# US 2023/0056119 A1 · Glasses having high fracture toughness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0056119 A1
- Document ID: US20230056119A1
- Status: Published application
- Kind: A1
- Application number: 17/974,784
- Filed: 2022-10-27
- Published: 2023-02-23
- Earliest claimed: 2018-03-29
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Xiaoju Guo; Peter Joseph Lezzi; Jian Luo
- Web page: https://patentgrep.com/patent/US20230056119A1

## CPC

- C03C 3/095: containing rare earths
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- G02F 1/133308: {Support structures for LCD panels, e.g. frames or bezels}
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2201/10: containing boron (C03C2201/14 takes precedence)
- C03C 2201/28: containing phosphorus
- C03C 2201/32: containing aluminium (C03C2201/36 takes precedence)
- C03C 2201/3411: Yttrium
- C03C 2201/36: containing rare earth metals and aluminium, e.g. Er-Al co-doped
- C03C 2201/42: containing titanium
- C03C 2201/50: containing alkali metals
- G02F 1/133331: {Cover glasses}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A glass composition includes: 50 mol % to 69 mol % SiO2; 12.5 mol % to 25 mol % Al2O3; 0 mol % to 8 mol % B2O3; greater than 0 mol % to 4 mol % CaO; greater than 0 mol % to 17.5 mol % MgO; 0.5 mol % to 8 mol % Na2O; 0 mol % to 2.5 mol % La2O3; and greater than 8 mol % to 18 mol % Li2O, wherein (Li2O+Na2O+MgO)/Al2O3 is from 0.9 to less than 1.3; and Al2O3+MgO+Li2O+ZrO2+La2O3+Y2O3 is from greater than 23 mol % to less than 50 mol %. The glass composition may be characterized by at least one of the following: a K1C value measured by a chevron short bar method of at least 0.75; and a K1C value measured by a double torsion method of at least 0.8. The glass composition is chemically strengthenable. The glass composition may be used in a glass article or a consumer electronic product.

## Claims

### Claim 1

A glass article, comprising:
SiO2;
Al2O3; and
Li2O,
wherein the glass is characterized by at least one of the following:
a K1C value measured by a chevron short bar method of at least 0.75; and
a K1C value measured by a double torsion method of at least 0.8.

### Claim 2 (depends on 1)

The glass article of claim 1, further comprising MgO.

### Claim 3 (depends on 1)

The glass article of claim 1, further comprising CaO.

### Claim 4 (depends on 1)

The glass article of claim 1, further comprising TiO2.

### Claim 5 (depends on 1)

The glass article of claim 1, further comprising ZrO2.

### Claim 6 (depends on 1)

The glass article of claim 1, further comprising SrO.

### Claim 7 (depends on 1)

The glass article of claim 1, further comprising Y2O3.

### Claim 8 (depends on 1)

The glass article of claim 1, further comprising K2O.

### Claim 9 (depends on 1)

The glass article of claim 1, further comprising Na2O.

### Claim 10 (depends on 1)

The glass article of claim 1, wherein (Li2O+Na2O+MgO)/Al2O3 is from 0.9 to less than 1.3.

### Claim 11 (depends on 1)

The glass article of claim 1, wherein Al2O3+MgO+Li2O+ZrO2+La2O3+Y2O3 is from greater than 23 mol % to less than 50 mol %.

### Claim 12 (depends on 1)

The glass article of claim 1, further comprising B2O3.

### Claim 13 (depends on 1)

The glass article of claim 1, wherein the glass is fusion formable.

### Claim 14 (depends on 1)

The glass article of claim 1, wherein 5.631+0.148.Al2O3+0.142.B2O3−0.062.CaO−0.188.K2O+0.030.MgO−0.099.Na2O−0.043.Li2O−0.188.P2O5+0.020.ZnO−0.062.SrO+0.200.ZrO2≥6.5, wherein the value of each component is in mol %.

### Claim 15 (depends on 1)

A consumer electronic product, comprising:
a housing having a front surface, a back surface and side surfaces;
electrical components provided at least partially within the housing, the electrical components including at least a controller, a memory, and a display, the display being provided at or adjacent the front surface of the housing; and
a cover glass disposed over the display,
wherein at least one of a portion of the housing or a portion of the cover glass comprises the glass article of claim 1.