# US 2023/0036469 A1 · Process for recycling laminated polymer packaging comprising aluminium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0036469 A1
- Document ID: US20230036469A1
- Status: Published application
- Kind: A1
- Application number: 17/785,157
- Filed: 2020-11-20
- Published: 2023-02-02
- Earliest claimed: 2019-12-19
- Inventors: Edson JOAQUIM ANTUNES QUEVEDO; Henrique SILVA DE ARAUJO
- Web page: https://patentgrep.com/patent/US20230036469A1

## CPC

- B29B 17/02: Separating plastics from other materials
- B29B 17/04: Disintegrating plastics, {e.g. by milling}(B29B9/02, B29B11/02, B29B13/10, {B29B17/02} take precedence)
- B29B 17/0412: {to large particles, e.g. beads, granules, flakes, slices}
- C08J 11/06: without chemical reactions
- B29B 17/0026: {by agglomeration or compacting}
- B29B 2017/0015: {Washing, rinsing}
- B29B 2017/0224: {Screens, sieves}
- B29B 2017/0244: {in liquids}
- B29B 2017/0286: {Cleaning means used for separation}
- B29B 2017/0296: {Dissolving the materials in aqueous alkaline solutions, e.g. NaOH or KOH}
- B29B 2017/0448: {Cutting discs}
- B29B 2017/0468: {Crushing, i.e. disintegrating into small particles}
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2067/003: {PET, i.e. poylethylene terephthalate}
- B29K 2105/26: Scrap {or recycled material}
- B29K 2705/02: Aluminium
- B29L 2009/003: {comprising a metal layer}
- C08J 2323/06: Polyethene
- C08J 2323/12: Polypropene
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2423/06: Polyethene
- C08J 2423/12: Polypropene
- C08J 2467/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08J2467/06 takes precedence)
- Y02W 30/62: Plastics recycling; Rubber recycling
- Y02W 30/80: Packaging reuse or recycling, e.g. of multilayer packaging (bio-packaging Y02W90/10)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

“PROCESS FOR RECYCLING LAMINATED POLYMER PACKAGING COMPRISING ALUMINIUM” contained in the application field of recycling processes, more precisely in the field of recycling processes for laminate polymeric packaging. Said process comprises stages of crushing and preliminary washing of laminate polymeric packages comprising aluminum, selective aluminum dissolution reaction, cleaning and drying, obtaining recycled fragments. The recycling process showed in the invention stands out from its similar by using the process of selective dissolution of laminate polymeric packaging comprising aluminum complemented by a combination of process parameters and steps that aim to accelerate and optimize the dissolution process and guarantee the purity and yield of the products obtained according to the process described herein.

## Claims

### Claim at position 1

-41. (canceled)

### Claim 42

PROCESS FOR RECYCLING LAMINATED POLYMER PACKAGING COMPRISING ALUMINIUM, said packages comprising a plurality of polymeric layers comprising polyethylene and polypropylene, characterized in that it comprises the following steps:
(a) crushing in a wet or dry fashion and preliminary washing of the laminate polymeric packages comprising aluminum, forming crushed laminate polymeric packages;
(b) transferring the crushed laminate polymeric packages to a reactor;
(c) applying a volume limiting screen to the reactor;
(e) immersing said crushed laminate polymeric packages into an aqueous alkaline solution, forming a first solution;
(h) temperature adjustment of the first solution;
(i) aluminum selective dissolution reaction in the first solution, forming a second solution comprising polyethylene and polypropylene fragments;
(j) draining the second solution from the reactor, so that the fragments from step (i) are retained at the bottom of the reactor;
(k) removing the fragments from the reactor and cleaning said fragments;
(l) mechanical disaggregation of the fragments of step (k), forming disaggregated fragments;
(m) decontamination of the disaggregated fragments, obtaining clean fragments based on polyethylene and polypropylene, transferring said cleaned fragments directly to the subsequent step (o); and
(o) drying the clean fragments obtained according to step (m), obtaining recycled fragments of polyethylene and polypropylene.

