# US 2023/0055650 A1 · High-strength seamless steel pipe and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055650 A1
- Document ID: US20230055650A1
- Status: Published application
- Kind: A1
- Application number: 17/787,397
- Filed: 2020-11-24
- Published: 2023-02-23
- Earliest claimed: 2019-12-26
- Assignees: Jfe Steel Corporation
- Applicants: JFE Steel Corporation
- Inventors: Mitsuhiro Okatsu; Masao Yuga; Toshiharu Hirama
- Web page: https://patentgrep.com/patent/US20230055650A1

## CPC

- C21D 9/085: {Cooling or quenching}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/19: by interrupted quenching
- C21D 1/26: Methods of annealing
- C21D 1/78: Combined heat-treatments not provided for above
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/10: during manufacturing of tubular bodies
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/54: with boron
- F16L 9/02: of metal (F16L9/16 - F16L9/22 take precedence)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

Provided herein is a high-strength seamless steel pipe, and a method for manufacturing same. A high-strength seamless steel pipe of the present invention has a yield strength of 758 MPa or more, and a KILIMIT value of 23.0 MPa√m or more as an evaluation index of sulfide stress corrosion cracking resistance.

## Claims

### Claim 1

A high-strength seamless steel pipe having a yield strength of 758 MPa or more, and a KILIMIT value of 23.0 MPa√m or more as an evaluation index of sulfide stress corrosion cracking resistance,
where KILIMIT is a value determined from the intersection between (i) a linear regression line created by a stress intensity factor KISSC obtained in a DCB (Double Cantilever Beam) test conducted multiple times under different test conditions, and an applied stress intensity factor KIapplied at the tip of a notch in a test specimen before start of the DCB test, and (ii) a straight line on which KISSC and KIapplied are one-to-one.

### Claim 2 (depends on 1)

The high-strength seamless steel pipe according to claim 1, which has a steel microstructure with a prior austenite grain size of 10.5 or more in terms of a grain size number in compliance with ASTM E112.

### Claim 3 (depends on 1)

The high-strength seamless steel pipe according to claim 1, which has a composition that comprises, in mass %, C: 0.23 to 0.27%, Si: 0.35% or less, Mn: 0.45 to 0.70%, P: 0.010% or less, S: 0.0010% or less, Cr: 0.80 to 1.20%, Mo: 0.50 to 0.90%, Al: 0.080% or less, Cu: 0.09% or less, Nb: 0.050% or less, V: 0.050% or less, B: 0.0015 to 0.0030%, Ti: 0.005% or less, O: 0.0020% or less, and N: 0.0050% or less, and in which the balance is Fe and incidental impurities.

### Claim 4 (depends on 2)

The high-strength seamless steel pipe according to claim 2, which has a composition that comprises, in mass %, C: 0.23 to 0.27%, Si: 0.35% or less, Mn: 0.45 to 0.70%, P: 0.010% or less, S: 0.0010% or less, Cr: 0.80 to 1.20%, Mo: 0.50 to 0.90%, Al: 0.080% or less, Cu: 0.09% or less, Nb: 0.050% or less, V: 0.050% or less, B: 0.0015 to 0.0030%, Ti: 0.005% or less, O: 0.0020% or less, and N: 0.0050% or less, and in which the balance is Fe and incidental impurities.

### Claim 5 (depends on 3)

The high-strength seamless steel pipe according to claim 3, wherein the composition further comprises, in mass %, Ca: 0.0020% or less.

### Claim 6 (depends on 4)

The high-strength seamless steel pipe according to claim 4, wherein the composition further comprises, in mass %, Ca: 0.0020% or less.

### Claim 7 (depends on 1)

A method for manufacturing the high-strength seamless steel pipe of claim 1,
the method comprising:
a step of heating a steel pipe material to a heating temperature in a temperature region of 1,200 to 1,300° C.;
a first hot rolling step of hot rolling the heated steel pipe material by piercing and elongating the steel pipe material with a rolling end temperature of 800° C. or more;
an intermediate cooling step of cooling a raw steel pipe after the first hot rolling step, the raw steel pipe being cooled from a cooling start temperature of 700° C. or more under the conditions that the average cooling rate is 40° C./s or more, and the recuperation temperature Tr of the raw steel pipe at a pipe surface is (Ms+150° C.) or less, where Ms is a martensitic transformation start temperature;
an intermediate heating step of heating the raw steel pipe after the intermediate cooling step, the raw steel pipe being heated to a surface temperature of 800 to 1,000° C. after a lapse of a waiting time tW of 300 seconds or less by being charged into a reheating furnace;
a second hot rolling step of subjecting the raw steel pipe after the intermediate heating step to sizing hot rolling from a temperature equal to or greater than (Ar3+100° C.), where Ar3 is a ferrite transformation start temperature, and ending the hot rolling at a temperature of (Ar3+50° C.) or more;
a direct quenching step of directly quenching the raw steel pipe continuously from the second hot rolling step, the raw steel pipe being quenched from a temperature equal to or greater than (Ar3+10° C.) under the conditions that the average cooling rate is 40° C./s or more, and the cooling stop temperature is 200° C. or less; and
a heat treatment step of subjecting the raw steel pipe after the direct quenching step to at least one run of a heat treatment that quenches the raw steel pipe after reheating to a temperature of 850 to 930° C., and continuously tempers the raw steel pipe by heating to 650 to 730° C.,
the recuperation temperature Tr and the waiting time tW in the intermediate heating step satisfying the following formula (1):
(Tr−Ms)≤10+0.0024×(tW)2 (1).

### Claim 8 (depends on 7)

The method for manufacturing the high-strength seamless steel pipe according to claim 7, wherein the high-strength seamless steel pipe has a steel microstructure with a prior austenite grain size of 10.5 or more in terms of a grain size number in compliance with ASTM E112.

### Claim 9 (depends on 7)

The method for manufacturing the high-strength seamless steel pipe according to claim 7, wherein the steel pipe material has a composition that comprises, in mass %, C: 0.23 to 0.27%, Si: 0.35% or less, Mn: 0.45 to 0.70%, P: 0.010% or less, S: 0.0010% or less, Cr: 0.80 to 1.20%, Mo: 0.50 to 0.90%, Al: 0.080% or less, Cu: 0.09% or less, Nb: 0.050% or less, V: 0.050% or less, B: 0.0015 to 0.0030%, Ti: 0.005% or less, O: 0.0020% or less, and N: 0.0050% or less, and in which the balance is Fe and incidental impurities.

### Claim 10 (depends on 8)

The method for manufacturing the high-strength seamless steel pipe according to claim 8, wherein the steel pipe material has a composition that comprises, in mass %, C: 0.23 to 0.27%, Si: 0.35% or less, Mn: 0.45 to 0.70%, P: 0.010% or less, S: 0.0010% or less, Cr: 0.80 to 1.20%, Mo: 0.50 to 0.90%, Al: 0.080% or less, Cu: 0.09% or less, Nb: 0.050% or less, V: 0.050% or less, B: 0.0015 to 0.0030%, Ti: 0.005% or less, O: 0.0020% or less, and N: 0.0050% or less, and in which the balance is Fe and incidental impurities.

### Claim 11 (depends on 9)

The method for manufacturing the high-strength seamless steel pipe according to claim 9, wherein the composition further comprises, in mass %, Ca: 0.0020% or less.

### Claim 12 (depends on 10)

The method for manufacturing the high-strength seamless steel pipe according to claim 10, wherein the composition further comprises, in mass %, Ca: 0.0020% or less.