# US 2023/0056854 A1 · Dry electrode manufacture with lubricated active material mixture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0056854 A1
- Document ID: US20230056854A1
- Status: Published application
- Kind: A1
- Application number: 17/967,408
- Filed: 2022-10-17
- Published: 2023-02-23
- Earliest claimed: 2020-09-08
- Assignees: Licap Technologies, Inc.
- Applicants: Licap Technologies, Inc.
- Inventors: Linda Zhong; Erika Shaw; Bae Kyun Kim
- Web page: https://patentgrep.com/patent/US20230056854A1

## CPC

- H01M 4/043: {involving compressing or compaction}
- H01M 4/364: {as mixtures}
- H01G 11/24: characterised by structural features of the materials making up or comprised in the electrodes, e.g. form, surface area or porosity; characterised by the structural features of powders or particles used therefor
- H01G 11/26: characterised by their structure, e.g. multi-layered, porosity or surface features
- H01G 11/30: characterised by their material
- H01G 11/50: specially adapted for lithium-ion capacitors, e.g. for lithium-doping or for intercalation
- H01M 4/0435: {Rolling or calendering}
- H01M 4/139: Processes of manufacture
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/621: {Binders}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0567: characterised by the additives
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of manufacturing a free-standing electrode film includes preparing a mixture including an electrode active material, a binder, and an additive solution or conductive paste, the additive solution or conductive paste being in an amount less than 5% by weight of the mixture and including a polymer additive and a liquid carrier, as well as a conductive material in the case of a conductive paste. The mixture may have total solid contents greater than 95% by weight. Preparing the mixture may include mixing the additive solution or conductive paste with the electrode active material to lubricate the electrode active material and subsequently adding and mixing in the binder. The method may further include subjecting the mixture to a shear force and, after the mixture has been subjected to the shear force, pressing the mixture into a free-standing film.

## Claims

### Claim 1

A method of manufacturing a free-standing electrode film, the method comprising:
preparing a mixture including an electrode active material, a binder, and an additive solution, the additive solution being in an amount less than 5% by weight of the mixture and including a polymer additive and a liquid carrier, the mixture having total solid contents greater than 95% by weight, said preparing comprising mixing the additive solution with the electrode active material to lubricate the electrode active material and subsequently adding the binder;
subjecting the mixture to a shear force; and,
after the mixture has been subjected to the shear force, pressing the mixture into a free-standing film.

### Claim 2 (depends on 1)

The method of claim 1, further comprising mixing the polymer additive with the liquid carrier to produce the additive solution.

### Claim 3 (depends on 1)

The method of claim 1, wherein the polymer additive is 0.5-10% by weight of the additive solution.

### Claim 4 (depends on 3)

The method of claim 3, wherein the polymer additive is 1-5% by weight of the additive solution.

### Claim 5 (depends on 1)

The method of claim 1, wherein the mixture further includes a conductive material, said preparing comprising mixing the additive solution with the electrode active material to lubricate the electrode active material and subsequently adding the binder and the conductive material.

### Claim 6 (depends on 1)

The method of claim 1, wherein said pressing includes applying a roller press to the mixture.

### Claim 7 (depends on 1)

A method of manufacturing an electrode, the method comprising:
the method of claim 1; and
laminating the free-standing film on a current collector.

### Claim 8

A method of manufacturing a free-standing electrode film, the method comprising:
preparing a mixture including an electrode active material, a binder, and a conductive paste, the conductive paste being in an amount less than 5% by weight of the mixture and including a polymer additive, a liquid carrier, and a conductive material, the mixture having total solid contents greater than 95% by weight, said preparing comprising mixing the conductive paste with the electrode active material to lubricate the electrode active material and subsequently adding the binder;
subjecting the mixture to a shear force; and,
after the mixture has been subjected to the shear force, pressing the mixture into a free-standing film.

### Claim 9 (depends on 8)

The method of claim 8, further comprising mixing the polymer additive, the liquid carrier, and the conductive material to produce the conductive paste.

### Claim 10 (depends on 9)

The method of claim 9, wherein said mixing the polymer additive, the liquid carrier, and the conductive material to produce the conductive paste comprises mixing the polymer additive and the liquid carrier to produce an additive solution and, thereafter, mixing the conductive material into the additive solution.

### Claim 11 (depends on 10)

The method of claim 10, wherein the polymer additive is 0.5-10% by weight of the additive solution.

### Claim 12 (depends on 11)

The method of claim 11, wherein the polymer additive is 1-5% by weight of the additive solution.

### Claim 13 (depends on 8)

The method of claim 8, wherein the conductive material is 1-20% by weight of the conductive paste.

### Claim 14 (depends on 13)

The method of claim 13, wherein the conductive material is 2-15% by weight of the conductive paste.

### Claim 15 (depends on 14)

The method of claim 14, wherein the conductive material is 5-10% by weight of the conductive paste.

### Claim 16 (depends on 8)

The method of claim 8, wherein the mixture further includes a second conductive material other than the conductive material included in the conductive paste, said preparing comprising mixing the conductive paste with the electrode active material to lubricate the electrode active material and subsequently adding the binder and the second conductive material.

### Claim 17 (depends on 8)

The method of claim 8, wherein said pressing includes applying a roller press to the mixture.

### Claim 18 (depends on 8)

A method of manufacturing an electrode, the method comprising:
the method of claim 8; and
laminating the free-standing film on a current collector.

### Claim 19

A powdery mixture for use in manufacturing a free-standing electrode film, the powdery mixture comprising:
an electrode active material;
a binder; and
an additive solution in an amount less than 5% by weight of the powdery mixture, the additive solution including a polymer additive and a liquid carrier,
wherein the powdery mixture has total solid contents greater than 95% by weight.

### Claim 20 (depends on 19)

The powdery mixture of claim 19, further comprising a conductive material.

### Claim 21 (depends on 19)

The powdery mixture of claim 19, wherein the polymer additive is 0.5-10% by weight of the additive solution.