### Claim 43 (depends on 42)

The PROCESS, according to claim 42, characterized in that it additionally comprises the independently optional steps and in the detailed order:
(d) applying a vacuum comprises pressure values between 100 and 630 mmHg to the reactor; and/or
(f) stirring the first solution in a rotation range comprising the interval between 10 and 500 RPM; and/or
(g) applying ultrasound to the first solution; and/or
(p) pelletizing said recycled fragments.

### Claim 44 (depends on 42)

The PROCESS, according to claim 42, characterized in that the laminate polymeric packages comprising aluminum are present in amounts of up to 80% of the volumetric capacity of the reactor, wherein the reactor comprises a volume between 100 L and 50,000 L, and the aluminum amount comprises the range between 0.01% and up to 40% (mass/mass) for each Kg of said laminate polymeric packages comprising aluminum.

### Claim 45 (depends on 42)

The PROCESS, according to claim 42, characterized in that the crushing and washing in step (a) are performed through devices selected from the group that comprises chippers, shredders, cutting mills, mills rotary and plastic sprayers, wherein the crushed laminate polymeric packages comprise particles and/or fragments in any format and have dimensions between 50 microns and 5 cm and the volume limiting screen is selected from the group comprising perforated sheet, a metal screen or a plastic screen, and comprises openings of up to 01 cm.

### Claim 46 (depends on 42)

The PROCESS, according to claim 42, characterized in that the aqueous alkaline solution comprises a strong base at concentrations between 1 and 50% by mass/volume, wherein the amount of strong base comprises the range between 1.0 and 5.0 kg for each kg of aluminum present in step (e), wherein the strong base is selected from the group comprising alkali-metal hydroxides and alkaline-earth metal hydroxides and the alkali-metal hydroxides are selected from the group comprising lithium hydroxide (LiOH), sodium hydroxide (NaOH) and potassium hydroxide (KOH) and the alkaline earth metal hydroxides are selected from the group comprising calcium hydroxide Ca(OH)2, magnesium hydroxide Mg(OH)2 and barium hydroxide Ba(OH)2.

### Claim 47 (depends on 42)

The PROCESS, according to claim 42, characterized in that the temperature of the first solution in step (h) is adjusted to values between 35 and 90° C., when the crushed laminate polymeric packages comprise aluminum as an aluminum foil; or said temperature is adjusted to values between 35 and 95° C., when the crushed laminate polymeric packages comprise aluminum as a metallization layer, wherein the selective dissolution reaction of aluminum in the first solution occurs at the time range between 30 minutes and 6 hours and the fragments of step (k) are cleaned by pressing, centrifuging or suspending said fragments on an opening screen of size varying between 250 microns and 0.1 cm.

### Claim 48 (depends on 42)

The PROCESS, according claim 42, characterized in that the mechanical disaggregation is performed wet and through equipment selected from the group comprising turbine, cellulose re-pulper, high torque disperser and high shear disperser, wherein the decontamination is performed through the use of immersion water or a water-curtain system, with the water comprising a pH between 4.0 and 7.0 and the drying of clean fragments is performed in equipment comprising means for press, centrifugation and for applications of cyclone techniques, with or without hot air.

### Claim 49

A PROCESS FOR RECYCLING LAMINATE POLYMERIC PACKAGING COMPRISING ALUMINUM, said packages comprising a plurality of polymeric layers comprising polyethylene, polypropylene and polyethylene terephthalate, characterized in that it comprises the following steps:
(a) crushing in a wet or dry fashion and preliminary washing of the laminate polymeric packages comprising aluminum, forming crushed laminate polymeric packages;
(b) transferring the crushed laminate polymeric packages to a reactor;
(c) applying of a volume limiting screen to the reactor;
(e) immersing said crushed laminate polymeric packages in an aqueous alkaline solution, forming a first solution;
(h) temperature adjustment of the first solution;
(i) selective dissolution reaction of aluminum in the first solution, forming a second solution comprising polyethylene, polypropylene and polyethylene terephthalate fragments;
(j) draining the second solution from the reactor, so that the fragments from step (i) are retained at the bottom of the reactor;
(k) removing the fragments from the reactor and cleaning said fragments;
(l) mechanical disaggregation of the fragments of step (k), forming disaggregated fragments;
(m) decontamination of the disaggregated fragments, obtaining clean fragments based on polyethylene, polypropylene and polyethylene terephthalate, and transferring said clean fragments to a water tank for gravitational separation in the subsequent step (n);
(n) gravitational separation of the cleaned fragments comprising polyethylene, polypropylene and polyethylene terephthalate, in the water tank; obtaining polyethylene and polypropylene fragments in the supernatant and polyethylene terephthalate at the bottom of the tank; removing and obtaining clean polyethylene and polypropylene fragments; removing and obtaining clean polyethylene terephthalate fragments; transferring the cleaned polyethylene and polypropylene fragments to the subsequent step (o); and transferring the cleaned polyethylene terephthalate fragments to the subsequent step (o); and
(o) drying the clean fragments obtained according to step (n), obtaining recycled fragments of polyethylene, polypropylene and polyethylene terephthalate.

