# US 2023/0055929 A1 · Manufacturing method for semiconductor silicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055929 A1
- Document ID: US20230055929A1
- Status: Published application
- Kind: A1
- Application number: 17/797,874
- Filed: 2021-02-16
- Published: 2023-02-23
- Earliest claimed: 2020-02-19
- Assignees: Globalwafers Japan Co., Ltd.
- Applicants: Globalwafers Japan Co., Ltd.
- Inventors: Takeshi SENDA; Shingo NARIMATSU
- Web page: https://patentgrep.com/patent/US20230055929A1

## CPC

- H10P 14/2905: {Silicon, silicon germanium or germanium}
- C23C 16/24: Deposition of silicon only
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 25/16: Controlling or regulating (controlling or regulating in general G05)
- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 25/20: the substrate being of the same materials as the epitaxial layer
- C30B 29/06: Silicon
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2926: {Crystal orientations}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/36: {characterised by treatments done before the formation of the materials}
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A semiconductor silicon wafer manufacturing method is provided, where P aggregate defects and SF in an epitaxial layer can be suppressed. A silicon wafer substrate cut from a monocrystal ingot is doped with phosphorus and has a resistivity of 1.05 mΩ·cm or less and a concentration of solid-solution oxygen of 0.9×1018 atoms/cm3. The method includes steps of mirror-polishing substrates and heat treatment, where after the mirror-polishing step, the substrate is kept at a temperature from 700° C. to 850° for 30 to 120 minutes, then after the temperature rise, kept at a temperature from 100° C. to 1250° for 30 to 120 minutes, and after cooling, kept at a temperature from 700° C. to 450° C. for less than 10 minutes as an experience time. The heat treatment step is performed in a mixture gas of hydrogen and argon. The method includes an epitaxial layer deposition step to a thickness of 1.3 μm to 10.0 μm.

## Claims

### Claim 1

A method for manufacturing a semiconductor silicon wafer composed of a silicon wafer substrate and a silicon monocrystalline epitaxial layer thereon,
where the silicon wafer substrate is sliced from a monocrystalline silicon ingot doped with phosphorus which is grown by the Czochralski method at a pulling speed of 0.5 mm/min or more and 1.0 mm/min or less with the application of a magnetic field of 2000 G or more and 4000 G or less, and the silicon wafer substrate has a resistivity of 1.05 mΩ·cm or less, a concentration of solid-solution oxygen of 0.9×1018 atoms/cm3, and Si—P defects that are substantially P aggregation defects generated by forcibly cooling the grown crystal with a water-cooler which is installed within the pulling-up furnace,
the method comprising:
a step of mirror-polishing a front surface of the silicon wafer substrate;
a step of heat treatment of the silicon wafer substrate after mirror-polishing, in the heat treatment step, the substrate being kept at a constant temperature between 700° C. or higher and 850° C. or lower for 30 minutes or longer to 120 minutes or shorter, then after rising the temperature the silicon wafer substrate being kept at a temperature between 1100° C. or higher and 1250° C. or lower for 30 minutes or longer to 120 minutes or shorter, and then after, an experience time for the silicon wafer substrate to experience temperatures between 700° C. and 450° C. at a time of temperature cooling being less than 10 minutes, wherein in the series of the heat treatment, a furnace atmosphere is a mixed gas composed of hydrogen H2 and argon Ar; and
after the heat treatment step, a step of depositing a silicon monocrystalline epitaxial layer to a thickness equal to 1.3 μm or more and 10.0 μm or less.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, wherein a maximum side length of Si—P defects in the silicon wafer substrate is less than 100 nm and the density of the defects is less than 1×1012/cm3.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, wherein the furnace atmosphere in the heat treatment step is diluted argon gas with hydrogen (H2) having a partial pressure ranging from 50% to 80% at the time of raising the temperature from 700° C. or higher to less than 850° C. and diluted argon gas with hydrogen (H2) having a partial pressure ranging from 0.01% to 20% at a temperature of 850° C. or higher.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, further comprising a step of surface cleaning of the silicon wafer substrate before the step of deposition of an epitaxial layer thereon, in the surface cleaning step, silicon on the substrate surface to be etched to a depth of 50 nm or more to 150 nm or less with a mixture gas of hydrogen (H2), hydrogen chloride (HCl), and Si—H—Cl.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, wherein in the step of deposition of a silicon monocrystalline epitaxial layer, the epitaxial layer is deposited at a deposition temperature of 1100° C. or higher and 1150° C. or lower at a deposition rate of 3.5 μm/min or higher and 6.0 μm/min or lower.

### Claim 6 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, further comprising a step of oxide-film removal, from the mirror-polished wafer substrate before heat treatment in which the surface oxide film thereof is removed with an acid solution or an acid atmosphere.

### Claim 7 (depends on 1)

The method for manufacturing a semiconductor silicon wafer according to claim 1, wherein a slicing angle of the silicon wafer substrate before mirror-polishing against the primary plane orientation ranges from 0.1 degrees or larger to 0.4 degrees or smaller.