# US 2023/0053953 A1 · Group iii nitride structures and manufacturing methods thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053953 A1
- Document ID: US20230053953A1
- Status: Published application
- Kind: A1
- Application number: 17/434,543
- Filed: 2020-05-12
- Published: 2023-02-23
- Earliest claimed: 2020-05-12
- Assignees: Enkris Semiconductor, Inc.
- Applicants: Enkris Semiconductor, Inc.
- Inventors: Kai CHENG; Weihua LIU
- Web page: https://patentgrep.com/patent/US20230053953A1

## CPC

- H10P 14/3216: {Nitrides}
- H10H 20/0133: {with a substrate not being Group III-V materials}
- H10H 20/0137: {the light-emitting regions comprising nitride materials}
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/276: {Lateral overgrowth}
- H10P 14/3416: {Nitrides}
- H10H 20/817: characterised by the crystal structures or orientations, e.g. polycrystalline, amorphous or porous
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A group-III-nitride structure and a manufacturing method thereof are provided. In the manufacturing method, one or more grooves are formed by etching a first group-III-nitride epitaxial layer with a patterned first mask layer as a mask; then a second mask layer is formed at least on one or more bottom walls of the one or more grooves, and a first epitaxial growth is performed on the first group-III-nitride epitaxial layer to laterally grow and form a second group-III-nitride epitaxial layer with the second mask layer as a mask, where the one or more grooves are filled with the second group III-nitride epitaxial layer; a second epitaxial growth is then performed on the second group-III-nitride epitaxial layer to grow and form a third group-III-nitride epitaxial layer on the second group-III-nitride epitaxial layer and the patterned first mask layer.

## Claims

### Claim 1

A method of manufacturing a group-III-nitride structure, comprising:
providing a first group-III-nitride epitaxial layer; forming a patterned first mask layer on the first group-III-nitride epitaxial layer; and etching the first group-III-nitride epitaxial layer to form one or more grooves with the patterned first mask layer as a mask;
forming a second mask layer at least on one or more bottom walls of the one or more grooves; and laterally growing and forming a second group-III-nitride epitaxial layer by performing a first epitaxial growth on the first group-III-nitride epitaxial layer with the second mask layer as a mask, where the one or more grooves are filled with the second group-III-nitride epitaxial layer; and
growing and forming a third group-III-nitride epitaxial layer on the second group-III-nitride epitaxial layer and the patterned first mask layer by performing a second epitaxial growth on the second group-III-nitride epitaxial layer.

### Claim 2 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein the first group-III-nitride epitaxial layer is located on a substrate the one or more bottom walls of the one or more grooves expose the substrate and the substrate serves as the second mask layer.

### Claim 3 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein the second mask layer is further formed on the patterned first mask layer, and the third group-III-nitride epitaxial layer is grown and formed on the second mask layer.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein a material of the first group-III-nitride epitaxial layer, a material of the second group-III-nitride epitaxial layer and a material of the third group-III-nitride epitaxial layer are the same, and comprise at least one of GaN, AlN, AlGaN, InGaN or AlInGaN.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein the processes for the epitaxial growth of the second group-III-nitride epitaxial layer and the third group-III-nitride epitaxial layer are the metal organic compound chemical vapor deposition method; and forming the second mask layer, and growing the second group-III-nitride epitaxial layer and the third group-III-nitride epitaxial layer are performed in a same metal organic compound chemical vapor deposition device.

### Claim 8 (depends on 7)

The method of manufacturing the group-III-nitride structure according to claim 7, wherein etching to form the one or more grooves forming the second mask layer, and growing the second group-III-nitride epitaxial layer and the third group-III-nitride epitaxial layer are performed in the same metal organic compound chemical vapor deposition device.

### Claim 9 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein when the third group-III-nitride epitaxial layer on the patterned first mask layer is not coalesced, further growing and forming a fourth group-III-nitride epitaxial layer on the patterned first mask layer and the third group-III-nitride epitaxial layer.

### Claim 10 (depends on 9)

The method of manufacturing the group-III-nitride structure according to claim 9, further comprising: growing an LED structure on the fourth group-III-nitride epitaxial layer.

### Claim 11 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, further comprising: growing an LED structure on the third group-III-nitride epitaxial layer.

### Claim 12 (depends on 1)

The method of manufacturing the group-III-nitride structure according to claim 1, wherein a method of forming the first group-III-nitride epitaxial layer comprises: epitaxially growing the first group-III-nitride epitaxial layer on a substrate.

### Claim 13

(canceled)

### Claim 14

A group-III-nitride structure, comprising:
a first group-III-nitride epitaxial layer, where a patterned first mask layer is located on the first group-III-nitride epitaxial layer;
a second group-III-nitride epitaxial layer extending into the first group-III-nitride epitaxial layer from one or more openings of the patterned first mask layer, wherein a second mask layer is provided between a bottom wall of the second group-III-nitride epitaxial layer and the first group-III-nitride epitaxial layer, and a sidewall of the second group-III-nitride epitaxial layer is connected with the first group-III-nitride epitaxial layer; and
a third group-III-nitride epitaxial layer located on the second group-III-nitride epitaxial layer and the patterned first mask layer, wherein [0001] crystal orientations of the first group-III-nitride epitaxial layer, the second group-III-nitride epitaxial layer and the third group-III-nitride epitaxial layer are parallel to a thickness direction.

### Claim 15 (depends on 14)

The group-III-nitride structure according to claim 14, wherein a material of the first group-III-nitride epitaxial layer, a material of the second group-III-nitride epitaxial layer and a material of the third group-III-nitride epitaxial layer are the same, and comprise at least one of GaN, AlN, AlGaN, InGaN or AlInGaN.

### Claim 16 (depends on 14)

The group-III-nitride structure according to claim 14, further comprising: a substrate, wherein the first group-III-nitride epitaxial layer is located on the substrate.

### Claim 17 (depends on 16)

The group-III-nitride structure according to claim 16, wherein the substrate serves as the second mask layer.

### Claim 18

(canceled)

### Claim 19 (depends on 14)

The group-III-nitride structure according to claim 14, wherein the patterned first mask layer further has the second mask layer located thereon, and the third group-III-nitride epitaxial layer is located on the second mask layer.

### Claim 20 (depends on 14)

The group-III-nitride structure according to claim 14, wherein a material of the first mask layer comprises at least one of silicon dioxide or silicon nitride; and/or a material of the second mask layer comprises at least one of silicon dioxide or silicon nitride.

### Claim 21 (depends on 14)

The group-III-nitride structure according to claim 14, wherein the second group-III-nitride epitaxial layer is an in-situ second group-III-nitride epitaxial layer; and/or the second mask layer is an in-situ second mask layer.

### Claim 22 (depends on 14)

The group-III-nitride structure according to claim 14, wherein the third group-III-nitride epitaxial layer located on the patterned first mask layer is not coalesced, and the patterned first mask layer and the third group-III-nitride epitaxial layer have a fourth group-III-nitride epitaxial layer located thereon.

### Claim 23 (depends on 22)

The group-III-nitride structure according to claim 22, further comprising: an LED structure located on the fourth group-III-nitride epitaxial layer.

### Claim 24 (depends on 14)

The group-III-nitride structure according to claim 14, further comprising: an LED structure located on the third group-III-nitride epitaxial layer.