# US 2023/0053417 A1 · Film deposition methods in furnace tube, and semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053417 A1
- Document ID: US20230053417A1
- Status: Published application
- Kind: A1
- Application number: 17/438,831
- Filed: 2021-05-24
- Published: 2023-02-23
- Earliest claimed: 2020-12-03
- Assignees: Changxin Memory Technologies, Inc.
- Applicants: Changxin Memory Technologies, Inc.
- Inventors: Qizan HUANG
- Web page: https://patentgrep.com/patent/US20230053417A1

## CPC

- H10P 72/0602: {Temperature monitoring}
- C23C 16/345: {Silicon nitride}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/46: characterised by the method used for heating the substrate (C23C16/48, C23C16/50 take precedence)
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C 16/56: After-treatment
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

The present disclosure discloses a film deposition method in furnace tube, and a semiconductor device. The film deposition method in furnace tube includes: providing a furnace tube, a process chamber in the furnace tube being divided into a plurality of process regions in the top-bottom direction, a plurality of temperature controllers being in one-to-one correspondence to the plurality of process regions to separately control the temperature of the plurality of process regions; providing a substrate, performing a deposition process of a film on the substrate, the temperature controllers being controlled so that the set deposition temperatures of the process regions gradually decrease in a gradient in the top-to-bottom direction; and performing an annealing process, the temperature controllers being controlled so that the set annealing temperatures of the process regions gradually increase in a gradient in the top-to-bottom direction.

## Claims

### Claim 1

A film deposition method in furnace tube, comprising:
providing a furnace tube, a process chamber in the furnace tube being divided into a plurality of process regions in the top-bottom direction, a plurality of temperature controllers being in one-to-one correspondence to the plurality of process regions to separately control the temperature of the plurality of process regions;
providing a substrate, performing a deposition process of a film on the substrate, the temperature controllers being controlled so that the set deposition temperatures of the process regions gradually decrease in a gradient in the top-to-bottom direction; and
performing an annealing process, the temperature controllers being controlled so that the set annealing temperatures of the process regions gradually increase in a gradient in the top-to-bottom direction.

### Claim 2 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the temperature difference between the set deposition temperatures of any two adjacent process regions is 2° C. to 5° C.

### Claim 3 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the set deposition temperatures of any two adjacent process regions gradually decrease in a constant gradient.

### Claim 4 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the temperature difference between the set annealing temperatures of any two adjacent process regions is 2° C. to 5° C.

### Claim 5 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the set annealing temperatures of any two adjacent process regions gradually increase in a constant gradient.

### Claim 6 (depends on 3)

The film deposition method in furnace tube according to claim 3, wherein the set annealing temperatures of any two adjacent process regions gradually increase in a constant gradient.

### Claim 7 (depends on 6)

The film deposition method in furnace tube according to claim 6, wherein, the temperature gradient value by which the set deposition temperatures of any two adjacent process regions gradually decrease in a constant gradient is the same as the temperature gradient value by which the set annealing temperatures of any two adjacent process regions gradually increase in a constant gradient.

### Claim 8 (depends on 6)

The film deposition method in furnace tube according to claim 6, wherein the set deposition temperatures of the process regions in the top-to-bottom direction during the deposition process of the film are the same as the set annealing temperatures of the process regions in the bottom-to-top direction during the annealing process.

### Claim 9 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the set annealing temperatures of the process regions and the set deposition temperatures of the process regions are greater than or equal to 500° C. and less than or equal to 650° C.

### Claim 10 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the maximum temperature of the set deposition temperatures during the deposition process of the film and the maximum temperature of the set annealing temperatures during the annealing process are predetermined maximum temperatures.

### Claim 11 (depends on 10)

The film deposition method in furnace tube according to claim 10, wherein the predetermined maximum temperature is 650° C.

### Claim 12 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the minimum temperature of the set deposition temperatures during the deposition process of the film and the minimum temperature of the set annealing temperatures during the annealing process are predetermined minimum temperatures.

### Claim 13 (depends on 12)

The film deposition method in furnace tube according to claim 12, wherein the predetermined minimum temperature is 500° C.

### Claim 14 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the annealing process lasts for 120 min to 300 min.

### Claim 15 (depends on 1)

The film deposition method in furnace tube according to claim 1, during the annealing process, the film deposition method further comprising: introducing inert gas into the furnace tube.

### Claim 16 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the film is a silicon nitride film.

### Claim 17 (depends on 1)

The film deposition method in furnace tube according to claim 1, wherein the deposition process of the film comprises an atomic layer deposition process or a low pressure chemical vapor deposition method.

### Claim 18 (depends on 6)

The film deposition method in furnace tube according to claim 6, wherein the film is deposited on the surface of the substrate, the film is a continuous plane; and in the deposition process of the film, there is a first temperature difference between the set deposition temperatures of any two adjacent process regions; in the annealing process of the film, there is a second temperature difference between the set annealing temperatures of any two adjacent process regions; and the first temperature difference is greater than the second temperature difference.

### Claim 19 (depends on 6)

The film deposition method in furnace tube according to claim 6, wherein a trench is formed on the substrate, the film is formed on the surface of the trench and extends along the surface of the substrate; and in the deposition process of the film, there is a third temperature difference between the set deposition temperatures of any two adjacent process regions; in the annealing process of the film, there is a fourth temperature difference between the set annealing temperatures of any two adjacent process regions; and the third temperature difference is not greater than the fourth temperature difference.

### Claim 20 (depends on 1)

A semiconductor device, comprising: a substrate and a film arranged on the surface of the substrate, the film being formed according to the film deposition method of claim 1.