# US 2023/0055755 A1 · Silicon carbide semiconductor device and method of manufacturing silicon carbide semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055755 A1
- Document ID: US20230055755A1
- Status: Published application
- Kind: A1
- Application number: 17/855,063
- Filed: 2022-06-30
- Published: 2023-02-23
- Earliest claimed: 2021-08-17
- Assignees: Fuji Electric Co., Ltd.
- Applicants: Fuji Electric Co., Ltd.
- Inventors: Yasuyuki KAWADA
- Web page: https://patentgrep.com/patent/US20230055755A1

## CPC

- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 12/038: {having a recessed gate, e.g. trench-gate IGBTs}
- H10D 12/481: {having gate structures on slanted surfaces, on vertical surfaces, or in grooves, e.g. trench gate IGBTs}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 62/107: {Buried supplementary regions, e.g. buried guard rings (multi-RESURF H10D62/111)}
- H10D 62/8325: {Silicon carbide}
- H10D 64/513: {within recesses in the substrate, e.g. trench gates, groove gates or buried gates}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

After trench etching but before formation of a gate insulating film, a 15-minute to 60-minute heat treatment under a mixed gas atmosphere containing nitric oxide gas and nitrogen gas at a temperature from 1200 degrees C. to 1350 degrees C. and a 30-minute to 75-minute heat treatment under a nitrogen gas atmosphere held at the temperature of the 15-minute to 60-minute heat treatment are successively performed, oxidizing etching damage of inner walls of trenches. The total treatment time of the heat treatments includes a total time of at least 90 minutes when the temperature is a predetermined maximum temperature. The oxide layer of the trench inner walls is removed, exposing a clean face. Emission intensity of band edge emission for SiC obtained by CL analysis of surface areas of the inner walls of the trenches is at least equal to the emission intensity of the band edge emission for SiC obtained by the CL analysis of a surface free of dry etching.

## Claims

### Claim 1

A silicon carbide semiconductor device having an insulated gate with a three-layered structure including a gate, an oxide film, and a semiconductor, the silicon carbide semiconductor device, comprising:
a semiconductor substrate containing silicon carbide and constituting the semiconductor, the semiconductor substrate having a main surface; and
a trench gate structure including the gate, the oxide film, and the semiconductor, the trench gate structure further including
a trench having a predetermined depth below the main surface of the semiconductor substrate, in a depth direction;
a gate insulating film provided along an inner wall of the trench, the gate insulating film being in contact with the semiconductor substrate at the inner wall of the trench and constituting the oxide film; and
a gate electrode provided on the gate insulating film in the trench, the gate electrode constituting the gate, wherein
the trench gate structure has a channel formed along a sidewall of the inner wall of the trench in the semiconductor substrate when the device is on, and
a first emission intensity of a first band edge emission of the silicon carbide in a first surface area of the inner wall of the trench is at least equal to a second emission intensity of a second band edge emission of the silicon carbide in a second surface area of a surface of the semiconductor substrate, the first emission intensity and the second emission intensity being obtained by a cathodoluminescence technique, the second surface area being free of dry etching.

### Claim 2 (depends on 1)

The silicon carbide semiconductor device according to claim 1, wherein
in a distribution of the first emission intensity of the silicon carbide in the first surface area of the inner wall of the trench, a ratio of a long-wavelength emission intensity of a long-wavelength emission to the first emission intensity of the first band edge emission is less than 35 when an acceleration voltage for electrons irradiated on the inner wall of the trench during analysis by the cathodoluminescence technique is 2 kV, or at most 9 when the acceleration voltage for the electrons irradiated on the inner wall of the trench during the analysis by the cathodoluminescence method is 5 kV, or satisfies both, the distribution of the first emission intensity and the long-wavelength emission intensity being obtained by the cathodoluminescence technique, the long-wavelength emission occurring in a wavelength band that is located at a wavelength side that is longer than a wavelength of a peak of the first band edge emission, the wavelength band of the long-wavelength emission being broader than a wavelength band of the first band edge emission.

### Claim 3 (depends on 1)

The silicon carbide semiconductor device according to claim 1, wherein
a third emission intensity of a third band edge emission of the silicon carbide in a surface of the inner wall of the trench is at least equal to a fourth emission intensity of a fourth band edge emission of the silicon carbide in a surface of the semiconductor substrate that is free of dry etching, the third emission intensity and the fourth emission intensity being obtained by the cathodoluminescence technique.

### Claim 4 (depends on 1)

The silicon carbide semiconductor device according to claim 1, wherein
the first and second band edge emissions of the silicon carbide are each free exciton emission observed at a wavelength around 390 nm.

### Claim 5

A method of manufacturing a silicon carbide semiconductor device having an insulated gate with a three-layered structure including a gate, an oxide film, and a semiconductor, the method, comprising:
performing dry etching and thereby forming a trench in a semiconductor substrate that has a main surface and contains silicon carbide constituting the semiconductor, the trench extending a predetermined depth from the main surface of the semiconductor substrate, in a depth direction;
performing a treatment that includes a first heat treatment performed under a gas atmosphere containing a nitric oxide gas and a second heat treatment performed successively after the first heat treatment, under a nitrogen gas atmosphere, the treatment being performed after forming the trench;
exposing the inner wall of the trench by performing the treatment and thereby removing an oxide layer formed on an inner wall of the trench;
forming a gate insulating film on and along the inner wall of the trench, after removing the oxide layer and exposing the inner wall of the trench, the gate insulating film constituting the oxide film;
baking the gate insulating film by a third heat treatment; and
forming a gate electrode on the gate insulating film in the trench after baking the gate insulating film and thereby forming a trench gate structure in which a channel is formed along a sidewall of the trench in the semiconductor substrate when the device is on, the gate electrode constituting the gat, wherein
performing the treatment includes:
performing the first heat treatment at a temperature in a range of 1200 degrees C. to 1350 degrees C., and
maintaining the temperature of the first heat treatment, switching to the nitrogen gas atmosphere, and performing the second heat treatment, and
a total treatment time of the first heat treatment and the second heat treatment includes a total time of at least 90 minutes when the temperature is a predetermined maximum temperature.

### Claim 6 (depends on 5)

The method according to claim 5, wherein
performing the treatment includes:
performing the first heat treatment for 15 minutes to 60 minutes, and
performing the second heat treatment for 30 minutes to 75 minutes.

### Claim 7 (depends on 5)

The method according to claim 5, wherein
the first heat treatment is performed under the gas atmosphere containing the nitric oxide gas at a percentage of 5% to 20% mixed with a nitrogen gas.

### Claim 8 (depends on 5)

The method according to claim 5, wherein
a damaged layer is formed on the inner wall of the trench by the dry etching, the method further comprising oxidizing the damaged layer to form the oxide layer, by the first heat treatment.

### Claim 9 (depends on 5)

The method according to claim 5, wherein
performing the treatment includes terminating a defect of the inner wall of the trench by nitrogen contained in the nitric oxide gas in the first heat treatment.

### Claim 10 (depends on 5)

The method according to claim 5, further comprising
repairing a disturbance in a crystal structure of the silicon carbide of the semiconductor substrate by the second heat treatment.