# US 2023/0053945 A1 · Methods for processing semiconductor structures and methods for forming semiconductor structures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053945 A1
- Document ID: US20230053945A1
- Status: Published application
- Kind: A1
- Application number: 17/438,454
- Filed: 2021-05-24
- Published: 2023-02-23
- Earliest claimed: 2020-07-02
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Ning XI
- Web page: https://patentgrep.com/patent/US20230053945A1

## CPC

- H10P 50/694: {characterised by their behaviour during the process, e.g. soluble masks or redeposited masks}
- H10P 70/20: {Cleaning during device manufacture}
- H10P 50/283: {by chemical means}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments of the present application provide a method for processing a semiconductor structure and a method for forming a semiconductor structure. The method for processing a semiconductor structure includes: providing a semiconductor substrate, the semiconductor substrate being provided with a feature portion, the aspect ratio of the feature portion being greater than a preset aspect ratio, a mask layer being provided on the top of the feature portion; ashing a semiconductor structure, the semiconductor structure comprising the semiconductor substrate, the feature portion, and the mask layer; cleaning the semiconductor structure; drying the semiconductor structure; and removing the mask layer.

## Claims

### Claim 1

A method for processing a semiconductor structure, comprising:
providing a semiconductor substrate, the semiconductor substrate being provided with feature portions, an aspect ratio of the feature portions being greater than a preset aspect ratio, mask layers being provided on a top of feature portions;
ashing a semiconductor structure, the semiconductor structure comprising the semiconductor substrate, the feature portions, and the mask layers;
cleaning the semiconductor structure;
drying the semiconductor structure; and
removing the mask layers;
wherein, during the drying process, one mask layer in at least a set of adjacent mask layers is tilted toward the adjacent mask layer, and after the drying process, the distance between the tilted mask layer and the adjacent mask layer is less than the distance between the two before the drying process.

### Claim 2 (depends on 1)

The method for processing a semiconductor structure according to claim 1, wherein the ashing the semiconductor structure comprises:
ashing the semiconductor structure with a first mixed gas containing no oxygen.

### Claim 3 (depends on 2)

The method for processing a semiconductor structure according to claim 2, the first mixed gas comprises at least hydrogen and nitrogen.

### Claim 4 (depends on 1)

The method for processing a semiconductor structure according to claim 1, wherein the ashing the semiconductor structure comprises:
ashing the semiconductor structure with a second mixed gas containing oxygen.

### Claim 5 (depends on 4)

The method for processing a semiconductor structure according to claim 4, the second mixed gas comprises at least hydrogen, nitrogen, and oxygen.

### Claim 6 (depends on 1)

The method for processing a semiconductor structure according to claim 1, wherein the cleaning the semiconductor structure comprises:
subjecting the semiconductor structure to a first cleaning process, with an oxide layer formed on a surface of the semiconductor structure after the first cleaning process; and
subjecting the semiconductor structure to a second cleaning process, the second cleaning process being used to remove the oxide layer.

### Claim 7 (depends on 6)

The method for processing a semiconductor structure according to claim 6, the first cleaning process uses a mixed liquid of NH4OH, H2O2, and H2O, and a volume ratio of NH4OH, H2O2 and H2O is NH4OH:H2O2:H2O=1:1-4:20-100.

### Claim 8 (depends on 6)

The method for processing a semiconductor structure according to claim 6, the second cleaning process uses a mixed liquid of HF with concentration 30%-70% and H2O, and a volume ratio of HF with concentration 30%-70% and H2O is HF with concentration 30%-70%:H2O=100-300:1.

### Claim 9 (depends on 1)

The method for processing a semiconductor structure according to claim 1, wherein the drying the semiconductor structure comprises:
drying surfaces of the feature portions with isopropanol at a first temperature; and
drying a bottom of the semiconductor substrate with deionized water at a second temperature while drying the surfaces of the feature portions.

### Claim 10 (depends on 9)

The method for processing a semiconductor structure according to claim 9, the first temperature ranges from 60° C. to 80° C. and the second temperature ranges from 60° C. to 80° C.

### Claim 11 (depends on 1)

The method for processing a semiconductor structure according to claim 1, wherein the removing the mask layers comprise:
providing, to mask layers, a chemical gas which chemically reacts with the mask layers at a third temperature; and
after the chemical reaction, heating the mask layers at a fourth temperature while providing a carrier gas to the mask layers to remove the mask layers by evaporation.

### Claim 12 (depends on 11)

The method for processing a semiconductor structure according to claim 11, the third temperature ranges from 30° C. to 150° C. and the fourth temperature ranges from 100° C. to 200° C.

### Claim 13 (depends on 11)

The method for processing a semiconductor structure according to claim 11, the etch selectivity ratio of the chemical gas to the mask layers and the feature portions is greater than 500:1.

### Claim 14 (depends on 13)

The method for processing a semiconductor structure according to claim 13, the chemical gas comprises at least ammonia and hydrogen fluoride, and the carrier gas comprises at least nitrogen or argon.

### Claim 15 (depends on 1)

The method for processing a semiconductor structure according to claim 1, the preset aspect ratio is 10.

### Claim 16

A method for forming a semiconductor structure, comprising:
providing a semiconductor substrate and a mask layer on the semiconductor substrate;
etching, by using the mask layer as a mask, the semiconductor substrate to form discrete feature portions, a aspect ratio of the feature portions being greater than a preset aspect ratio;
sequentially ashing, cleaning and drying the semiconductor structure, the semiconductor structure comprising the semiconductor substrate, the feature portions, and the mask layer; and
removing the mask layer.

### Claim 17 (depends on 16)

The method for forming a semiconductor structure according to claim 16, the preset aspect ratio is 10.