# US 2023/0054285 A1 · Supercritical fluid injection foaming polylactide foam material and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0054285 A1
- Document ID: US20230054285A1
- Status: Published application
- Kind: A1
- Application number: 17/795,538
- Filed: 2020-09-11
- Published: 2023-02-23
- Earliest claimed: 2020-02-11
- Assignees: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Scieinces
- Applicants: Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Scieinces
- Inventors: Long WANG; Wenge ZHENG; Qian REN; Lihua ZHANG; Minghui WU; Fei WU; Haibin LUO
- Web page: https://patentgrep.com/patent/US20230054285A1

## CPC

- B29C 44/42: using pressure difference, e.g. by injection or by vacuum
- B29B 7/20: with intermeshing devices, e.g. screws
- B29B 7/726: {Measuring properties of mixture, e.g. temperature or density (B29B7/724 takes precedence)}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- B32B 5/18: characterised by features of a layer {of} foamed material
- C08J 5/06: using pretreated fibrous materials
- C08J 9/0061: {characterized by the use of several polymeric components}
- C08J 9/122: {Hydrogen, oxygen, CO2, nitrogen or noble gases}
- B29B 7/48: with intermeshing devices, e.g. screws
- B29B 7/603: {in measured doses, e.g. proportioning of several materials}
- B29B 7/7404: {Mixing devices specially adapted for foamable substances (B29B7/76 takes precedence)}
- B29B 7/84: Venting or degassing {; Removing liquids, e.g. by evaporating components}
- B29B 7/845: {Venting, degassing or removing evaporated components in devices with rotary stirrers}
- B29B 7/847: {Removing of gaseous components before or after mixing}
- B29B 7/92: Wood chips or wood fibres
- B29B 7/94: Liquid charges
- B29C 44/3442: {Mixing, kneading or conveying the foamable material (mixing plastics B29B7/00; mixing in general B01F)}
- B29C 44/3446: {Feeding the blowing agent}
- B29K 2067/046: {PLA, i.e. polylactic acid or polylactide}
- B29K 2201/00: Use of cellulose, modified cellulose or cellulose derivatives, e.g. viscose, as reinforcement
- B32B 2250/40: Symmetrical or sandwich layers, e.g. ABA, ABCBA, ABCCBA
- B32B 2266/0264: Polyester
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/72: Density
- C08J 9/0071: {Nanosized fillers, i.e. having at least one dimension below 100 nanometers}
- C08J 9/0076: {Nanofibres}
- C08J 9/0085: {Use of fibrous compounding ingredients (C08J9/0076 takes precedence)}
- C08J 9/009: {Use of pretreated compounding ingredients}
- C08J 2201/03: Extrusion of the foamable blend
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2203/08: Supercritical fluid
- C08J 2205/044: Micropores, i.e. average diameter being between 0,1 micrometer and 0,1 millimeter
- C08J 2367/04: Polyesters derived from hydroxy carboxylic acids, e.g. lactones (C08J2367/06 takes precedence)
- C08J 2401/02: Cellulose; Modified cellulose
- D21H 11/20: Chemically or biochemically modified fibres
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

The present application relates to a supercritical fluid injection foaming polylactide foam material and a preparation method therefor. The method includes: first obtaining a surface-modified cellulose nanofiber aqueous solution; then melting and blending the cellulose nanofiber aqueous solution and a polylactide twice; passing same through extrusion, cooling under water, and granulation so as to obtain a polylactide/cellulose nanofiber composite material; then plasticizing and melting the polylactide/cellulose nanofiber composite material in a microporous foaming injection molding machine; uniformly mixing same with a supercritical fluid foaming agent in the injection molding machine; injecting same into a mold cavity; and subjecting the resultant to post-treatment so as to obtain a polylactide foam material. The polylactide foam material has a sandwich structure, in which two outer surface layers are solid layers that do not contain any foam, and the sandwiched layer is a foam layer having a cellular structure.

## Claims

### Claim 1

A method for preparing a polylactide foam material by a supercritical fluid injection foaming method, comprising,
(1) adding dry cellulose pulp into an organic solvent and stirring at room temperature to obtain a modified cellulose nanofiber paste, successively washing the modified cellulose nanofiber paste with alcohol and deionized water to obtain a surface-modified cellulose nanofiber aqueous solution;
(2) adding a polylactide into a twin-screw extruder via a main feed inlet of the twin-screw extruder, and adding the surface-modified cellulose nanofiber aqueous solution into the twin-screw extruder via an additive feed inlet of the twin-screw extruder, mixing, melting, and extruding the polylactide and the surface-modified cellulose nanofiber firstly, to obtain a first extrudate, while removing vapor via a vent disposed on a charging barrel of the twin-screw extruder,
melting, mixing, and extruding the first extrudate secondly via the twin-screw extruder to obtain a mixture, extruding the mixture to obtain a second extrudate, cooling the second extrudate in water, and dicing to obtain a polylactide/cellulose nanofiber composite;
(3) disposing the polylactide/cellulose nanofiber composite in a microporous foaming injection molding machine to plastify and melt the polylactide/cellulose nanofiber composite, and injecting a supercritical foaming agent into the microporous foaming injection molding machine with a supercritical fluid equipment to obtain a homogeneous polymer/gas-mixed polymer melt; and
(4) injecting the polymer/gas-mixed polymer melt into a cavity of a die, maintaining a pressure in the die, opening the die, and foaming the polymer/gas-mixed polymer melt, and cooling and molding to obtain a polylactide foam material.

