# US 2023/0056794 A1 · Polyethylene Powder and Molded Article Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0056794 A1
- Document ID: US20230056794A1
- Status: Published application
- Kind: A1
- Application number: 17/792,007
- Filed: 2021-01-25
- Published: 2023-02-23
- Earliest claimed: 2020-01-31
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Kazuya Shikata; Haruka Yokoyama
- Web page: https://patentgrep.com/patent/US20230056794A1

## CPC

- C08F 110/02: Ethene
- C08F 10/02: Ethene
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08J 3/12: Powdering or granulating
- H01M 50/417: Polyolefins
- Y02E 60/10: Energy storage using batteries
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A polyethylene powder satisfying (Requirements 1 to 3): (Requirement 1): viscosity-average molecular weight (Mv) is 200,000 or more and 3,000,000 or less (Requirement 2): complex viscosity |η*|m obtained by measurement under predetermined <Conditions for Measurement of Slurry Viscoelasticity>satisfies the following formula (1): 590.0×(Mv×10−4)1.18≥|η*|m≥13.3×(Mv×10−4)1.18 (1) (Requirement 3): a value of any peak when d(log|η*|)/dT is plotted against temperature is 1.0 or more and 3.0 or less.

## Claims

### Claim 1

A polyethylene powder satisfying the following (Requirements 1 to 3):
(Requirement 1): viscosity-average molecular weight (Mv) is 200,000 or more and 3,000,000 or less
(Requirement 2): complex viscosity |η*|m obtained by measurement under the following <Conditions for Measurement of Slurry Viscoelasticity>satisfies the following formula (1):
590.0×(Mv×104)1.18≥|η*|m≥13.3×(Mv×10−4)1.18 (1)
<Conditions for Measurement of Slurry Viscoelasticity>
measuring apparatus: MARS Ill manufactured by Thermo Fisher Scientific K.K.
stage: 20 mm ϕ
plate: 20 mm ϕ parallel plate
gap: 0.5 mm
slurry composition: 30 parts by mass of a polyethylene powder, 70 parts by mass of a liquid paraffin
(the polyethylene powder: a powder passing through a sieve having an opening of 425 μm in accordance with JIS Z 8801 standard is used for measurement)
measurement conditions: complex viscosity |η*| is measured by the following steps 1 to 2:
step 1 a slurry is kept at 100° C. for 2 min
step 2 after the step 1, temperature is increased from 100° C. to 140° C. at 1° C./min, and viscoelasticity during the temperature increase is measured at a frequency of 1 Hz and a strain of 10% under a nitrogen atmosphere
determination of |η*|m: a temperature at a point in time when a value of d(log|η*|)/dT associated with dissolution of the polyethylene powder first reaches 0.03 or less after passing a peak is regarded as a temperature at which the dissolution of the polyethylene powder is completed, and complex viscosity |η*| at the temperature is |η*|m
(T is measurement temperature)
(Requirement 3): a value of any peak when d(log |η*|)/dT is plotted against temperature is 1.0 or more and 3.0 or less.

### Claim 2 (depends on 1)

The polyethylene powder according to claim 1, wherein number of peaks when d(log|η*|)/dT is plotted against temperature is 2 or more.

### Claim 3 (depends on 1)

The polyethylene powder according to claim 1, wherein a value of the |η*|m is 1.0×103 or more and 3.0×104 or less.

### Claim 4 (depends on 1)

The polyethylene powder according to claim 1, wherein an amount of a fraction remaining on a sieve having an opening of 300 μm obtained by classification is 3.0% by mass or less.

### Claim 5 (depends on 1)

The polyethylene powder according to claim 1, wherein isothermal crystallization time at 125° C. obtained by the following <Conditions for Measurement of Isothermal Crystallization Time>is less than 4.0 min,
<Conditions for Measurement of Isothermal Crystallization Time>
step A1: the polyethylene powder is maintained at 50° C. for 1 min, and then temperature is increased to 180° C. at a temperature increase rate of 10° C./min
step A2: the polyethylene powder is maintained at 180° C. for 5 min, and then the temperature is decreased to 125° C. at a temperature decrease rate of 80° C./min
step A3: the polyethylene powder is maintained at 125° C., and a time when an exothermic peak top due to crystallization is obtained is taken as isothermal crystallization time, provided that a point in time when the temperature reaches 125° C. is regarded as a starting point (0 min).

### Claim 6 (depends on 1)

The polyethylene powder according to claim 1, wherein the polyethylene powder is an ethylene homopolymer.

### Claim 7 (depends on 1)

The polyethylene powder according to claim 1, wherein the viscosity-average molecular weight (Mv) is 230,000 or more and 2,800,000 or less.

### Claim 8 (depends on 1)

The polyethylene powder according to claim 1, wherein the viscosity-average molecular weight (Mv) is 250,000 or more and 2,200,000 or less.

### Claim 9 (depends on 1)

The polyethylene powder according to claim 1, wherein the complex viscosity |η*|m satisfies the following formula (2):
100.0×(Mv×104)1.18≥|η*|m>20.0×(Mv×104)1.18 (2).

### Claim 10 (depends on 1)

The polyethylene powder according to claim 1, wherein the value of any peak when d(log |η*|)/dT is plotted against temperature is 1.2 or more and 2.7 or less.

### Claim 11 (depends on 1)

The polyethylene powder according to claim 1, wherein the value of any peak when d(log|η*|)/dT is plotted against temperature is 1.4 or more and 2.5 or less.

### Claim 12 (depends on 1)

The polyethylene powder according to claim 1, wherein a value of a maximum peak when d(log|η*|)/dT is plotted against temperature is 1.0 or more and 3.0 or less.

### Claim 13 (depends on 1)

The polyethylene powder according to claim 1, wherein the value of the maximum peak when d(log |η*|)/dT is plotted against temperature is 1.2 or more and 2.7 or less.

### Claim 14 (depends on 1)

The polyethylene powder according to claim 1, wherein the value of the maximum peak when d(log |η*|)/dT is plotted against temperature is 1.4 or more and 2.5 or less.

### Claim 15 (depends on 1)

The polyethylene powder according to claim 1, wherein a value of the complex viscosity |η*|m is 2.0×103 or more and 1.5×104 or less.

### Claim 16 (depends on 1)

The polyethylene powder according to claim 1, wherein Mw/Mn and Mz/Mw obtained by GPC (gel permeation chromatography) measurement in which a differential refractometer and a light scattering detector are connected are 4.0 or more and 10.0 or less, and 2.0 or more and 7.0 or less, respectively.

### Claim 17 (depends on 1)

A molded article of the polyethylene powder according to claim 1.

### Claim 18 (depends on 17)

The molded article according to claim 17, wherein the molded article is a separator for a battery.

### Claim 19 (depends on 18)

The molded article according to claim 18, wherein the molded article is a separator for a lithium ion secondary battery.

### Claim 20 (depends on 2)

The polyethylene powder according to claim 2, wherein a value of the |η*|m is 1.0×103 or more and 3.0×104 or less.