# US 2023/0053509 A1 · Silicon carbide single crystal wafer, crystal, preparation methods therefor, and semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053509 A1
- Document ID: US20230053509A1
- Status: Published application
- Kind: A1
- Application number: 17/796,863
- Filed: 2020-12-03
- Published: 2023-02-23
- Earliest claimed: 2020-11-25
- Assignees: Tankeblue Semiconductor Co., Ltd.; Xinjiang Tankeblue Semiconductor Co. Ltd; Jiangsu Tankeblue Semiconductor Co., Ltd
- Applicants: Tankeblue Semiconductor Co., Ltd.; Xinjiang Tankeblue Semiconductor Co. Ltd; Jiangsu Tankeblue Semiconductor Co., Ltd
- Inventors: Chunjun LIU; Yanfang LOU; Tonghua PENG; Bo WANG; Ning ZHAO; Yu GUO; Jian YANG; Ping ZHANG; Yu ZOU; Fan YANG
- Web page: https://patentgrep.com/patent/US20230053509A1

## CPC

- H10D 62/8325: {Silicon carbide}
- C01B 32/956: Silicon carbide
- C30B 23/00: Single-crystal growth by condensing evaporated or sublimed materials
- C30B 23/02: Epitaxial-layer growth
- C30B 29/36: Carbides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H10D 62/405: {Orientations of crystalline planes}
- C01P 2006/10: Solid density
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A silicon carbide single crystal wafer and a preparation method therefor, a silicon carbide crystal and a preparation method therefor, and a semiconductor device. The surface of the silicon carbide single crystal wafer is such that an included angle between a normal direction and a c direction is 0-8 degrees, and aggregated dislocations on the silicon carbide single crystal wafer are less than 300/cm2; the aggregated dislocation is a dislocation aggregated condition in which the distance between the geometric centers of any two corrosion pits in the corrosion pits obtained after corrosion of melted KOH is less than 80 microns. Even if the dislocation density is relatively high, the aggregated dislocation density is relatively small, thereby increasing the yield of a silicon carbide-based devices.

## Claims

### Claim 1

A silicon carbide monocrystalline wafer, wherein:
an included angle between a normal direction of a surface of the silicon carbide monocrystalline wafer and a direction of a c-axis ranges from 0° to 8°, end points included;
a density of clustered dislocations in the silicon carbide monocrystalline wafer is lower than 300/cm2; and
the clustered dislocations constitute a dislocation cluster, in which a distance between geometric centers of every two of etching pits is less than 80 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein the etching pits are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 2 (depends on 1)

The silicon carbide monocrystalline wafer according to claim 1, wherein:
the clustered dislocations are clustered threading screw dislocations;
the included angle between the normal direction of the surface of the silicon carbide monocrystalline wafer and the direction of the c-axis ranges from 0° to 8°, end points included;
a density of the clustered threading screw dislocations on the silicon carbide monocrystalline wafer is less than 20/cm2; and
the clustered threading screw dislocations constitute a dislocation cluster in which a distance between geometric centers of every two of etching pits corresponding to threading screw dislocations is less than 80 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein the etching pits corresponding to the threading screw dislocations are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 3 (depends on 2)

The silicon carbide monocrystalline wafer according to claim 2, wherein:
the clustered dislocations are clustered threading screw dislocations;
the included angle between the normal direction of the surface of the silicon carbide monocrystalline wafer and the direction of the c-axis ranges from 0° to 8°, end points included;
a density of the clustered threading screw dislocations on the silicon carbide monocrystalline wafer is less than 5/cm2; and
the clustered threading screw dislocations constitute a dislocation cluster in which a distance between geometric centers of every two of etching pits corresponding to threading screw dislocations is less than 60 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein the etching pits corresponding to the threading screw dislocations are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 4 (depends on 1)

