# US 2023/0055218 A1 · Method for forming a porous activited asphaltene material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0055218 A1
- Document ID: US20230055218A1
- Status: Published application
- Kind: A1
- Application number: 17/981,544
- Filed: 2022-11-07
- Published: 2023-02-23
- Earliest claimed: 2018-04-04
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: MOHAMMAD NAHID SIDDIQUI
- Web page: https://patentgrep.com/patent/US20230055218A1

## CPC

- B01J 20/186: {Chemical treatments in view of modifying the properties of the sieve, e.g. increasing the stability or the activity, also decreasing the activity}
- B01J 20/0259: {Compounds of N, P, As, Sb, Bi}
- B01J 20/0262: {Compounds of O, S, Se, Te}
- B01J 20/041: {Oxides or hydroxides}
- B01J 20/28004: {Sorbent size or size distribution, e.g. particle size}
- B01J 20/28061: {being in the range 100-500 m2/g}
- B01J 20/28064: {being in the range 500-1000 m2/g}
- B01J 20/28066: {being more than 1000 m2/g}
- B01J 20/28071: {being less than 0.5 ml/g}
- B01J 20/28073: {being in the range 0.5-1.0 ml/g}
- B01J 20/3028: {Granulating, agglomerating or aggregating}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3416: {of sorbents or filter aids comprising free carbon, e.g. activated carbon}
- C02F 1/281: {using inorganic sorbents}
- C02F 1/286: {using natural organic sorbents or derivatives thereof}
- B01J 2220/42: Materials comprising a mixture of inorganic materials (materials coated or impregnated on a carrier B01J20/32)
- C02F 2101/206: {Manganese or manganese compounds}
- C02F 2101/22: Chromium or chromium compounds, e.g. chromates
- C02F 2101/308: {Dyes; Colorants; Fluorescent agents}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

A porous activated asphaltene material is described with a method of making and a method of using for the adsorption of a contaminant from a solution. The porous activated asphaltene material may be made by functionalizing solid asphaltene with nitric acid, and then treating the product with a metal hydroxide. The resulting porous activated asphaltene material exhibits a high porosity, and may be cleaned and reused for adsorbing contaminants.

## Claims

### Claim 1

(canceled)

### Claim 2 (depends on 8)

The method of claim 8, wherein the porous activated asphaltene material has an average particle size of 1-20 μm.

### Claim 3 (depends on 8)

The method of claim 8, wherein the porous activated asphaltene material has a particle size distribution of 0.5-100 μm, wherein at least 60% of the particles have a particle size of 1-20 μm.

### Claim 4 (depends on 8)

The method of claim 8, wherein the porous activated asphaltene material has a BET specific surface area of 2,000-4,700 m2/g.

### Claim 5 (depends on 8)

The method of claim 8, wherein the porous activated asphaltene material has a BET specific surface area of 4,000-4,600 m2/g.

### Claim 6

(canceled)

### Claim 7 (depends on 8)

The method of claim 8, wherein the porous activated asphaltene material has a pore volume of 0.1-0.7 cm3/g.

### Claim 8

A method for producing a porous activated asphaltene material, comprising:
refluxing a solid asphaltene in nitric acid for 1-8 hours to produce a refluxed mixture;
washing and drying the refluxed mixture to produce a functionalized asphaltene solid;
grinding the functionalized asphaltene solid with a metal hydroxide to produce a ground mixture;
heating the ground mixture at 300-1000° C. for 10-60 minutes to produce an activated powder;
washing and drying the activated powder to produce the porous activated asphaltene material;
wherein porous activated asphaltene material, comprises:
an asphaltene compound having an elemental composition of 55-77 wt % C, 10-40 wt % O, 1-3 wt % S, 0.6-1.7 wt % H, and 0.2-1.2 wt % N each relative to a total weight of the asphaltene compound, wherein the asphaltene compound has at least one active group selected from the group consisting of an amine group, a nitro group, a carbonyl group, a carboxylic group and a hydroxyl group, the at least one active group covalently bonded to an asphaltene core,
wherein the porous activated asphaltene material has a hierarchical porosity with a multi-modal pore distribution including first pores having a pore diameter in a range of 5-50 nm and second pores having a pore diameter of 3-5 μm, wherein the interior of the second pores connects with the first pores; and
wherein the porous activated asphaltene material has a BET specific surface area of 1,000-4,800 m2/g.

### Claim 9 (depends on 8)

The method of claim 8, wherein a mass ratio of the functionalized asphaltene solid to the metal hydroxide is 1:1-1:8.

### Claim 10 (depends on 8)

The method of claim 8, wherein the metal hydroxide is KOH.

### Claim 11 (depends on 8)

The method of claim 8, wherein during the heating, the ground mixture is maintained in an atmosphere consisting essentially of N2.

### Claim at position 12

12-30. (canceled)