to the side of the substrate, is 30 nm or less.

### Claim 13 (depends on 11)

The manufacturing method of an antiglare film according to claim 11,
wherein a consumption rate of polymerizable groups in the polytnerizable compound (a1) in the first layer coating film semi-cured in the semi-curing is 1% to 40%.

### Claim 14 (depends on 11)

The manufacturing method of an antiglare film according to claim 11,
wherein a recovery rate of the first layer coating film semi-cured in the semi-curing is 2% to 50%.