# US 2023/0057640 A1 · Ammoxidation catalyst for propylene, manufacturing method of the same catalyst, ammoxidation method using the same catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0057640 A1
- Document ID: US20230057640A1
- Status: Published application
- Kind: A1
- Application number: 17/778,744
- Filed: 2021-07-13
- Published: 2023-02-23
- Earliest claimed: 2020-07-14
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Kyungyeon Kang; Ji Yeon Kim; Jun Seon Choi
- Web page: https://patentgrep.com/patent/US20230057640A1

## CPC

- B01J 23/31: combined with bismuth
- B01J 23/8876: {Arsenic, antimony or bismuth}
- B01J 21/08: Silica
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/887: containing in addition other metals, oxides or hydroxides provided for in groups B01J23/02 - B01J23/36
- B01J 23/8872: {Alkali or alkaline earth metals}
- B01J 35/30: characterised by their physical properties
- B01J 35/38: Abrasion or attrition resistance
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 35/647: {2-50 nm}
- B01J 37/0045: {Drying a slurry, e.g. spray drying}
- B01J 37/02: Impregnation, coating or precipitation ({B01J37/0009 and B01J37/0018 take precedence } ; protection by coating B01J33/00)
- B01J 37/0201: {Impregnation}
- B01J 37/0203: {the impregnation liquid containing organic compounds}
- B01J 37/0205: {in several steps}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/0221: {of particles}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- C07C 253/26: containing carbon-to-carbon multiple bonds, e.g. unsaturated aldehydes
- B01J 35/31: Density
- B01J 35/397: {Egg shell like}
- B01J 35/50: characterised by their shape or configuration
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2523/00: Constitutive chemical elements of heterogeneous catalysts
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure relates to an ammoxidation catalyst for propylene, a manufacturing method of the same, and an ammoxidation method of propylene using the same. Specifically, in one embodiment of the present disclosure, there is provided a catalyst having a structure in which a metal oxide is supported on a silica support having a narrow particle size distribution, and excellent wear resistance.

## Claims

### Claim 1

An ammoxidation catalyst for propylene comprising:
a silica support containing a pore having a diameter of 2 to 15 nm and an apparent density of 0.25 to 1.0 g/cc; and
a metal oxide supported on the silica support and comprising molybdenum (Mo), bismuth (Bi) and a dissimilar metal.

### Claim 2 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the silica support contains a pore having a diameter of 2 to 13 nm.

### Claim 3 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the silica support has an apparent density of 0.3 to 1.0 g/cc.

### Claim 4 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the silica support has a D50 particle diameter of 50 to 150 gm.

### Claim 5 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the silica support has an ammonia (NH3) desorption amount of 1.3 mmol/g or less, and greater than 0.0, measured by an ammonia temperature programmed desorption method.

### Claim 6 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the metal oxide is represented by the following Chemical Formula 1:
Mo12BiaFebAcBdCeOx [Chemical Formula 1]
in the Chemical Formula 1,
A is at least one element of Ni, Mn, Co, Zn, Mg, Ca and Ba,
B is at least one element of Li, Na, K, Rb and Cs,
C is at least one element of Cr, W, B, Al, Ca and V,
a to e and x are each a fraction of an atom or atomic group, a is 0.1 to 5, b is 0.1 to 5, c is 0.01 to 10, d is 0.01 to 2, e is 0 to 10, and x is 24 to 48.

### Claim 7 (depends on 1, 6)

The ammoxidation catalyst of claim 6,
wherein the Chemical Formula 1 is the following Chemical Formula 1-1:
Mo12BiaFebCocKdOx [Chemical Formula 1-1]
in the Chemical Formula 1-1, each definition of a to d and x is the same as in claim 1.

### Claim 8 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein a weight ratio of the metal oxide to the silica support is 15:85 to 35:65.

### Claim 9 (depends on 46)

The ammoxidation catalyst of claim 46, wherein the catalyst comprises:
a silica support containing a second pore;
an inner coating layer continuously coating a wall surface of the second pore and comprising the metal oxide represented by the Chemical Formula 1; and
a first pore positioned inside the second pore and occupying an empty space excluding the inner coating layer.

### Claim 10 (depends on 1)

The ammoxidation catalyst of claim 1,
wherein the catalyst has a D10 particle size, a D50 particle size and a D90 particle size satisfying a relationship of Equation 1 below:
(D90−D10)/D50≤2.0 [Equation 1]

### Claim 11 (depends on 1)

The ammoxidation catalyst of claim 1, wherein the catalyst has an attrition loss of 10% or less according to an ASTM9797-00 method.

### Claim 12

A manufacturing method of an ammoxidation catalyst for propylene comprising the steps of:
preparing a first precursor aqueous solution containing a Mo precursor;
preparing a second precursor aqueous solution containing a Bi precursor and a dissimilar metal precursor;
supporting a mixture of the first and second precursor aqueous solutions on a silica support containing a pore having a diameter of 2 to 15 nm and an apparent density of 0.25 to 1.0 g/cc;
drying the silica support on which the mixture of the first and second precursor aqueous solutions is supported; and
calcining the dried material.

### Claim 13 (depends on 12)

The manufacturing method of claim 12,
wherein in the preparing of the second precursor aqueous solution,
the second precursor aqueous solution contains a Bi precursor, a Fe precursor, an A precursor, and a B precursor,
wherein the A precursor comprises at least one of Ni, Mn, Co, Zn, Mg, Ca, and Ba, and the B precursor comprises at least one of Li, Na, K, Rb and Cs.

### Claim 14 (depends on 12)

The manufacturing method of claim 12,
wherein in the preparing of the second precursor aqueous solution,
the second precursor aqueous solution contains a Bi precursor, a Fe precursor, a Co precursor, and a K precursor.

### Claim 15 (depends on 12)

The manufacturing method of claim 12,
wherein in the preparing of the second precursor aqueous solution,
the second precursor aqueous solution further contains a C precursor, wherein the C precursor comprises at least one of Cr, W, B, Al, Ca and V.

### Claim 16 (depends on 12)

The manufacturing method of claim 12,
wherein the mixture of the first and second precursor aqueous solutions has a molar ratio of the metals satisfying a stoichiometric molar ratio of the following Chemical Formula 1:
Mo12BiaFebAcBdCeOx [Chemical Formula 1]
in the Chemical Formula 1,
A is at least one element of Ni, Mn, Co, Zn, Mg, Ca and Ba,
B is at least one element of Li, Na, K, Rb and Cs,
C is at least one element of Cr, W, B, Al, Ca and V,
a to e and x are each a fraction of an atom or atomic group, a is 0.1 to 5, b is 0.1 to 5, c is 0.01 to 10, d is 0.01 to 2, e is 0 to 10, and x is 24 to 48.

### Claim 17 (depends on 12)

The manufacturing method of claim 12,
wherein the drying of the silica support on which the mixture of the first and second precursor aqueous solutions is supported comprises the steps of:
primarily vacuum-drying the silica support on which the mixture of the first and second precursor aqueous solutions is supported at 120 to 160 mbar; and
secondarily vacuum-drying the primarily vacuum-dried material at 30 to 50 mbar.

### Claim 18 (depends on 17)

The manufacturing method of claim 17,
further comprising a step of tertiarily drying the secondarily vacuum-dried material at atmospheric pressure.

### Claim 19 (depends on 12)

The manufacturing method of claim 12,
wherein the calcining of the dried material is carried out at 500 to 700° C.

### Claim 20 (depends on 1)

An ammoxidation method of propylene, comprising the step of reacting propylene and ammonia in the presence of the catalyst of claim 1 in a reactor.