# US 2023/0055938 A1 · Process for synthesizing indium phosphide by liquid phosphorus injection method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055938 A1
- Document ID: US20230055938A1
- Status: Published application
- Kind: A1
- Application number: 17/797,073
- Filed: 2020-09-10
- Published: 2023-02-23
- Earliest claimed: 2020-06-02
- Assignees: The 13th Research Institute of China Electronics Technology Group Corporation
- Applicants: The 13Th Research Institute of China Electronics Technology Group Corporation
- Inventors: Lijie FU; Niefeng SUN; Shujie WANG; Xiaolan LI; Xin ZHANG; Xiaodan ZHANG; Yanlei SHI; Huimin SHAO; Yang WANG
- Web page: https://patentgrep.com/patent/US20230055938A1

## CPC

- C30B 15/02: adding crystallising materials or reactants forming it in situ to the melt
- C30B 15/002: {Continuous growth}
- C30B 27/02: by pulling from a melt
- C30B 29/40: AIIIBV compounds {wherein A is B, Al, Ga, In or Tl and B is N, P, As, Sb or Bi}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present invention relates to a process for synthesizing indium phosphide by liquid phosphorus injection method, which belongs to the field of semiconductor technology. The method comprises: converting gaseous phosphorus into liquid phosphorus through a condenser, injecting the liquid phosphorus into an indium melt while preventing phosphorus vaporization by randomly delivering a low temperature inert gas, and causing an instantaneous reaction between the liquid phosphorus and the liquid indium melt, so that an indium phosphide melt can be synthesized at a relatively low temperature, with advantages of high efficiency, high purity, precise proportioning, large capacity, aiding in the growth of a phosphorus-rich indium phosphide polycrystal and facilitating the growth of an indium phosphide monocrystal. The method includes the steps of indium cleaning, phosphorus charging, furnace loading, communication of condenser, synthesis, preparation of crystals, etc.

## Claims

### Claim 1

A process for synthesizing indium phosphide by liquid phosphorus injection method based on a synthesis system comprising a quartz phosphorus bubble, a condenser, a phosphorus source furnace, a lifting crucible, a low temperature inert gas random delivery system and a monocrystal furnace, characterized in that the method comprises the following steps:
1) indium cleaning: performing a surface cleaning treatment on indium, and drying the cleaned indium for later use;
2) phosphorus charging: charging red phosphorus into the quartz phosphorus bubble under the protection of a nitrogen atmosphere;
3) furnace loading: placing the quartz phosphorus bubble into the phosphorus source furnace for heating; then loading the phosphorus source furnace equipped with the quartz phosphorus bubble, the condenser, a seed crystal, the crucible filled with indium and a mated graphite support, an insulation jacket and a heater into a hearth of the monocrystal furnace, and placing a boron oxide protective agent;
4) communication of condenser: communicating an inlet of the condenser with the low temperature inert gas random delivery system and a mouth of the quartz phosphorus bubble, and checking whether there is air leakage;
5) synthesis:
A, closing a furnace door, vacuuming the furnace, randomly delivering a low temperature inert gas by the low temperature inert gas random delivery system into the furnace through the condenser, and maintaining the pressure in the furnace greater than the dissociation pressure of indium phosphide;
B, heating the indium in the crucible until the indium melts,
C, lifting the crucible to allow an outlet end of the condenser to inserted into the indium melt, and introducing a circulating cooling liquid into the condenser; and
D, vaporizing the phosphorus in the quartz phosphorus bubble by heating the phosphorus source furnace, condensing the vaporized phosphorus vapor into liquid white phosphorus through the condenser, and flowing the liquid white phosphorus into the indium melt to react and synthesize a proportioned indium phosphide; and
6) preparation of crystals: after the phosphorus in the quartz phosphorus bubble is completely vaporized and injected into the indium melt, lowering the crucible away from the outlet of the condenser, and then lowering the seed crystal to perform a high-pressure liquid encapsulation Czochralski (HP-LEC) crystal growth.

### Claim 2 (depends on 1)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 1, characterized in that: the indium cleaning in step 1) comprises removing oxides and residual impurities on the indium surface, wherein after cleaning, the indium reaches a purity of 6N, and has no dust impurities on the surface.

### Claim 3 (depends on 1)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 1, characterized in that, the purity of phosphorus in step 2) is 6N.

### Claim 4 (depends on 1)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 1, characterized in that, the degree of vacuum in the phosphorus source furnace in step 5) is 30-100 Pa.

### Claim 5 (depends on 4)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 4, characterized in that: the temperature of the low temperature inert gas in step 5) is less than 156° C.

### Claim 6 (depends on 5)

The method for synthesizing indium phosphide by liquid phosphorus injection according to claim 5, characterized in that, nitrogen or argon of 2 MPa is filled in the low temperature inert gas random delivery system.

### Claim 7 (depends on 1)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 1, characterized in that, the heating power of the phosphorus source furnace in step 5) is increased from 0 W to 3000 W within 2 hours, and phosphorus is gradually vaporized by 770 K.

### Claim 8 (depends on 1)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 1, characterized in that, the temperature in the crucible in step 5) is 1300-1400 K.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to any one of claims 1 to 8, characterized in that, a condensing medium in the condenser is a gallium indium alloy.

### Claim 10 (depends on 9)

The process for synthesizing indium phosphide by liquid phosphorus injection method according to claim 9, characterized in that, the low temperature inert gas random delivery system includes a differential pressure controller that controls the pressure.