# US 2023/0057258 A1 · Selective patterning with molecular layer deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0057258 A1
- Document ID: US20230057258A1
- Status: Published application
- Kind: A1
- Application number: 17/407,504
- Filed: 2021-08-20
- Published: 2023-02-23
- Earliest claimed: 2021-08-20
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Bhaskar Jyoti Bhuyan; Zeqing Shen; Susmit Singha Roy; Abhijit Basu Mallick
- Web page: https://patentgrep.com/patent/US20230057258A1

## CPC

- H10P 14/61: using masks
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- C23C 16/04: Coating on selected surface areas, e.g. using masks
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/683: {carbon-based polymeric organic materials, e.g. polyimides, poly cyclobutene or PVC}
- H10P 50/287: {by chemical means}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/098: {by filling between adjacent conductive parts}
- B05D 1/36: Successively applying liquids or other fluent materials, e.g. without intermediate treatment
- B05D 1/60: {Deposition of organic layers from vapour phase (vapour phase deposition in general C23C14/00, C23C16/00)}
- B05D 1/62: {Plasma-deposition of organic layers (plasma deposition in general C23C14/00, C23C16/00)}
- B05D 2202/00: Metallic substrate
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10W 20/074: {of dielectric parts comprising thin functional dielectric layers, e.g. dielectric etch-stop, barrier, capping or liner layers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

Exemplary methods of semiconductor processing may include forming a layer of carbon-containing material on a substrate disposed within a processing region of a semiconductor processing chamber. The substrate may include an exposed region of a first dielectric material and an exposed region of a metal-containing material. The layer of carbon-containing material may be selectively formed over the exposed region of the metal-containing material. Forming the layer of carbon-containing material may include one or more cycles of providing a first molecular species that selectively couples with the metal-containing material. Forming the layer of carbon-containing material may include providing a second molecular species that selectively couples with the first molecular species. The methods may include selectively depositing a second dielectric material on the exposed region of the first dielectric material.

## Claims

### Claim 1

A semiconductor processing method comprising:
forming a layer of carbon-containing material on a substrate disposed within a processing region of a semiconductor processing chamber, wherein the substrate comprises an exposed region of a first dielectric material and an exposed region of a metal-containing material, wherein the layer of carbon-containing material is selectively formed over the exposed region of the metal-containing material, and wherein forming the layer of carbon-containing material comprises one or more cycles of:
providing a first molecular species that selectively couples with the metal-containing material, and
providing a second molecular species that selectively couples with the first molecular species; and
selectively depositing a second dielectric material on the exposed region of the first dielectric material.

### Claim 2 (depends on 1)

The semiconductor processing method of claim 1, wherein the layer of carbon-containing material is formed to a thickness of greater than or about 5 nm.

### Claim 3 (depends on 1)

The semiconductor processing method of claim 1, wherein forming the layer of carbon-containing material is performed at a substrate temperature of greater than or about 100° C.

### Claim 4 (depends on 1)

The semiconductor processing method of claim 1, further comprising:
performing an etch of the layer of carbon-containing material to expose the first dielectric material.

### Claim 5 (depends on 1)

The semiconductor processing method of claim 1, further comprising:
removing the layer of carbon-containing material by oxidizing the carbon-containing material or annealing the carbon-containing material.

### Claim 6 (depends on 5)

The semiconductor processing method of claim 5, wherein the metal-containing material comprises a first metal-containing material, the semiconductor processing method further comprising:
forming a second metal-containing material on the first metal-containing material.

### Claim 7 (depends on 1)

The semiconductor processing method of claim 1, wherein the first molecular species is characterized by a head group comprising an amine, diamine, diol, or dithiol.

### Claim 8 (depends on 7)

The semiconductor processing method of claim 7, wherein the second molecular species is characterized by a head group comprising oxygen.

### Claim 9 (depends on 1)

The semiconductor processing method of claim 1, wherein selectively depositing the second dielectric material comprises a plasma-enhanced deposition.

### Claim 10 (depends on 1)

The semiconductor processing method of claim 1, wherein forming the layer of carbon-containing material comprises at least 10 cycles.

### Claim 11

A semiconductor processing method comprising:
forming a layer of carbon-containing material on a substrate disposed within a processing region of a semiconductor processing chamber, wherein the substrate comprises an exposed region of a dielectric material and an exposed region of a metal-containing material, and wherein the layer of carbon-containing material is selectively formed over the exposed region of the metal-containing material to a thickness of at least twice a thickness formed on the dielectric material; and
selectively depositing a second dielectric material on the exposed region of the dielectric material.

### Claim 12 (depends on 11)

The semiconductor processing method of claim 11, wherein forming the layer of carbon-containing material comprises one or more cycles of:
providing a first molecular species that selectively couples with the metal-containing material, and
providing a second molecular species that selectively couples with the first molecular species.

### Claim 13 (depends on 11)

The semiconductor processing method of claim 11, further comprising:
removing the layer of carbon-containing material by oxidizing the carbon-containing material or annealing the carbon-containing material.

### Claim 14 (depends on 11)

The semiconductor processing method of claim 11, wherein the layer of carbon-containing material is formed to a thickness of greater than or about 5 nm.

### Claim 15 (depends on 11)

The semiconductor processing method of claim 11, wherein the metal-containing material comprises a first metal-containing material, the semiconductor processing method further comprising:
forming a second metal-containing material on the first metal-containing material.

### Claim 16 (depends on 11)

The semiconductor processing method of claim 11, wherein forming the layer of carbon-containing material is performed at a substrate temperature of greater than or about 100° C.

### Claim 17 (depends on 11)

The semiconductor processing method of claim 11, further comprising:
performing an etch of the layer of carbon-containing material to expose the dielectric material.

### Claim 18

A semiconductor processing method comprising:
forming a layer of carbon-containing material on a substrate disposed within a processing region of a semiconductor processing chamber at a substrate temperature of greater than or about 100° C., wherein the substrate comprises an exposed region of a first dielectric material and an exposed region of a metal-containing material, wherein the layer of carbon-containing material is selectively formed over the exposed region of the metal-containing material, and wherein forming the layer of carbon-containing material comprises one or more cycles of:
providing a first molecular species that selectively couples with the metal-containing material, wherein the first molecular species comprises an amine head group, and
providing a second molecular species that selectively couples with the first molecular species, wherein the second molecular species comprises oxygen; and
selectively depositing a second dielectric material on the exposed region of the first dielectric material.

### Claim 19 (depends on 18)

The semiconductor processing method of claim 18, further comprising:
performing an etch of the layer of carbon-containing material to expose the first dielectric material.

### Claim 20 (depends on 18)

The semiconductor processing method of claim 18, further comprising:
removing the layer of carbon-containing material by oxidizing the carbon-containing material or annealing the carbon-containing material.