# US 2023/0047189 A1 · Multi-stage polymeric latexes, coating compositions containing such latexes, and articles coated therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0047189 A1
- Document ID: US20230047189A1
- Status: Published application
- Kind: A1
- Application number: 17/882,332
- Filed: 2022-08-05
- Published: 2023-02-16
- Earliest claimed: 2017-09-01
- Assignees: Swimc LLC
- Applicants: Swimc LLC
- Inventors: Robert M. O'BRIEN; Mark STUETELBERG; Joseph D. DESOUSA; Mary Jo SCANDOLARI; Nikolaus KOCH; Stephen POLLIN; Nusrah HUSSAIN
- Web page: https://patentgrep.com/patent/US20230047189A1

## CPC

- C09D 5/027: {Dispersing agents (anti-settling agents C09D7/45)}
- B65D 25/14: Linings or internal coatings (of containers made by folding or erecting blanks made of paper B65D5/56 {; linings for domestic water storage heaters F24H1/183})
- B65D 25/34: Coverings or external coatings (of containers made by folding or erecting blanks made of paper B65D5/62; covering or external coating for bottles or jars not otherwise provided for B65D23/08; wrappers B65D65/00)
- C08F 220/06: Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 265/06: Polymerisation of acrylate or methacrylate esters on to polymers thereof
- C08F 291/06: on to oxygen-containing macromolecules
- C09D 151/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C09D151/04, C09D151/06 take precedence)}
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

An aqueous coating composition is provided that is useful in coating a variety of substrates, including interior or exterior portions of food or beverage cans. The coating composition includes a resin system that includes a multi-stage latex. In some embodiments, the multi-stage latex is formed using a process that includes emulsion polymerizing two or more stages in the presence of an aqueous dispersion including a water-dispersible polymer. In certain preferred embodiments, the water-dispersible polymer is a polyether polymer.

## Claims

### Claim at position 1

1-44. (canceled)

### Claim 45

An aqueous coating composition comprising:
a resin system including:
a water-dispersible polymer comprising a solution-polymerized acrylic polymer, a polyether polymer, a polyolefin polymer, a polyester polymer, or a mixture or copolymer thereof; and
a multi-stage polymeric latex having two or more emulsion polymerized stages in an aqueous carrier liquid, wherein the water-dispersible polymer is incorporated into the multi-stage polymeric latex, blended with the multi-stage polymeric latex, or both; the aqueous coating composition is a sprayable composition for a food or beverage container;
and wherein the latex has one or both of:
a lower Tg emulsion polymerized stage having a calculated Tg that is at least 20° C. lower than a calculated Tg of a higher Tg emulsion polymerized stage, or
(ii) a gradient Tg with at least a 20° C. differential in the calculated Tg of monomers fed at the start of polymerization compared to monomers fed at the end of polymerization; and
wherein the coating composition is substantially free of each of bisphenol A, bisphenol F, and bisphenol S.

### Claim 46 (depends on 45)

The coating composition of claim 45, wherein the aqueous carrier liquid contains greater than about 5% organic solvent based on the total weight of the aqueous carrier liquid.

### Claim 47 (depends on 45)

The coating composition of claim 45, wherein the latex polymer has the gradient Tg.

### Claim 48 (depends on 45)

The coating composition of claim 45, wherein the two or more emulsion polymerized stages are emulsion polymerized in the presence of the water-dispersible polymer.

### Claim 49 (depends on 48)

The coating composition of claim 48, wherein the weight ratio of water-dispersible polymer to emulsion polymerized stages is less than 50:50.

### Claim 50 (depends on 49)

The coating composition of claim 49, wherein the weight ratio of water-dispersible polymer to emulsion polymerized stages is less than 40:60, and wherein the coating composition does not contain styrene.

### Claim 51 (depends on 49)

The coating composition of claim 49, wherein the weight ratio of water-dispersible polymer to emulsion polymerized stages is less than 30:70.

### Claim 52 (depends on 49)

The coating composition of claim 49, wherein the water-dispersible polymer comprises an aromatic polyether polymer.

### Claim 53 (depends on 50)

The coating composition of claim 50, wherein the water-dispersible polymer comprises a polyether polymer formed from reactants including (i) an extender and (ii) a diepoxide of: an aromatic diol, an aromatic diacid, an aliphatic diol, an aliphatic diacid, a cycloaliphatic diol, a cycloaliphatic diacid, or a combination thereof.

### Claim 54 (depends on 49)

The coating composition of claim 49, wherein the water-dispersible polymer comprises a polyether-acrylate copolymer.

### Claim 55 (depends on 49)

The coating composition of claim 49, wherein the water-dispersible polymer has an acid number from 40 to 200 mg KOH per gram.

### Claim 56 (depends on 49)

The coating composition of claim 49, wherein the latex has a lower Tg emulsion polymerized stage having a calculated Tg that is at least 40° C. lower than a calculated Tg of the higher Tg emulsion polymerized stage.

### Claim 57 (depends on 45)

The coating composition of claim 45, wherein more than 50 weight percent of the emulsion polymerized stages have a calculated Tg of at least 40° C.

### Claim 58 (depends on 57)

The coating composition of claim 57, wherein polymerization of the lower Tg emulsion polymerized stage is initiated before initiating polymerization of the higher Tg emulsion polymerized stage.

