# US 2023/0057346 A1 · Glass-based articles including a stress profile comprising two regions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0057346 A1
- Document ID: US20230057346A1
- Status: Published application
- Kind: A1
- Application number: 17/961,188
- Filed: 2022-10-06
- Published: 2023-02-23
- Earliest claimed: 2016-04-08
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Timothy Michael Gross; Xiaoju Guo; Pascale Oram; Kevin Barry Reiman; Rostislav Vatchev Roussev; Vitor Marino Schneider; Trevor Edward Wilantewicz
- Web page: https://patentgrep.com/patent/US20230057346A1

## CPC

- C03C 3/093: containing zinc or zirconium
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- H05K 5/0217: {Mechanical details of casings (covers, lids, hoods or members for covering apertures H05K5/03)}
- H05K 5/03: Covers
- H04B 1/3888: Arrangements for carrying or protecting transceivers
- H04M 1/0266: {for a display module assembly}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H04B: TRANSMISSION
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)

## Abstract

Glass-based article including a first surface and a second surface opposing the first surface defining a thickness (t), and a stress profile are disclosed having a thickness (t) of about 3 millimeters or less, and wherein all points of the stress profile between a thickness range from about 0·t up to 0.3·t and from greater than 0.7·t, comprise a tangent with a slope that is less than about −0.1 MPa/micrometers or greater than about 0.1 MPa/micrometers. Also disclosed are glass-based articles having a thickness (t) in a range of 0.1 mm and 2 mm; and wherein at least one point of the stress profile in a first thickness range from about 0·t up to 0.020·t and greater than 0.98·t comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer, and wherein all points of the stress profile in a second thickness range from about 0.035·t and less than 0.965·t comprise a tangent with a slope of from about −15 MPa/micrometer to about 15 MPa/micrometer.

## Claims

### Claim 1

A glass-based article comprising:
a first surface and a second surface opposing the first surface defining a thickness (t) in a range of 0.1 mm and 2 mm; and
a stress profile extending along the thickness (t) according to a mathematical formula that is a function of the thickness,
wherein all points of the mathematical formula for stress profile in a first thickness range from about 0·t up to 0.020·t and greater than 0.98t comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer,
wherein all points of the mathematical formula for stress profile in a second thickness range from 0.035·t to less than 0.965·t comprise a tangent with a slope of from about −15 MPa/micrometer to about 15 MPa/micrometer, wherein the mathematical formula for stress profile along the span of the second thickness range forms a power-law function having a power exponent, wherein the power exponent is from about 1.2 to about 3.2, and
wherein the stress profile comprises a surface compressive stress of from about 300 MPa to about 1100 MPa and a maximum central tension of 50 MPa or more.

### Claim 2 (depends on 1)

The glass-based article of claim 1, wherein the stress profile comprises a depth of compression ranging from about 0.1·t to 0.25·t.

### Claim 3 (depends on 1)

The glass-based article of claim 1, further comprising a maximum central tension that is less than or equal to 80 MPa.

### Claim 4 (depends on 1)

The glass-based article of claim 1, wherein all points of the stress profile in the second thickness range comprise a tangent having a slope of from about −2 MPa/micrometer to about 2 MPa/micrometer.

### Claim 5 (depends on 3)

The glass-based article of claim 3, wherein the first thickness range extends from about 0.02·t up to 0.025·t and greater than 0.975·t to 0.98·t, and all points of the mathematical formula for stress profile in the extended first thickness range comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer.

### Claim 6 (depends on 5)

The glass-based article of claim 5, wherein the first thickness range further extends from about 0.025·t up to 0.035·t and greater than 0.965·t up to about 0.975·t, and all points of the mathematical formula for stress profile in the further extension of the first thickness range comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer.

### Claim 7 (depends on 2)

The glass-based article of claim 2, wherein the thickness (t) is less than or equal to 1 mm, the surface compressive stress is greater than or equal to 500 MPa, and the depth of compression is greater than or equal to 0.14·t.

### Claim 8 (depends on 2)

The glass-based article of claim 2, further comprising a potassium depth of layer that extends over the first thickness range.

### Claim 9 (depends on 2)

The glass-based article of claim 2, wherein at least one of:
(i) the Knoop Scratch Lateral Cracking Threshold of the strengthened glass-based substrate is greater than 10N and is less than 16N;
(ii) the strengthened glass-based substrate has a survival rate of from 40% to 100%, when impacted on one of the first and second major surfaces with a force of 400N or more according to the surface Impact Threshold Test with 180 grit abrasive; and
(iii) the strengthened glass-based substrate can survive an edge-impact of from more than 300N to less than 500N, or an edge-impact of from more than 0.68 J to less than 1.58 J according to the edge Impact Threshold Test with 30 grit abrasive.

### Claim 10

A glass-based article comprising:
a center plane, wherein the center plane comprises from about 2 to about 20 mol-% Li2O;
a maximum central tension of 50 MPa or more, and
a stress profile extending along the thickness (t) according to a mathematical formula that is a function of the thickness,
wherein all points of the mathematical formula for stress profile in a first thickness range from about 0·t up to 0.020·t and greater than 0.98·t comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer,
wherein a mathematical formula for stress profile along the span of a second thickness range, extending from 0.035·t to less than 0.965·t, forms a power-law function having a power exponent, wherein the power exponent is from about 1.2 to about 3.4,
wherein the stress profile comprises a depth of compression ranging from about 0.05·t to 0.25·t.

### Claim 11 (depends on 10)

The glass-based article of claim 10, wherein the stress profile comprises a surface compressive stress of from about 300 MPa to about 1100 MPa.

### Claim 12 (depends on 10)

The glass-based article of claim 10, further comprising a maximum central tension that is less than or equal to 80 MPa.

### Claim 13 (depends on 11)

The glass-based article of claim 11, further comprising a first surface and a second surface opposing the first surface defining a thickness (t) in a range of 0.1 mm to 1 mm, wherein the surface compressive stress is greater than or equal to 500 MPa, and the depth of compression is greater than or equal to 0.14·t.

### Claim 14 (depends on 11)

The glass-based article of claim 11, wherein the glass-based article comprises a composition comprising about 0.5 mol % to about 10 mol % P2O5.

### Claim 15 (depends on 11)

The glass-based article of claim 11, wherein the center plane further comprises a composition comprising from about 0.5 mol % to about 20 mol % Na2O.

### Claim 16 (depends on 11)

The glass-based article of claim 11, further comprising a potassium depth of layer that extends over the first thickness range.

### Claim 17 (depends on 11)

The glass-based article of claim 11, wherein the surface compressive stress ranges from about 690 MPa to 1100 MPa.

### Claim 18 (depends on 10)

The glass-based article of claim 10, wherein all points of the stress profile in the second thickness range comprise a tangent having a slope of from about −2 MPa/micrometer to about 2 MPa/micrometer.

### Claim 19 (depends on 10)

The glass-based article of claim 10, wherein the first thickness range extends from about 0.02·t up to 0.025·t and greater than 0.975·t to 0.98·t, and all points of the mathematical formula for stress profile in the extended first thickness range comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer.

### Claim 20 (depends on 19)

The glass-based article of claim 19, wherein the first thickness range further extends from about 0.025·t up to 0.035·t and greater than 0.965·t up to about 0.975·t, and all points of the mathematical formula for stress profile in the further extension of the first thickness range comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer.