# US 2023/0053375 A1 · Method for fabricating oleophilic-hydrophobic nanofiber membrane and separation of water-in-oil emulsion using same method and waste heat

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0053375 A1
- Document ID: US20230053375A1
- Status: Published application
- Kind: A1
- Application number: 17/893,215
- Filed: 2022-08-23
- Published: 2023-02-23
- Earliest claimed: 2021-08-23
- Assignees: Postech Research and Business Development Foundation
- Applicants: POSTECH Research and Business Development Foundation
- Inventors: Geunbae LIM; Hyeonsu WOO
- Web page: https://patentgrep.com/patent/US20230053375A1

## CPC

- B01D 69/02: characterised by their properties
- B01D 17/045: {with coalescers}
- B01D 17/085: {with membranes}
- B01D 61/027: {Nanofiltration}
- B01D 67/0002: {Organic membrane manufacture}
- B01D 67/00042: {by deposition of fibres, nanofibres or nanofibrils}
- B01D 67/0086: {Mechanical after-treatment}
- B01D 69/04: Tubular membranes
- B01D 71/281: {Polystyrene}
- B01D 71/34: Polyvinylidene fluoride
- C02F 1/40: Devices for separating or removing fatty or oily substances or similar floating material (cleaning or keeping clear the surface of open water from oil or like materials E02B15/04; devices in sewers for separating liquid or solid substances from sewage E03F5/14, e.g. for use in drains leading to the sewer E03F5/16)
- C02F 1/44: by dialysis, osmosis or reverse osmosis {(general membrane separation processes B01D61/00, membrane modules B01D63/00, electrodialysis C02F1/4693, combination of membrane modules and bioreactors C02F3/1268)}
- C02F 1/442: {by nanofiltration}
- B01D 2323/10: Specific pressure applied
- B01D 2323/39: Electrospinning
- B01D 2325/0283: Pore size
- B01D 2325/04: Characteristic thickness
- B01D 2325/24: Mechanical properties, e.g. strength
- B01D 2325/38: Hydrophobic membranes
- C02F 2101/32: Hydrocarbons, e.g. oil
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)

## Abstract

The present invention relates to a lipophilic and hydrophobic nanofiber membrane and a method of preparing the same. The lipophilic and hydrophobic nanofiber membrane according to an exemplary embodiment may be compressed at a pressure of 10 kPa to 100 kPa and may have an average thickness of 10 μm to 1,500 μm.

## Claims

### Claim 1

A lipophilic and hydrophobic nanofiber membrane, wherein the lipophilic and hydrophobic nanofiber membrane is compressed at a pressure of 10 kPa to 100 kPa and has an average thickness of 10 μm to 1,500 μm.

### Claim 2 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
an average pore size of the lipophilic and hydrophobic nanofiber membrane is 500 μm or less.

### Claim 3 (depends on 2)

The lipophilic and hydrophobic nanofiber membrane of claim 2, wherein:
the average pore size of the lipophilic and hydrophobic nanofiber membrane is 5 μm to 100 μm.

### Claim 4 (depends on 3)

The lipophilic and hydrophobic nanofiber membrane of claim 3, wherein:
the lipophilic and hydrophobic nanofiber membrane is compressed at a pressure of 30 kPa to 60 kPa and has an average thickness of 200 μm to 1,000 μm.

### Claim 5 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
a porosity of the lipophilic and hydrophobic nanofiber membrane is 75% to 95%.

### Claim 6 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
a material of the lipophilic and hydrophobic nanofiber membrane includes at least one of polystyrene and polyvinylidene fluoride.

### Claim 7 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
the lipophilic and hydrophobic nanofiber membrane is formed of fibers having a long cylindrical shape, and the fibers have a crushed shape by being pressed against each other.

### Claim 8 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
the lipophilic and hydrophobic nanofiber membrane has a contact angle with respect to water of 100 degrees to 140 degrees when measured based on a surface of the lipophilic and hydrophobic nanofiber membrane.

### Claim 9 (depends on 1)

The lipophilic and hydrophobic nanofiber membrane of claim 1, wherein:
a contact angle with respect to oil is not measured based on a surface of the lipophilic and hydrophobic nanofiber membrane.

### Claim 10

A method of preparing a lipophilic and hydrophobic nanofiber membrane, the method comprising:
electrospinning a nanofiber membrane material on a substrate and collecting nanofibers; and
physically compressing the collected nanofibers to prepare a nanofiber membrane having a thickness of 10 μm to 1,500 μm,
wherein the compressing of the collected nanofibers is performed at a pressure of 10 kPa to 100 kPa.

### Claim 11 (depends on 10)

The method of claim 10, wherein:
in the electrospinning of the nanofiber membrane material on the substrate and the collecting of the nanofibers,
the electrospinning is performed for 1 minute to 60 minutes.

### Claim 12 (depends on 10)

The method of claim 10, wherein:
the compressing of the collected nanofibers is performed at a pressure of 10 kPa to 100 kPa, and
a thickness of the prepared nanofiber membrane is 10 μm to 1,500 μm.