### Claim 59 (depends on 45)

The coating composition of claim 45, wherein the coating composition, when spray applied onto an interior of a 355 mL no. 211 two-piece drawn and ironed aluminum beverage can at 115 milligrams per can coating weight and cured at 188° C. to 199° C. (measured at the can dome) for 55 seconds, exhibits:
(i) a global extraction result of less than 50 ppm,
(ii) a metal exposure of less than 3 mA on average when the can is filled with 1% NaCl in deionized water and tested pursuant to the Initial Metal Exposure test method disclosed herein, and
(iii) a metal exposure of less than 10 mA when tested pursuant to the Metal Exposure after Drop Damage test disclosed herein.

### Claim 60 (depends on 50)

The coating composition of claim 50, wherein the coating composition, when spray applied onto an interior of a 355 mL no. 211 two-piece drawn and ironed aluminum beverage can at 115 milligrams per can coating weight and cured at 188° C. to 199° C. (measured at the can dome) for 55 seconds, exhibits:
(i) a global extraction result of less than 50 ppm,
(ii) a metal exposure of less than 3 mA on average when the can is filled with 1% NaCl in deionized water and tested pursuant to the Initial Metal Exposure test method disclosed herein, and
(iii) a metal exposure of less than 3.5 mA when tested pursuant to the Metal Exposure after Drop Damage test disclosed herein.

### Claim 61 (depends on 59)

The coating composition of claim 59, wherein the coating composition, when spray applied onto an interior of a 355 mL no. 211 two-piece drawn and ironed aluminum beverage can at 115 milligrams per can coating weight and cured at 188° C. to 199° C. (measured at the can dome) for 55 seconds, exhibits a lower sidewall adhesion rating value of 9 or 10 after retort in 2% citric acid under pressure at 121° C. and tested according to ASTM D 3359—Test Method B.

### Claim 62 (depends on 57)

The coating composition of claim 57, wherein the coating composition, when spray applied onto an interior of a 355 mL no. 211 two-piece drawn and ironed aluminum beverage can at 115 milligrams per can coating weight and cured at 188° C. to 199° C. (measured at the can dome) for 55 seconds, is capable of passing a necking and flanging test as indicated by a change of metal exposure after necking of less than 1.0 mA.

### Claim 63 (depends on 49)

The coating composition of claim 49, wherein the resin system does not include and is not derived from any acrylamide-type monomers.

### Claim 64 (depends on 45)

The coating composition of claim 45, wherein the coating composition does not contain formaldehyde or formaldehyde-containing compounds.

### Claim 65 (depends on 64)

The coating composition of claim 64, wherein the coating composition comprises a beta-hydroxyalkyl-amide crosslinker.

### Claim 66

An aqueous coating composition comprising:
a resin system including:
a water-dispersible polymer having an acid number of at least 40 mg KOH per gram and comprising a solution-polymerized acrylic polymer, a polyether polymer, a polyolefin polymer, a polyester polymer, or a mixture or copolymer thereof;
and a multi-stage polymeric latex having two or more emulsion polymerized stages, wherein the two or more emulsion polymerized stages are emulsion polymerized in the presence of the water-dispersible polymer, and wherein the latex has one or both of a lower Tg emulsion polymerized stage having a calculated Tg that is at least 30° C. lower than a calculated Tg of a higher Tg emulsion polymerized stage; and
an aqueous carrier liquid that includes at least 5 wt-% of organic solvent; and
wherein the weight ratio of water-dispersible polymer to emulsion polymerized stages is less than 50:50; and
wherein the coating composition is an inside spray beverage can coating composition; is substantially free of each of bisphenol A, bisphenol F, and bisphenol S; and has a total solids weight of about 15 to about 25%, based on the total weight of the coating composition.

### Claim 67 (depends on 66)

The coating composition of claim 66, wherein more than 50 weight percent of the emulsion polymerized stages have a calculated Tg of at least 50° C.

### Claim 68 (depends on 67)

The coating composition of claim 67, wherein polymerization of the lower Tg emulsion polymerized stage is initiated before initiating polymerization of the higher Tg emulsion polymerized stage.

### Claim 69 (depends on 66)

The coating composition of claim 66, wherein the coating composition, when spray applied onto an interior of a 355 mL no. 211 two-piece drawn and ironed aluminum beverage can at 115 milligrams per can coating weight and cured at 188° C. to 199° C. (measured at the can dome) for 55 seconds, exhibits:
(i) a global extraction result of less than 50 ppm,
(ii) a metal exposure of less than 3 mA on average when the can is filled with 1% NaCl in deionized water and tested pursuant to the Initial Metal Exposure test method disclosed herein,
(iii) a metal exposure of less than 3.5 mA when tested pursuant to the Metal Exposure after Drop Damage test disclosed herein, and
(iv) a lower sidewall adhesion rating value of 9 or 10 after retort in 2% citric acid under pressure at 121° C. and tested according to ASTM D 3359—Test Method B.

### Claim 70 (depends on 69)

The coating composition of claim 69, wherein the coating composition does not include styrene.

### Claim 71 (depends on 66)

The coating composition of claim 66, wherein the resin system does not include and is not derived from any acrylamide-type monomers.

### Claim 72 (depends on 66)

The coating composition of claim 66, wherein the coating composition does not contain formaldehyde or formaldehyde-containing compounds.

### Claim 73 (depends on 66)

The coating composition of claim 66, wherein the coating composition comprises a beta-hydroxyalkyl-amide crosslinker.