# US 2023/0056012 A1 · Diamond Structures For Tooling

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0056012 A1
- Document ID: US20230056012A1
- Status: Published application
- Kind: A1
- Application number: 17/975,027
- Filed: 2022-10-27
- Published: 2023-02-23
- Earliest claimed: 2021-07-20
- Assignees: Akhan Semiconductor, Inc.
- Applicants: AKHAN Semiconductor, Inc.
- Inventors: Adam Khan; Kiran Kumar Kovi
- Web page: https://patentgrep.com/patent/US20230056012A1

## CPC

- C23C 16/27: Diamond only
- C30B 25/18: characterised by the substrate
- C30B 29/04: Diamond
- H10P 72/0411: {for wet cleaning or washing}
- H10P 72/0418: {for etching}
- H10P 72/0471: {comprising at least one ion or electron beam chamber}
- H10P 72/0474: {comprising at least one lithography chamber}
- H10P 72/0476: {comprising at least one plating chamber}
- H10P 72/78: using vacuum or suction, e.g. Bernoulli chucks
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A substrate for a tool including at least one sidewall includes at least one diamond layer. The diamond layer has a thickness between 10 nanometers and 1000 nanometers and is formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.

## Claims

### Claim 1

A structure, comprising:
a substrate having a surface including at least one sidewall; and
a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the sidewall is defined on a protrusion extending away from the substrate.

### Claim 3 (depends on 1)

The structure of claim 1, wherein the sidewall is defined on a cavity extending into the substrate.

### Claim 4 (depends on 1)

The structure of claim 1, wherein the diamond layer is formed to continuously cover the surface of the substrate.

### Claim 5 (depends on 1)

The structure of claim 1, wherein the diamond layer is formed to partially cover the surface of the substrate.

### Claim 6 (depends on 1)

The structure of claim 1, wherein the diamond layer is formed to conformally cover the surface of the substrate.

### Claim 7 (depends on 1)

The structure of claim 1, wherein the diamond layer is formed to thin or thicken by less than 20% across the surface of the substrate.

### Claim 8 (depends on 1)

The structure of claim 1, wherein the diamond layer thickness is uniformly thick over selected regions of the surface of the substrate.

### Claim 9 (depends on 1)

The structure of claim 1, wherein the diamond layer can be at least one of multiple diamond and non-diamond layers formed to cover at least a portion of the surface of the substrate.

### Claim 10 (depends on 1)

The structure of claim 1, wherein the diamond layer on the surface and the sidewall is formed to have 50% of grains sized to be between 2 nanometers and 500 nanometers in size.

### Claim 11 (depends on 1)

The structure of claim 1, wherein the substrate is opaque at optical wavelengths.

### Claim 12 (depends on 1)

The structure of claim 1, wherein the diamond layer is deposited at less than 600 degrees Celsius.

### Claim 13

A method for depositing a layer, comprising:
providing a substrate having a surface including at least one sidewall; and
depositing a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.

### Claim 14 (depends on 13)

The method of claim 13, wherein the sidewall is defined on a protrusion extending away from the substrate.

### Claim 15 (depends on 13)

The method of claim 13, wherein the sidewall is defined on a cavity extending into the substrate.

### Claim 16 (depends on 13)

The method of claim 13, wherein the diamond layer is formed to continuously cover the surface of the substrate.

### Claim 17 (depends on 13)

The method of claim 13, wherein the diamond layer is formed to partially cover the surface of the substrate.

### Claim 18 (depends on 13)

The method of claim 13, wherein the diamond layer is formed to conformally cover the surface of the substrate.

### Claim 19 (depends on 13)

The method of claim 13, wherein the diamond layer is formed to thin or thicken by less than 20% across the surface of the substrate.

### Claim 20 (depends on 13)

The method of claim 13, wherein the diamond layer thickness is uniformly thick over selected regions of the surface of the substrate.

### Claim 21 (depends on 13)

The method of claim 13, wherein the diamond layer can be at least one of multiple diamond and non-diamond layers formed to cover at least a portion of the surface of the substrate.

### Claim 22 (depends on 13)

The method of claim 13, wherein the diamond layer on the surface and the sidewall is formed to have 50% of grains sized to be between 2 nanometers and 500 nanometers in size.

### Claim 23 (depends on 13)

The method of claim 13, wherein the substrate is opaque at optical wavelengths.

### Claim 24 (depends on 13)

The method of claim 13, wherein the diamond layer is deposited at less than 600 degrees Celsius.

### Claim 25

A wafer tooling structure, comprising:
wafer tooling including a substrate having a surface including at least one sidewall; and
a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.

### Claim 26 (depends on 25)

The structure of claim 25, wherein the sidewall is defined on a protrusion extending away from the substrate.

### Claim 27 (depends on 25)

The structure of claim 25, wherein the sidewall is defined on a cavity extending into the substrate.

### Claim 28 (depends on 25)

The structure of claim 25, wherein the diamond layer is formed to continuously cover the surface of the substrate.

### Claim 29 (depends on 25)

The structure of claim 25, wherein the diamond layer is formed to partially cover the surface of the substrate.

### Claim 30 (depends on 25)

The structure of claim 25, wherein the diamond layer is formed to conformally cover the surface of the substrate.

### Claim 31 (depends on 25)

The structure of claim 25, wherein the diamond layer is formed to thin or thicken by less than 20% across the surface of the substrate.

### Claim 32 (depends on 25)

The structure of claim 25, wherein the diamond layer thickness is uniformly thick over selected regions of the surface of the substrate.

### Claim 33 (depends on 25)

The structure of claim 25, wherein the diamond layer can be at least one of multiple diamond and non-diamond layers formed to cover at least a portion of the surface of the substrate.

### Claim 34 (depends on 25)

The structure of claim 25, wherein the diamond layer on the surface and the sidewall is formed to have 50% of grains sized to be between 2 nanometers and 500 nanometers in size.

### Claim 35 (depends on 25)

The structure of claim 25, wherein the substrate is opaque at optical wavelengths.

### Claim 36 (depends on 25)

The structure of claim 25, wherein the diamond layer is deposited at less than 600 degrees Celsius.

### Claim 37

A method for depositing a layer on wafer tooling, comprising:
providing a wafer tool including a substrate having a surface that further includes at least one sidewall; and
depositing a diamond layer having a thickness between 10 nanometers and 1000 nanometers and formed from diamond grains sized to be 50% or less of diamond layer thickness, with the diamond coating being deposited on the surface of the substrate over the at least one sidewall.