### Claim 2 (depends on 1)

The method of claim 1, wherein in step (1), the organic solvent is a mixed liquid of toluene, acetic acid, perchloric acid and acetic anhydride, wherein a volume ratio of toluene, acetic acid, perchloric acid and acetic anhydride is 100:80:(0.2-1.2):(1-10), a mass percentage of the cellulose nanofiber in the modified cellulose nanofiber paste is in a range of 5% to 40%, a diameter of the cellulose nanofiber is in a range of 5 nm to 50 nm, a length-diameter ratio of the cellulose nanofiber is in a range of 100 to 1000, and a duration of stirring at room temperature is in a range of 1 hour to 5 hours.

### Claim 3 (depends on 1)

The method of claim 1, wherein in step (1), the cellulose is one selected from ramie fiber, flax fiber, sisal fiber, jute fiber, hemp fiber, or bamboo fiber; and
in step (2), the polylactide is L-polylactic acid and/or D-polylactic acid, and a weight-average molecular weight of the polylactide is in a range of 100000 to 400000.

### Claim 4 (depends on 1)

The method of claim 1, wherein in step (2), a mass percentage of the cellulose nanofiber in the polylactide/cellulose nanofiber composite is in a range of 1% to 20%.

### Claim 5 (depends on 1)

The method of claim 1, wherein in step (2), a barrel temperature of mixing and melting the polylactide and the surface-modified cellulose nanofiber is in a range of 93 degrees centigrade to 99 degrees centigrade, and a screw speed of mixing and melting the polylactide and the surface-modified cellulose nanofiber is in a range of 100 rpm to 200 rpm; and a barrel temperature of melting and mixing the first extrudate is in a range of 140 degrees centigrade to 180 degrees centigrade, and a screw speed of melting and mixing the first extrudate is in a range of 100 rpm to 200 rpm.

### Claim 6 (depends on 1)

The method of claim 1, wherein in step (3), the supercritical foaming agent is selected from the group consisting of supercritical carbon dioxide, supercritical nitrogen, and any combination thereof.

### Claim 7 (depends on 6)

The method of claim 6, wherein the supercritical foaming agent is the supercritical carbon dioxide, and a mass percentage of the supercritical carbon dioxide in the polymer/gas-mixed polymer melt is in a range of 3% to 8%.

### Claim 8 (depends on 1)

The method of claim 1, wherein in step (3), a pressure of the supercritical foaming agent is in a range of 18 MPa to 30 MPa, and a screw temperature of the microporous foaming injection molding machine is in a range of 160 degrees centigrade to 240 degrees centigrade.

### Claim 9 (depends on 1)

The method of claim 1, wherein in step (4), an injection rate of the polymer/gas-mixed polymer melt is in a range of 1 mm/s to 300 mm/s, a temperature of the die is in a range of 40 degrees centigrade to 90 degrees centigrade, the pressure in the die is maintained in a range of 5 MPa to 100 MPa, and a duration of maintaining the pressure in the die is in a range of 0.2 seconds to 10 seconds, a speed of opening the die is in a range of 10 mm/s to 30 mm/s, an expansion ratio of the polymer/gas-mixed polymer melt is in a range of 2 times to 20 times, and duration of cooling is in a range of 5 seconds to 300 seconds.

### Claim 10 (depends on 1)

A polylactide foam material prepared by the method of claim 1, wherein the polylactide foam material is in a sandwich-shaped structure, which includes two outer surface layers and a sandwiched layer,
the two outer surface layers are solid layers without any foam, and the sandwiched layer is a foam layer comprising porous structures,
wherein a density of the polylactide foam material is in a range of 0.05 g/cm3 to 0.7 g/cm3, and a maximum tensile strength of the polylactide foam material is 60 MPa, and a maximum Young's modulus of the polylactide foam material is 2.2 GPa.

### Claim 11 (depends on 6)

The method of claim 6, wherein the supercritical foaming agent is the supercritical nitrogen, and a mass percentage of the supercritical nitrogen in the polymer/gas-mixed polymer melt is in a range of 0.2% to 0.8%.