# US 2023/0055556 A1 · Method for degrading polyethylene terephthalate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055556 A1
- Document ID: US20230055556A1
- Status: Published application
- Kind: A1
- Application number: 17/563,510
- Filed: 2021-12-28
- Published: 2023-02-23
- Earliest claimed: 2021-08-05
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Chien-Wei Hsu; Ssu-Ting Lin; Ying-Chieh Lee
- Web page: https://patentgrep.com/patent/US20230055556A1

## CPC

- C08J 11/16: by treatment with inorganic material (C08J11/14 takes precedence)
- B01J 6/001: {Calcining}
- B01J 21/08: Silica
- B01J 21/18: Carbon
- B01J 23/02: of the alkali- or alkaline earth metals or beryllium
- B01J 23/06: of zinc, cadmium or mercury
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/618: {more than 1000 m2/g}
- B01J 37/0201: {Impregnation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/084: {Decomposition of carbon-containing compounds into carbon}
- B01J 37/088: {Decomposition of a metal salt}
- C08J 11/24: containing hydroxyl groups
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for degrading polyethylene terephthalate is provided. The method includes: providing polyethylene terephthalate material, providing a catalyst composite including a porous carrier having a pore size of 45 Å to 250 Å and a metal compound including at least one selected from a group consisting of zinc oxide, zinc hydroxide, zinc carbonate, magnesium oxide, calcium oxide, zirconium oxide, and titanium dioxide, in which the metal oxide is loaded on the porous carrier; and performing a degradation reaction, in which the polyethylene terephthalate material is reacted with the catalyst composite in the presence of an alcohol solvent.

## Claims

### Claim 1

A method for degrading polyethylene terephthalate, comprising:
providing polyethylene terephthalate material;
providing a catalyst composite, comprising:
a porous carrier having a pore size of 45 Å to 250 Å; and
a metal compound loaded on the porous carrier, comprising at least one selected from a group consisting of zinc oxide, zinc hydroxide, zinc carbonate, magnesium oxide, calcium oxide, zirconium oxide, and titanium dioxide; and
performing a degradation reaction on the polyethylene terephthalate material and the catalyst composite in the presence of an alcohol solvent.

### Claim 2 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein the porous carrier comprises an activated carbon, silicon dioxide, or a combination thereof.

### Claim 3

The method for degrading polyethylene terephthalate as claimed in claim wherein a content of the metal compound is 8 wt % to 35 wt % based on the total weight of the catalyst composite.

### Claim 4 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein a surface area of the porous carrier is 250 m2/g to 1500 m2/g,

### Claim 5 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein the polyethylene terephthalate material is a mixture comprising polyethylene terephthalate, the mixture comprises polyethylene terephthalate and a first polymer, wherein a content of the polyethylene terephthalate is 90 wt % to less than 100 wt %.

### Claim 6 (depends on 5)

The method for degrading polyethylene terephthalate as claimed in claim 5, wherein the first polymer comprises polylactic acid), polystyrene, polyolefin, or a combination thereof.

### Claim 7 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein the alcohol solvent comprises a mono-ol of C1-10, a diol of C1-10, or a combination thereof.

### Claim 8 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein a weight ratio of the catalyst composite to the polyethylene terephthalate material is 1:40 to 1:1.0.

### Claim 9 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein a source of the polyethylene terephthalate material is at least one selected front a group consisting of colorless transparent or multicolored polyethylene terephthalate bottles, polyethylene terephthalate flat sheets, polyethylene terephthalate packaging materials, and fabrics containing polyethylene terephthalate.

### Claim 10 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, wherein a reaction temperature of the degradation reaction is 160° C. to 230° C., and a time of the degradation reaction is 2 to 6 hours.

### Claim 11 (depends on 1)

The method for degrading polyethylene terephthalate as claimed in claim 1, further comprising recovering the catalyst composite after the degradation reaction is performed.