# US 2023/0043883 A1 · Silicate modified polymer foam material for filling and sealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0043883 A1
- Document ID: US20230043883A1
- Status: Published application
- Kind: A1
- Application number: 17/945,440
- Filed: 2022-09-15
- Published: 2023-02-09
- Earliest claimed: 2022-01-28
- Assignees: WELEAD Infrastructure Engineering Technology (Zhengzhou), Ltd.; SAFEKEY Engineering Technology (Zhengzhou), Ltd.
- Applicants: WELEAD Infrastructure Engineering Technology (Zhengzhou), Ltd.; SAFEKEY Engineering Technology (Zhengzhou), Ltd.
- Inventors: Peng Zhao; Hongyuan Fang; Lei Wang; Chengchao Guo; Mingrui Du; Chao Zhang; Guobin Qiao
- Web page: https://patentgrep.com/patent/US20230043883A1

## CPC

- C08G 18/7614: {containing only one aromatic ring}
- C08G 18/7621: {being toluene diisocyanate including isomer mixtures}
- C08G 18/388: {having phosphorus bound to carbon and/or to hydrogen}
- C08G 18/3895: {Inorganic compounds, e.g. aqueous alkalimetalsilicate solutions; Organic derivatives thereof containing no direct silicon-carbon bonds}
- C08G 18/8054: {with compounds of C08G18/38}
- C08G 18/837: {by silicon containing compounds}
- C08J 9/125: {Water, e.g. hydrated salts}
- C08G 2110/0083: prepared using water as the sole blowing agent
- C08G 2190/00: Compositions for sealing or packing joints
- C08J 2203/10: Water or water-releasing compounds
- C08J 2375/04: Polyurethanes
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A silicate modified polymer foam material for filling and sealing contains prepolymerized isocyanate and a silicate modified aqueous solution with a mass ratio in a range of 1:(1.2-1.4). In the prepolymerized isocyanate, a mass percentage of P is 4.4%, a mass percentage of N is 7.9%, and a mass percentage of —NCO is 11.9%. The silicate modified aqueous solution includes liquid sodium silicate, small molecule alcohol, water and a catalyst, wherein the liquid sodium silicate, the small molecule alcohol, the water and the catalyst account for 63-66%, 17-20%, 14-17% and 1.5-2.5% of the weight of the silicate modified aqueous solution respectively. A method of preparing the silicate modified polymer foam material for filling and sealing includes mixing the prepolymerized isocyanate with the silicate modified aqueous solution.

## Claims

### Claim 1

A silicate modified polymer foam material for filling and sealing, which contains prepolymerized isocyanate and a silicate modified aqueous solution with a mass ratio in a range of 1:(1.2-1.4), wherein in the prepolymerized isocyanate, a mass percentage of P is 4.4%, a mass percentage of N is 7.9%, a mass percentage of —NCO is 11.9%, a structural formula of the prepolymerized isocyanate is
wherein the silicate modified aqueous solution comprises liquid sodium silicate, small molecule alcohol, water and a catalyst, wherein the liquid sodium silicate accounts for 63-66% of a weight of the silicate modified aqueous solution, the small molecule alcohol accounts for 17-20% of the weight of the silicate modified aqueous solution, the water accounts for 14-17% of the weight of the silicate modified aqueous solution, and the catalyst accounts for 1.5-2.5% of the weight of the silicate modified aqueous solution.

### Claim 2 (depends on 1)

The silicate modified polymer foam material for filling and sealing according to claim 1, wherein the small molecule alcohol is highly active and highly polar polyether which takes ethylene glycol as a reagent and is polymerized and end-capped with ethylene oxide, and has a molecular weight in a range of 400 to 600.

### Claim 3 (depends on 2)

The silicate modified polymer foam material for filling and sealing according to claim 2, wherein the small molecule alcohol is polyethylene glycol 400 or polyethylene glycol 600 produced by Jiangsu Haian Petrochemical Plant, China;
the liquid sodium silicate is 2451 of Qingdao Gulf Chemical Co., Ltd., China, is an aqueous solution of sodium silicate, and its Baume degree is 40;
the catalyst is a tertiary amine catalyst, and is preferably DABCO-T produced by Evonik Specialty Chemicals (Shanghai) Co., Ltd., China), or ZF-10 (Huntsman).

### Claim 4 (depends on 1)

A method of preparing a silicate modified polymer foam material for filling and sealing according to claim 1, wherein the silicate modified polymer foam material is obtained by mixing prepolymerized isocyanate and a silicate modified aqueous solution;
the prepolymerized isocyanate is prepared by a method comprising steps of:
(A) preparing 2-carboxyethylphenyl ethylene glycol hypophosphite by performing an esterification reaction on 2-carboxyethylphenyl hypophosphorous acid and ethylene glycol with a molar ratio of 1:1, wherein a reaction equation of the esterification reaction is
(B) obtaining a phosphorus-containing diol intermediate by performing an addition reaction on the 2-carboxyethylphenyl ethylene glycol hypophosphite and propylene oxide with a molar ratio of 1:1, wherein a reaction equation of the addition reaction is
and
(C) obtaining a difunctional modified flame retardant isocyanate compound, namely, the prepolymerized isocyanate, by performing a polymerization reaction on the phosphorus-containing diol intermediate and TDI, wherein a reaction equation of the polymerization reaction is

### Claim 5 (depends on 4)

The method of preparing the silicate modified polymer foam material for filling and sealing according to claim 4, the method comprising steps of:
(a) putting 2-carboxyethylphenyl hypophosphorous acid which is produced by Wuhan Hezhong Biochemical Manufacturing Co., Ltd., China and ethylene glycol with a molar ratio of 1:1 into a reactor, performing an esterification reaction at 105-110° C. under catalysis of sulfuric acid or organotin, and obtaining 2-carboxyethylphenyl ethylene glycol hypophosphite after distilling water produced by the esterification reaction from a top of the reactor;
(b) heating the 2-carboxyethylphenyl ethylene glycol hypophosphite to 100-110° C. in the reactor, slowly adding propylene oxide into the reactor under a premise of using potassium hydroxide as a catalyst, wherein a molar ratio of the 2-carboxyethylphenyl ethylene glycol hypophosphite to the propylene oxide is 1:1, gradually increasing a pressure in the reactor, wherein a maximum pressure in the reactor is 2.5 kgf/cm2, keeping a temperature in the reactor at 100-115° C., keeping the pressure for 4 h after completing the addition of propylene oxide, keeping the temperature in the reactor at 100° C., and obtaining a phosphorus-containing diol intermediate after removing unreacted small molecules in vacuum;
(c) heating another reactor to 48-52° C., firstly adding TDI into the another reactor, and then adding the phosphorus-containing diol intermediate into the another reactor at a constant rate, wherein a molar ratio of the phosphorus-containing diol intermediate to the TDI is in a range of 1:(3-4);
(d) heating the reactor to 78-82° C. and reacting for 1.9-2.2 h;
(e) removing unreacted TDI with a thin film evaporator;
(f) obtaining prepolymerized isocyanate after cooling the reactor to 48-52° C., wherein in the prepolymerized isocyanate, a mass percentage of P is 4.4%, a mass percentage of N is 7.9% and a mass percentage of —NCO is 11.9%; and
(g) mixing the prepolymerized isocyanate with a silicate modified aqueous solution according to a mass ratio in a range of 1:(1.2-1.4), thereby obtaining the silicate modified polymer foam material for filling and sealing.