# US 2023/0055341 A1 · Multipod Nanostructures and Methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055341 A1
- Document ID: US20230055341A1
- Status: Published application
- Kind: A1
- Application number: 17/937,634
- Filed: 2022-10-03
- Published: 2023-02-23
- Earliest claimed: 2018-03-21
- Assignees: The Florida State University Research Foundation, Inc.
- Applicants: The Florida State University Research Foundation, Inc.
- Inventors: Parth Nalin Vakil; Geoffrey F. Strouse
- Web page: https://patentgrep.com/patent/US20230055341A1

## CPC

- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- B22F 1/0553: {Complex form nanoparticles, e.g. prism, pyramid, octahedron}
- B22F 1/054: Nanosized particles
- B22F 1/0545: Dispersions or suspensions of nanosized particles
- B22F 1/056: {Submicron particles having a size above 100 nm up to 300 nm}
- B22F 3/16: in successive or repeated steps
- B22F 2202/11: Use of irradiation
- B22F 2301/15: Nickel or cobalt
- B22F 2301/25: Noble metals, i.e. Ag Au, Ir, Os, Pd, Pt, Rh, Ru
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C22C 19/00: Alloys based on nickel or cobalt
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods of forming metal multipod nanostructures. The methods may include providing a mixture that includes a metal acetylacetonate, a reducing agent, and a carboxylic acid. The mixture may be contacted with microwaves to form the metal multipod nanostructures. The methods may offer control over the structure and/or morphology of the metal multipod nanostructures.

## Claims

### Claim 1

A method of forming metal multipod nanostructures, the method comprising:
providing a mixture disposed in a microwave reaction vessel, the mixture comprising—
a metal acetylacetonate,
a reducing agent comprising a C1-C30 hydrocarbyl-amine, and
a carboxylic acid of formula (A)—
wherein R is a monovalent C1-C30 hydrocarbyl; and
contacting the mixture with microwaves to form the metal multipod nanostructures;
wherein the contacting of the mixture with microwaves comprises (i) contacting the mixture with a first plurality of microwaves effective to heat the mixture to a first temperature, (ii) reducing the first temperature of the mixture to a second temperature, (iii) contacting the mixture with a second plurality of microwaves for a time effective to heat the mixture to the first temperature, and repeating steps (ii) and (iii) from 1 to 8 times.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first temperature is about 260° C. to about 300° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second temperature is about 220° C. to about 250° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the time effective to heat the mixture to the first temperature with the second plurality of microwaves is about 1 minute to about 20 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second plurality of microwaves comprises microwaves of different wattages.

### Claim 6 (depends on 5)

The method of claim 5, wherein the first temperature is about 260° C. to about 300° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second plurality of microwaves consists of microwaves of the same wattage.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first temperature is about 260° C. to about 300° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the metal acetylacetonate and the reducing agent are present in the mixture at a mole ratio of about 0.3:25 to about 3:25.

### Claim 10 (depends on 1)

The method of claim 1, wherein the reducing agent and the carboxylic acid of formula (A) are present in the mixture at a mole ratio of about 25:2 to about 25:8.

### Claim 11 (depends on 1)

The method of claim 1, wherein the metal acetylacetonate comprises a Ni acetylacetonate.

### Claim 12 (depends on 1)

The method of claim 1, wherein the metal acetylacetonate is selected from the group consisting of a Pt acetylacetonate, a Pd acetylacetonate, a Cu acetylacetonate, a Co acetylacetonate, a Au acetylacetonate, an Fe acetylacetonate, and a Rh acetylacetonate.

### Claim 13 (depends on 1)

The method of claim 1, wherein the C1-C30 hydrocarbyl-amine is an unsaturated C1-C30 hydrocarbyl-amine.

### Claim 14 (depends on 1)

The method of claim 1, wherein the C1-C30 hydrocarbyl-amine is oleylamine.

### Claim 15 (depends on 1)

The method of claim 1, wherein the carboxylic acid of formula (A) is oleic acid.