# US 2023/0057062 A1 · Membrane-electrode assembly and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0057062 A1
- Document ID: US20230057062A1
- Status: Published application
- Kind: A1
- Application number: 17/758,572
- Filed: 2021-12-01
- Published: 2023-02-23
- Earliest claimed: 2020-12-16
- Assignees: Kolon Industries, Inc.
- Applicants: Kolon Industries, Inc.
- Inventors: Jung Ho KIM; Jun Young Kim; Kah-Young SONG; Nakwon KONG; Jusung LEE; Kyoungsik NAM; Chanmi PARK
- Web page: https://patentgrep.com/patent/US20230057062A1

## CPC

- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 4/8668: {Binders}
- H01M 4/881: {Electrolytic membranes}
- H01M 4/8828: {Coating with slurry or ink}
- H01M 4/8882: {Heat treatment, e.g. drying, baking}
- H01M 4/921: {Alloys or mixtures with metallic elements}
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are: a membrane-electrode assembly having enhanced adhesion and interfacial durability between a polymer electrolyte membrane and electrodes; and a method for manufacturing a membrane-electrode assembly, in which, in forming electrodes by directly coating a catalyst slurry on a polymer electrolyte membrane, adhesion and interfacial durability between the polymer electrolyte membrane and the electrodes can be enhanced without a separate additional step, thus improving both the durability and the productivity of the membrane-electrode assembly. The method comprises the steps of: dispersing a catalyst and an ion conductor in a dispersion medium to obtain a catalyst slurry; applying the catalyst slurry onto a polymer electrolyte membrane; and drying the catalyst slurry applied onto the polymer electrolyte membrane to form an electrode. The dispersion medium is a solvent capable of forming a plurality of grooves on a surface of the polymer electrolyte membrane, and, when the electrode is formed through the drying step, at least some of the grooves are filled with the catalyst, the ion conductor, or a mixture thereof.

## Claims

### Claim 1

A membrane-electrode assembly comprising:
a polymer electrolyte membrane; and
a first electrode on a first surface of the polymer electrolyte membrane, wherein
the first electrode comprises a first catalyst and a first ion conductor,
a plurality of grooves are randomly formed on the first surface,
each of the grooves has a depth of 5 μm or less and a width of 10 μm or less,
each of the grooves is filled with a portion of the first electrode, and
a content of the first ion conductor in the portion of the first electrode with which the grooves are filled is higher than a content of the first ion conductor in a remaining portion of the first electrode.

### Claim 2 (depends on 1)

The membrane-electrode assembly according to claim 1, wherein a difference between the content of the first ion conductor in the portion of the first electrode with which the grooves are filled and the content of the first ion conductor in the remaining portion of the first electrode is 2 to 12% of the content of the first ion conductor in the remaining portion of the first electrode.

### Claim 3

A method of manufacturing a membrane-electrode assembly, the method comprising:
dispersing a first catalyst and a first ion conductor in a first dispersion medium in order to obtain a first catalyst slurry;
coating the first catalyst slurry on a first surface of a polymer electrolyte membrane; and
drying the first catalyst slurry coated on the first surface in order to form a first electrode, wherein
the first dispersion medium comprises (i) a first ingredient capable of partially melting the polymer electrolyte membrane at the first surface thereof or causing deformation of the first surface to form a plurality of grooves on the first surface and (ii) a second ingredient different from the first ingredient,
the first ingredient is alcohol, acetic acid, propionic acid, dimethylacetamide, or a mixture of two or more thereof,
the alcohol is methanol, ethanol, propanol, ethoxyethanol, butanol, or a mixture of two or more thereof,
the second ingredient is water, N-methyl pyrrolidone (NMP), dimethyl sulfoxide (DMSO), tetrahydrofuran (THF), or a mixture of two or more thereof,
a content of the first dispersion medium in the first catalyst slurry is 83 to 98 wt. %,
a content of the first ingredient in the first dispersion medium is 55 to 80 wt. %, and
when the first electrode is formed through the drying step, at least some of the grooves are filled with the first catalyst, the first ion conductor, or a mixture thereof.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the first catalyst slurry is coated on the first surface to a coating thickness of 10 to 200 μm.

### Claim 5 (depends on 3)

The method according to claim 3, wherein the drying is performed at a temperature of 50 to 150° C. for 10 to 300 seconds.

### Claim 6 (depends on 3)

The method according to claim 3, wherein (i) a content of the first dispersion medium in the first catalyst slurry, (ii) a content of the first ingredient in the first dispersion medium, (iii) an coating thickness of the first catalyst slurry, (iv) a temperature of the drying step, and (v) a time of the drying step are set such that each of the grooves has a depth of 5 μm or less and a width of 10 μm or less.

### Claim 7 (depends on 3)

The method according to claim 3, wherein the dispersing is performed using at least one selected from a group consisting of an ultrasonic homogenizer, a ball mill, a roll mill, a resonant acoustic mixer, a high-pressure homogenizer, a planetary mixer, and a homogeneous mixer.

### Claim 8 (depends on 3)

The method according to claim 3, wherein the polymer electrolyte membrane comprises a fluorine-based ion conductor.

### Claim 9 (depends on 3)

The method according to claim 3, wherein the drying is performed by hot-air drying, infrared drying, or hot-plate drying.

### Claim 10 (depends on 3)

The method according to claim 3, further comprising:
coating a second catalyst slurry on a second surface of the polymer electrolyte membrane opposite the first surface after forming the first electrode; and
drying the second catalyst slurry coated on the second surface in order to form a second electrode.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the coating the first catalyst slurry on the first surface is performed while a protective film is attached to the second surface of the polymer electrolyte membrane.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising removing the protective film from the second surface before coating the second catalyst slurry on the second surface.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising attaching a first protective sheet to the first surface having the first electrode formed thereon before removing the protective film from the second surface.

### Claim 14 (depends on 13)

The method according to claim 13, further comprising attaching a second protective sheet to the second surface having the second electrode formed thereon.

### Claim 15 (depends on 10)

The method according to claim 10, further comprising:
attaching a first masking film having a first window to the first surface before coating the first catalyst slurry on the first surface;
removing the first masking film after forming the first electrode;
attaching a second masking film having a second window to the second surface before coating the second catalyst slurry on the second surface; and
removing the second masking film after forming the second electrode, wherein
the coating the first catalyst slurry on the first surface is performed by coating the first catalyst slurry on a portion of the first surface exposed through the first window, and
the coating the second catalyst slurry on the second surface is performed by coating the second catalyst slurry on a portion of the second surface exposed through the second window.