# US 2023/0053998 A1 · Product containing an anionic cellulose derivative and its use in paper industry

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053998 A1
- Document ID: US20230053998A1
- Status: Published application
- Kind: A1
- Application number: 17/794,618
- Filed: 2021-01-22
- Published: 2023-02-23
- Earliest claimed: 2020-01-22
- Assignees: Kemira Oyj
- Applicants: Kemira Oyj
- Inventors: Mikko VIRTANEN; Kaisa KARISALMI; Sanna LEHTO; Jan-Luiken HEMMES
- Web page: https://patentgrep.com/patent/US20230053998A1

## CPC

- D21H 11/18: Highly hydrated, swollen or fibrillatable fibres
- D21H 17/25: Cellulose
- D21H 17/28: Starch
- D21H 17/29: cationic
- D21H 17/375: {Poly(meth)acrylamide}
- D21H 17/45: Nitrogen-containing groups
- D21H 17/68: siliceous, e.g. clays
- D21H 17/74: {of organic and inorganic material}
- D21H 21/10: Retention agents or drainage improvers
- D21H 21/20: Wet strength agents
- D21H 23/04: Addition to the pulp; After-treatment of added substances in the pulp
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A product includes a microfibrillated cellulose composition, a starch derivative, and an anionic cellulose derivative, as a combined preparation for simultaneous or separate use. The anionic cellulose derivative has a number average molecular weight comprised between 300000 g/mol and 800000 g/mol, and a degree of substitution comprised between 0.3 and 0.65. Additionally, a paper sheet includes the product as an additive to increase the initial wet web strength and/or dry tensile strength of the paper sheet.

## Claims

### Claim 1

A product comprising:
a microfibrillated cellulose composition,
a starch derivative, and
an anionic cellulose derivative having a number average molecular weight comprised between 300000 g/mol and 800000 g/mol, and a degree of substitution comprised between 0.3 and 0.65,
as a combined preparation for simultaneous or separate use.

### Claim 2 (depends on 1)

The product of claim 1, wherein the microfibrillated cellulose of the microfibrillated cellulose composition is not chemically modified nor physically modified.

### Claim 3 (depends on 1)

The product of claim 1, wherein the starch derivative is a cationic starch.

### Claim 4 (depends on 1)

The product of claim 1, wherein the degree of substitution of the anionic cellulose derivative is comprised between 0.45 and 0.5.

### Claim 5

An admixture composition comprising:
an aqueous pulp mixture,
a microfibrillated cellulose composition,
a starch derivative, and
an anionic cellulose derivative having a number average molecular weight comprised between 300000 g/mol and 800000 g/mol, and a degree of substitution comprised between 0.3 and 0.65.

### Claim 6 (depends on 5)

The admixture composition of claim 5, wherein the aqueous pulp mixture comprises at least 80 wt % of short fibers, relative to a total weight of fibers.

### Claim 7 (depends on 5)

The admixture composition of claim 5, wherein the microfibrillated cellulose of the microfibrillated cellulose composition is not chemically modified nor physically modified.

### Claim 8 (depends on 5)

The admixture composition of claim 5, wherein the starch derivative is a cationic starch.

### Claim 9 (depends on 5)

The admixture composition of claim 5, wherein the degree of substitution of the anionic cellulose derivative is comprised between 0.45 and 0.5.

### Claim 10 (depends on 5)

The admixture composition of claim 5, further comprising a retention system.

### Claim 11 (depends on 10)

The admixture composition of claim 10, wherein the retention system comprises at least one cationic polyacrylamide.

### Claim 12 (depends on 5)

The admixture composition of claim 5, wherein an amount of microfibrillated cellulose composition is comprised between 0.3 wt % and 5 wt %, based on a dry solid content of the microfibrillated cellulose composition relative to a dry solid content of the aqueous pulp mixture.

### Claim 13 (depends on 5)

The admixture composition of claim 5, wherein an amount of starch derivative is comprised between 0.1 wt % and 2 wt %, based on a dry solid content of the starch derivative relative to a dry solid content of the aqueous pulp mixture.

### Claim 14 (depends on 5)

The admixture composition of claim 5, wherein an amount of anionic cellulose derivative is comprised between 0.05 wt % and 0.3 wt %, based on a dry solid content of the anionic cellulose derivative relative to a dry solid content of the aqueous pulp mixture.

### Claim 15 (depends on 5)

A method for preparing the admixture composition of claim 5, comprising:
providing the aqueous pulp mixture, and
admixing to the aqueous pulp mixture, the microfibrillated cellulose composition, the starch derivative, and the anionic cellulose derivative, and.

### Claim 16 (depends on 15)

The method of claim 15, wherein the aqueous pulp mixture has a solid content of less than 3% of a total solids content in the aqueous pulp mixture.

### Claim 17 (depends on 15)

The method of claim 15, wherein the retention system of the admixture composition comprises at least one of cationic polyacrylamide and silica.

### Claim 18 (depends on 5)

A method for preparing a paper product, comprising:
providing an aqueous pulp mixture,
admixing to the aqueous pulp mixture, a microfibrillated cellulose composition, a starch derivative and an anionic cellulose derivative, to form the admixture composition of claim 5, and
forming a wet sheet by draining the admixture composition, and.

### Claim 19 (depends on 18)

The method of claim 18, wherein the anionic cellulose derivative is added to the aqueous pulp mixture at least 10 minutes before a wet sheet formation.

### Claim 20

A paper product comprising a microfibrillated cellulose composition, a starch derivative, and an anionic cellulose derivative having a number average molecular weight comprised between 300000 g/mol and 800000 g/mol, and a degree of substitution comprised between 0.3 and 0.65.

### Claim 21 (depends on 1)

A paper sheet comprising the product of claim 1, as an additive to increase at least one of an initial wet web strength and a dry tensile strength of the paper sheet.

### Claim 22 (depends on 15)

The method of claim 15, further comprising admixing a retention system.

### Claim 23 (depends on 16)

The method of claim 16, wherein the aqueous pulp mixture has a solid content of less than 3% of a total solids content in the aqueous pulp mixture.

### Claim 24 (depends on 20)

The method of claim 20, further comprising admixing a retention system to form the admixture composition.