# US 2023/0056504 A1 · Foamed article with excellent stiffness preservation and superior surface quality

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0056504 A1
- Document ID: US20230056504A1
- Status: Published application
- Kind: A1
- Application number: 17/785,723
- Filed: 2020-12-18
- Published: 2023-02-23
- Earliest claimed: 2019-12-24
- Assignees: Sabic Global Technologies B.V.
- Applicants: Sabic Global Technologies B.V.
- Inventors: Junhua Zhang; Dimphna Johanna Maria van Beek; Daniel Bande; Kar-Man Raymond Chu
- Web page: https://patentgrep.com/patent/US20230056504A1

## CPC

- C08L 23/12: Polypropene
- C08L 2203/14: used for foams
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2207/02: Heterophasic composition
- C08L 2207/04: Thermoplastic elastomer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to a foamed article comprising a polymer composition wherein the polymer composition comprises a first heterophasic propylene copolymer and an inorganic filler. The invention also relates to a process for the preparation of said foamed article and to the use of the foamed article for the preparation of automotive parts.

## Claims

### Claim 1

A foamed article comprising a polymer composition, wherein the polymer composition comprises a first heterophasic propylene copolymer (a) and an inorganic filler,
wherein the xylene soluble part of the first heterophasic propylene copolymer (a) is in the range from 18.1 to 27.6 wt% as determined by ISO16152:2005 based on the total amount of the first heterophasic propylene copolymer (a),
wherein the intrinsic viscosity of the xylene soluble part of the first heterophasic propylene copolymer (a) is in the range from 2.9 to 4.8 dl/g as measured according to ISO1628-1:2009 in decalin at 135° C.;
wherein the melt flow index (MFI) of the first heterophasic propylene copolymer (a) is in the range from 5.6 to 65.0 dg/min as determined according to ISO1133-1:2011 at 230° C. with 2.16 kg load,
wherein the amount of the first heterophasic propylene copolymer (a) is in the range from 18.2 to 79.7 wt% based on the total amount of the polymer composition,
wherein the ash content of the polymer composition as measured according to ISO 3451-1:2008 at 600° C. for 4 hours is in the range from 3.5 to 30.2 wt% based on the total amount of the polymer composition,
wherein the foamed article according to the present invention has an expansion ratio in the range from 1.05 to 2.14
, wherein the expansion ratio is the ratio between the density of the polymer composition before foaming and that of the foamed article and wherein the density is measured according to ISO 1183-1:2012.

### Claim 2 (depends on 1)

The foamed article according to claim 1, wherein the inorganic filler is a talc.

### Claim 3 (depends on 1)

The foamed article according to claim 1 wherein the inorganic filler has a mean particle size (D50) in the range from 0.12 to 10.2 µm as measured according to ISO 13317-3:2001, sedimentation analysis, Stockes' law.

### Claim 4 (depends on 1)

The foamed article according to claim 1 wherein the MFI of the first heterophasic propylene copolymer (a) is in the range from 8.6 to 45.1 dg/min as determined according to ISO1133-1:2011 at 230° C. with 2.16 kg load.

### Claim 5 (depends on 1)

The foamed article according to claim 1 wherein the xylene soluble part of the first heterophasic propylene copolymer (a) is in the range from 20.3 to 24.2 wt% as determined by ISO16152:2005 based on the total amount of the first heterophasic propylene copolymer (a).

### Claim 6 (depends on 1)

The foamed article according to claim 1 wherein the intrinsic viscosity of the xylene soluble part of the first heterophasic propylene copolymer (a) is in the range from 3.3 to 4.5 dl/g as measure according to ISO1628-1:2009 in decalin at 135° C.

### Claim 7 (depends on 1)

The foamed article according to claim 1 wherein the MFI of the polymer composition is in the range from 5 to 100 dg/min as measure according to ISO1133-1:2011 with a 2.16 kg load at 230° C.

### Claim 8 (depends on 1)

The foamed article according to claim 1 wherein the polymer composition further comprises a second heterophasic propylene copolymer (b), wherein the amount of the second heterophasic propylene copolymer (b) is in the range from 15 to 50 wt% based on the total amount of the polymer composition.

### Claim 9 (depends on 8)

The foamed article according to claim 8, wherein the MFI of the second heterophasic propylene copolymer (b) is in the range from 20 to 100 dg/min as determined according to ISO1133-1:2011 at 230° C. with 2.16 kg load.

### Claim 10 (depends on 8)

The foamed article according to claim 8, wherein the xylene soluble part of the second heterophasic propylene copolymer (b) is in the range from 12.1 to 20.6 wt% as determined by ISO16152:2005 based on the total amount of the second heterophasic propylene copolymer (b).

### Claim 11 (depends on 8)

The foamed article according to claim 8, wherein the intrinsic viscosity of the xylene soluble part of the second heterophasic propylene copolymer (a) is in the range from 3.6 to 6.2 dl/g as measured according to ISO1628-1:2009 in decalin at 135° C.

### Claim 12 (depends on 8)

The foamed article according to any claim 8, wherein the polymer composition further comprises a polyolefin based elastomer and additives, wherein the total amount of the first heterophasic propylene copolymer (a), the inorganic filler, the polyolefin based elastomer, the second heterophasic propylene copolymer (b) and the additives is preferably at least 95 wt% based on the total amount of the polymer composition.

### Claim 13 (depends on 1)

The foamed article according to claim 1, wherein the amount of the polymer composition is at least 93 wt% of the amount of the foamed article.

### Claim 14 (depends on 1)

A process for the preparation of a foamed article comprising sequential steps of:
Providing a mixture of a foaming agent and the polymer composition of claim 1;
melting the mixture to obtain a molten mixture,
injection molding the molten mixture into a mold,
applying a pressure to the molten mixture in the mold,
opening the mold at least partially to allow the molten mixture to form a soft foamed article and;
allowing the soft foamed article to solidify to form the foamed article and eject the foamed article from the mold.

### Claim 15 (depends on 1)

An article comprising the foamed article of claim 1 wherein the articles is an automotive part.