The silicon carbide monocrystalline wafer according to claim 1, wherein:
the clustered dislocations are clustered basal plane dislocations;
the included angle between the normal direction of the surface of the silicon carbide monocrystalline wafer and the direction of the c-axis ranges from 2° to 8°, end points included;
a density of the clustered basal plane dislocations on the silicon carbide monocrystalline wafer is less than 50/cm2; and
the clustered basal plane dislocations constitute a dislocation cluster in which a distance between geometric centers of every two of etching pits corresponding to basal plane dislocations is less than 40 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein the etching pits corresponding to the basal plane dislocations are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 5 (depends on 1)

The silicon carbide monocrystalline wafer according to claim 1, wherein:
the clustered dislocations are clustered threading edge dislocations;
the included angle between the normal direction of the surface of the silicon carbide monocrystalline wafer and the direction of the c-axis ranges from 0° to 8°, end points included;
a density of the clustered threading edge dislocations on the silicon carbide monocrystalline wafer is less than 200/cm2; and
the clustered threading edge dislocations constitute a dislocation cluster in which a distance between geometric centers of every two of etching pits is less than 40 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein the etching pits are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 6 (depends on 1)

The silicon carbide monocrystalline wafer according to claim 1, wherein:
the clustered dislocations are clustered hybrid dislocation;
the included angle between the normal direction of the surface of the silicon carbide monocrystalline wafer and the direction of the c-axis ranges from 2° to 8°, end points included;
a density of the clustered hybrid dislocations on the silicon carbide monocrystalline wafer is less than 50/cm2; and
the clustered hybrid dislocations constitute a dislocation cluster in which a distance between geometric centers of every two of etching pits that correspond to dislocations of different types is less than 60 μm when the silicon carbide monocrystalline wafer is etched by using molten potassium hydroxide, wherein and the etching pits are exposed on the surface of the silicon carbide monocrystalline wafer.

### Claim 7

A method for manufacturing a silicon carbide crystal, comprising:
sealing a crucible with a graphite cover having no seed crystal, wherein the crucible is filled with silicon carbide charge;
preprocessing the crucible sealed with the graphite cover;
providing a seed crystal, wherein a density of clustered dislocations in the seed crystal is less than 200/cm2;
installing a graphite cover having the seed crystal on the pre-processed crucible, wherein the pre-processed graphite cover is replaced with the graphite cover having the seed crystal;
and growing the silicon carbide crystal; and
performing in-situ annealing.

### Claim 8 (depends on 7)

The method according to claim 7, wherein a density of clustered screw dislocations in the seed crystal is less than 10/cm2.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the preprocessing comprises:
setting a temperature in the crucible in a range from 2000° C. to 2200° C. and a pressure in the crucible less than 10 Pa; and
exhausting the crucible continuously with a vacuum pump; and
wherein the pre-processing lasts for 1 hour to 10 hours.

### Claim 10 (depends on 7)

The method according to claim 7, wherein growing the silicon carbide crystal comprises:
growing the silicon carbide crystal by using the graphite cover having the seed crystal in which the density of the clustered dislocations is less than 200/cm2, under a growth temperature ranging from 2200° C. and 2300° C. and a growth pressure ranging from 50 Pa to 4000 Pa, wherein fluctuations of the growth temperature are less than 2° C. and fluctuations of the growth pressure are less than 0.2 Pa.

### Claim 11 (depends on 7)

The method according to claim 7, wherein the in-situ annealing comprises:
annealing, for a period ranging from 10 hours to 100 hours, at a temperature which is higher than the growth temperature by a difference ranging from 50° C. to 200° C. and at a pressure which is higher than 20000 Pa.

### Claim 12 (depends on 7, 8, 9, 10, 11)

A silicon carbide crystal, manufactured by the method according to any one of claims 7 to 11.

### Claim 13 (depends on 12)

A method for manufacturing a silicon carbide monocrystalline wafer, comprising:
providing the silicon carbide crystal according to claim 12, and cutting, grinding, and polishing the silicon carbide crystal to obtain a silicon carbide monocrystalline wafer.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6)

A semiconductor device, manufactured by using the silicon carbide monocrystalline wafer according to any one of claims 1 to 6.