# US 2023/0058186 A1 · Ultra-shallow dopant and ohmic contact regions by solid state diffusion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0058186 A1
- Document ID: US20230058186A1
- Status: Published application
- Kind: A1
- Application number: 17/884,090
- Filed: 2022-08-09
- Published: 2023-02-23
- Earliest claimed: 2021-08-20
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Robert D. Clark
- Web page: https://patentgrep.com/patent/US20230058186A1

## CPC

- C23C 16/45553: {characterized by the use of precursors specially adapted for ALD}
- C23C 16/303: {Nitrides}
- C23C 16/308: {Oxynitrides}
- C23C 16/40: Oxides
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/56: After-treatment
- H10D 30/019: {of FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 30/501: {FETs having stacked nanowire, nanosheet or nanoribbon channels}
- H10D 62/119: {Nanowire, nanosheet or nanotube semiconductor bodies}
- H10D 62/121: {oriented parallel to substrates}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 32/1408: {from or through or into an external applied layer, e.g. photoresist or nitride layers}
- H10P 32/141: {the applied layer comprising oxides only}
- H10P 32/171: {being group IV material}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 14/6939: {characterised by the metal}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method of processing a substrate that includes: loading the substrate in a processing chamber, the substrate including a raised feature of a semiconductor; forming a conformal dopant layer on the raised feature by atomic layer deposition (ALD); forming a metal layer over the raised feature; thermally treating the dopant layer to form an ultra-shallow dopant region in the raised feature by diffusion of a dopant from the dopant layer into the raised feature; and thermally treating the metal layer to form an ohmic contact region in the raised feature by diffusion of a metal from the metal layer into the raised feature.

## Claims

### Claim 1

A method of processing a substrate, the method comprising:
loading the substrate in a processing chamber, the substrate comprising a raised feature of a semiconductor;
forming a conformal dopant layer on the raised feature by atomic layer deposition (ALD);
forming a metal layer over the raised feature;
thermally treating the dopant layer to form an ultra-shallow dopant region in the raised feature by diffusion of a dopant from the dopant layer into the raised feature; and
thermally treating the metal layer to form an ohmic contact region in the raised feature by diffusion of a metal from the metal layer into the raised feature.

### Claim 2 (depends on 1)

The method of claim 1, wherein thermally treating the dopant layer is performed prior to thermally treating the metal layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the dopant layer comprises an oxide of the dopant, a nitride of the dopant, or an oxynitride of the dopant and the ohmic contact region comprises a metal silicide.

### Claim 4 (depends on 1)

The method of claim 1, wherein the dopant is selected from a group consisting of boron (B), aluminum (Al), gallium (Ga), indium (In), and thallium (Tl), nitrogen (N), phosphorous (P), arsenic (As), antimony (Sb), and bismuth (Bi), wherein the metal comprises titanium (Ti), nickel (Ni), platinum (Pt), or tungsten (W).

### Claim 5 (depends on 1)

The method of claim 1, further comprising, after thermally treating the metal layer, removing remnants of the metal layer from the substrate.

### Claim 6 (depends on 1)

The method of claim 1, wherein the ultra-shallow dopant region and ohmic contact region partially overlap in the substrate, and wherein the ultra-shallow dopant region extends further into the substrate than the ohmic contact region.

### Claim 7

A method for forming semiconductor device, the method comprising:
forming a dopant layer in direct contact with a silicon (Si) feature on a substrate;
forming a metal layer on the dopant layer, the metal layer containing a metal to form a metal silicide in the Si feature; and
performing a thermal treatment to form an ultra-shallow dopant region and a metal silicide region by diffusion of the dopant and the metal into the substrate, the thermal treatment comprising heating the substrate to an annealing temperature,
wherein, after forming the dopant layer and prior to the thermal treatment, the substrate is maintained below the annealing temperature.

### Claim 8 (depends on 7)

The method of claim 7, wherein forming the dopant layer comprises conformally depositing the dopant layer over the substrate by atomic layer deposition (ALD).

### Claim 9 (depends on 7)

The method of claim 7, wherein forming the dopant layer comprises depositing an oxide, nitride, oxynitride of the dopant.

### Claim 10 (depends on 7)

The method of claim 7, wherein forming the dopant layer comprises exposing the substrate to a vapor phase boron amide or an organoborane precursor.

### Claim 11 (depends on 7)

The method of claim 7, wherein forming the dopant layer comprises exposing the substrate to a vapor phase precursor containing arsenic or phosphorus.

### Claim 12 (depends on 7)

The method of claim 7, wherein the Si feature comprises a raised feature.

### Claim 13 (depends on 7)

The method of claim 7, wherein the dopant layer covers more than one face of the substrate.

### Claim 14 (depends on 7)

The method of claim 7, wherein the dopant is selected from a group consisting of boron (B), aluminum (Al), gallium (Ga), indium (In), and thallium (Tl), nitrogen (N), phosphorous (P), arsenic (As), antimony (Sb), and bismuth (Bi), and wherein the metal comprises titanium (Ti), nickel (Ni), platinum (Pt), or tungsten (W).

### Claim 15 (depends on 7)

The method of claim 7, wherein the annealing temperature is between 450° C. and 650° C.

### Claim 16

A method of processing a substrate, the method comprising:
loading the substrate in a processing chamber, the substrate comprising a vertical recess with a sidewall, the sidewall comprising a feature laterally protruding from a major surface of the sidewall, the feature having at least three faces exposed;
forming a dopant layer over the feature by atomic layer deposition (ALD) at a first temperature range, the dopant layer covering at least three faces of the feature conformally;
forming a metal layer over the feature at a second temperature range;
thermally treating the dopant layer by keeping the substrate above the first temperature range and the second temperature range to form an ultra-shallow dopant region in the feature; and
thermally treating the metal layer by keeping the substrate above the first temperature range and the second temperature range to form an ohmic contact region in the feature.

### Claim 17 (depends on 16)

The method of claim 16, wherein the metal layer is in direct contact with the dopant layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein thermally treating the dopant layer is performed prior to forming the metal layer, the metal layer being in direct contact with the feature.

### Claim 19 (depends on 16)

The method of claim 16, wherein thermally treating the dopant layer or thermally treating the metal layer is performed under an inert atmosphere or in an oxidizing atmosphere.

### Claim 20 (depends on 16)

The method of claim 16, wherein the feature comprises silicon (Si) and the ohmic contact region comprises metal silicide.