### Claim 50 (depends on 49)

The PROCESS, according to claim 49, characterized in that it additionally comprises the independently optional steps and in the detailed order:
(d) applying a vacuum comprises pressure values between 100 and 630 mmHg to the reactor; and/or
(f) stirring the first solution in a rotation range comprising the interval between 10 and 500 RPM; and/or
(g) applying ultrasound to the first solution; and/or
(p) pelletizing said recycled fragments.

### Claim 51 (depends on 49)

The PROCESS, according to claim 49, characterized in that the laminate polymeric packages comprising aluminum are present in amounts of up to 80% of the reactor volumetric capacity, wherein the reactor comprises a volume between 100 L and 50,000 L, and the aluminum amount comprises the range between 0.01% and up to 40% (mass/mass) for each Kg of said laminate polymeric packages comprising aluminum.

### Claim 52 (depends on 49)

The PROCESS, according to claim 49, characterized in that the crushing and washing in step (a) are performed through devices selected from the group that comprises chippers, shredders, cutting mills, rotary mills and plastic sprayers, wherein the crushed laminate polymeric packages comprise particles and/or fragments in any format and have dimensions between 50 microns and 5 cm and the volume limiting screen is selected from the group comprising perforated sheet, a metal screen or a plastic screen, and comprises openings of up to 01 cm.

### Claim 53 (depends on 49)

The PROCESS, according to claim 49, characterized in that the aqueous alkaline solution comprises a strong base in concentrations between 1 and 50% by mass/volume, wherein the amount of strong base comprises the range between 1.0 and 5.0 kg for each kg of aluminum present in step (e), wherein the strong base is selected from the group comprising alkali-metal hydroxides and alkaline-earth metal hydroxides and the alkali-metal hydroxides are selected from the group comprising lithium hydroxide (LiOH), sodium hydroxide (NaOH) and potassium hydroxide (KOH) and the alkaline-earth metal hydroxides are selected from the group comprising calcium hydroxide Ca(OH)2, magnesium hydroxide Mg(OH)2 and barium hydroxide Ba(OH)2.

### Claim 54 (depends on 49)

The PROCESS, according to claim 49, characterized in that the temperature of the first solution in step (h) is adjusted to values between 35 and 90° C., when the crushed laminate polymeric packages comprise aluminum as an aluminum foil; or said temperature is adjusted to values between 35 and 95° C., when the crushed laminate polymeric packages comprise aluminum as a metallization layer, wherein the selective dissolution reaction of aluminum in the first solution occurs in the time range between 30 minutes and 6 hours and the fragments of step (k) are cleaned by pressing, centrifuging or suspending said fragments on an opening screen of size varying between 250 micron and 0.1 cm.

### Claim 55 (depends on 49)

The PROCESS, according to claim 49, characterized in that the mechanical disaggregation is performed wet and through equipment selected from the group comprising turbine, cellulose re-pulper, high torque disperser and high shear disperser, wherein the decontamination is performed through the use of immersion water or a water-curtain system, with the water comprising a pH between 4.0 and 7.0, wherein in the gravitational separation the clean fragments of polyethylene and polypropylene are removed and obtained by means of an endless screw collector on the surface of the tank; and the clean polyethylene terephthalate fragments are removed and obtained by means of an endless screw collector at the bottom of the tank and drying of clean fragments is performed in equipment comprising means for press, centrifugation and for applications of cyclone techniques, with or without hot air.